Solving show-through depends on which mechanism dominates in the finished component:
- Ambient light passing through thin paper requires stepping up from lightweight text stock (80–120 gsm) to higher-opacity uncoated stock or cover-grade paperboard (200–300 gsm).
- High-contrast ink showing against a blank white interior requires adding an interior security pattern or dark flood coat on the inside face of the envelope.
- Contact transfer or tight-press visibility requires restoring box clearance (1.5–2.5 mm / 0.059–0.098 in across width and height; 1.5–3 mm / 0.059–0.118 in for stack height) or flipping dark card backs away from the single-ply envelope wall.
Ordered Diagnostic Checks
Inspect finished or pre-production samples in the following order to isolate the primary cause before changing paper or tooling specs. For related paper, binding, and booklet symptom checks, see the booklet and paper troubleshooting guide.
- Ambient vs. Backlit Stock Opacity Check
- How to check: Place the sealed envelope flat on a dark surface under normal room lighting, then lift it toward a direct light source.
- What it isolates: If text or card silhouettes are legible even when lying flat on a dark surface, the envelope stock lacks sufficient opacity (too thin or too porous) or dark inner ink is pressed directly against the paper fibers. If it is readable only when held up to a bright light, ambient opacity is borderline and an interior light-blocking layer is missing.
- Interior Security Barrier Check
- How to check: Open one envelope and inspect the unprinted inner face.
- What it isolates: A bare white interior offers zero contrast masking. When black clue text (100% K) or rich-black card backs sit directly behind an unprinted white inner wall, light reflects off the white fibers everywhere except where the dark ink absorbs it, making the hidden print readable from the outside.
- Box Packout Compression and Orientation Check
- How to check: Remove the envelopes from the game box and compare visibility before and after relieving lid pressure, noting which way the darkest card face or printed clue sheet points.
- What it isolates: If the clue is clearly visible only while packed inside the box—or fades once the envelope is shaken loose—tight stack height or width/height compression is forcing the dark artwork flush against the single-ply envelope face, eliminating the small air gap that normally scatters light.
Relevant Specifications
Paper Stock and Caliper
Paper weight must be specified in gsm alongside the correct US basis weight standard, because US Text LB (based on a 25 x 38 in sheet) and US Cover LB (based on a 20 x 26 in sheet) are not interchangeable:
- Lightweight interior / standard envelope paper: 80–120 gsm (approximately 54–81 lb US Text, 25 x 38 in basis), caliper 0.08–0.13 mm (0.003–0.005 in) per sheet. Uncoated sheets in this range are prone to show-through when enclosing 100% K text or dark cards without an interior tint.
- Cover-grade envelope / sleeve stock: 200–300 gsm (approximately 74–111 lb US Cover, 20 x 26 in basis). Stepping up to cover-grade stock increases sheet thickness and opacity, though it requires scored folds rather than standard light-paper creases.
- Enclosed card stock: Standard offset cards typically use 300 gsm art/blue core (0.28–0.31 mm / 0.011–0.012 in), 310 gsm black-core linen (0.30–0.32 mm / 0.012–0.013 in), 330 gsm black core (0.32–0.34 mm / 0.013–0.013 in), 350 gsm art stock (0.34–0.38 mm / 0.013–0.015 in), or 400 gsm stock (0.40–0.44 mm / 0.016–0.017 in), with double-sided film adding 0.03–0.05 mm (0.001–0.002 in) per card. Changing envelope stock thickness alters total stack height inside the box.
Prepress, Ink, and Coating
- File standards: Supply print-ready artwork in AI, PDF, or PSD using PDF/X-1a or PDF/X-4, with fonts outlined or embedded, ≥300 DPI resolution, CMYK color mode with separate spot layers if used, 3 mm (0.118 in) bleed per side, and ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered card backs).
- Black ink formulation: Keep fine clue text on inner sheets at 100% K. For dark solid areas or interior flood coats on the envelope, use rich black (C40–60 M30–40 Y30–40 K100) while keeping Total Area Coverage (TAC) at ≤280%–300%.
- Surface finish: Anti-scuff matte coating suits dark exterior or card artwork to prevent rub marks during tight packout, though exterior lamination alone does not block light transmission through low-opacity paper.
Box Packout Clearance
- Width and height clearance: Maintain 1.5–2.5 mm (0.059–0.098 in) clearance across envelope and card deck width and height inside the box or tray cavity.
- Stack height clearance: Maintain 1.5–3 mm (0.059–0.118 in) vertical clearance for the stacked components so the box lid does not clamp the envelope face tightly against dark enclosed cards.
Production Steps
When coordinating with specialist offset and tabletop manufacturing partners to resolve envelope show-through on a new or reprinted run, follow these job-specific steps:
- Select Stock Opacity or Interior Print: Either upgrade the envelope paper from 80–120 gsm uncoated stock toward opaque or 200–300 gsm cover stock, or add a second-side interior security tint / rich-black flood coat (TAC ≤280%–300%) to mask high-contrast inner elements.
- Orient High-Contrast Art Away from the Single-Ply Face: During assembly and packout, specify that enclosed dark-backed cards or bold clue sheets face toward the folded seam / double-ply back of the envelope rather than the single-ply front windowless face.
- Recalculate Box Cavity and Stack Height: Whenever envelope gsm increases or an inner liner sheet is added, verify that the combined stack height of cards, leaflets (4/6/8 panels), and envelopes still retains 1.5–3 mm (0.059–0.118 in) vertical clearance and 1.5–2.5 mm (0.059–0.098 in) width/height clearance.
Sign-Off Criteria
Approve pre-production samples or press proofs only when all of the following conditions are met:
- Zero legibility under ambient lighting: Sealed envelopes containing the darkest production card and finest 100% K clue sheet show no readable text or identifiable card silhouettes when inspected flat under normal room lighting.
- Clean interior ink cure: If an interior security pattern or dark flood coat is used, rub-test the enclosed cards and sheets after drying to confirm zero ink set-off or scuffing onto the contents.
- Verified packout clearance: Enclosed envelopes slide into the box cavity without forcing the walls outward, and the box lid closes flat with 1.5–3 mm (0.059–0.118 in) stack clearance intact.
Failure Modes
- Over-inking the interior flood coat: Exceeding TAC 280%–300% on the inside of an envelope slows drying and causes ink set-off or blocking, transferring dark smudges onto the enclosed clue cards or folded leaflets.
- Upgrading envelope stock without resizing the box: Moving from 100 gsm text stock to 250 gsm cover stock across multiple clue envelopes adds measurable stack height, eliminating the 1.5–3 mm (0.059–0.118 in) box clearance, bowing the lid, and compressing dark cards tightly against the envelope walls.
- Relying on exterior lamination for opacity: Adding standard matte or gloss film (0.03–0.05 mm / 0.001–0.002 in total when double-sided on cards) protects against scuffing but does not stop transmitted light from revealing high-contrast 100% K text through thin uncoated paper.
Parent guide Rulebook and Play Aid Troubleshooting
Related guides
- Why Do Clue Envelope Seams Pop Open or Flaps Fail to Seal?
- Why Are Staples Loose, Crooked, or Tearing Through Saddle-Stitched Booklets?
- Why Do Wire-O Bound Reference Guides Arrive Crushed or Snag Pages?
- Why Does Lamination Bubble or Lift on Rulebook Covers and Reference Sheets?