When diagnosing splits on receipt or during pack-out, check the competing causes in this order:
- Weld integrity first: Inspect whether the side or bottom seal peels open cleanly at the bond or tears along a thinned, over-heated edge.
- Card caliper and sleeve clearance second: Verify whether thick, laminated, or double-sleeved cards bow the film and overload the corner welds.
- Polymer film condition third: Flex an empty sleeve away from the seam to check for brittle cracking across the film body.
For related component issues outside paper stock, see non-paper pieces troubleshooting.
Competing Causes and Diagnostic Specifications
| Cause | Tear Pattern | Typical Trigger | Primary Physical Driver |
|---|---|---|---|
| Off-spec heat or ultrasonic sealing | Clean peel along the seam interface, or a straight tear right beside a thinned weld bead | Light insertion, first shuffle, or opening a fresh pack | Insufficient dwell/energy (cold weld) or excessive heat/pressure (scorched/thinned edge) |
| Tight sleeve sizing over thick cards | Split starts at the bottom-to-side corner junction and unzips upward | Forcing thick or laminated cards into a narrow sleeve | Card thickness consumes lateral slack, turning shear load into peel stress at the weld |
| Brittle polymer stock | Jagged snap or star-shaped crack propagating across the film face rather than following the weld | Shuffling, corner flexing, or cold-weather handling | Degraded, over-aged, or off-spec polymer film with low tear elongation |
Card stock thickness directly changes how much internal width a sleeve needs. When specifying or checking sleeves for custom deck formats, pair the sleeve's inner width with the actual finished card caliper rather than assuming a universal fit:
- 300 gsm art or blue core: 0.28–0.31 mm (0.011–0.012 in)
- 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in)
- 330 gsm black core: 0.32–0.34 mm (0.0126–0.0134 in)
- 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in)
- 400 gsm stock: 0.40–0.44 mm (0.016–0.017 in)
- PVC card stock: 0.30 mm (0.012 in)
- Double-sided lamination: Adds 0.03–0.05 mm (0.001–0.002 in) per card
When converting paper weights across specifications, specify gsm alongside caliper and distinguish US Cover LB (20 × 26 in basis sheet) from US Text LB (25 × 38 in basis sheet), as card stocks fall in the Cover LB range.
Step-by-Step Diagnostic and Production Checks
- Inspect the seam line and corner welds: Pull a split sleeve gently at an intact section of the same seam. If the two plies separate smoothly without stretching the film, sealing energy or dwell time was too low. If the film snaps cleanly along the edge of a narrow, glassy, or darkened bead, the weld over-heated and thinned the polymer.
- Measure card caliper and insertion clearance: Measure individual finished cards—including any double-sided film—and insert a card slowly. If the card bows the sleeve faces outward and stops short of the bottom corners without resistance-free seating, the sleeve width is too tight for the deck's caliper.
- Test empty film flexibility: Fold and flex an uninserted sleeve across its center body away from the welds. Healthy polymer bends without cracking or white stress-crazing; brittle stock snaps or develops micro-cracks under light finger pressure.
- Check boxed deck clearance: If sleeved decks ship inside a rigid box, verify box clearance of 1.5–2.5 mm (0.059–0.098 in) across width and height and 1.5–3 mm (0.059–0.118 in) for stack height so tight packaging does not compress sleeve corners in transit.
Sign-Off Criteria
- Seam continuity: Side and bottom welds are uniform in width with no pinholes, scorched edges, or unbonded gaps.
- Insertion and shuffle hold: Cards slide to the bottom corner without catching, and repeated riffle or mash shuffles do not initiate corner separation.
- Film ductility: Flexing an empty sleeve produces no surface cracking or sudden cross-film tears.
- Compliance documentation: Where partner-sourced sleeves or non-paper components are supplied for products subject to toy safety rules, retain the applicable EN 71 assessment and testing records with the production lot file.
Concrete Failure Modes
- Cold-weld peel: The side seam opens cleanly along the bond line with intact, unstretched film edges; caused by low sealing temperature, short dwell time, or contaminated film surfaces.
- Over-weld edge tear: The weld bead itself stays bonded, but the film shears immediately adjacent to it because excessive heat or ultrasonic pressure thinned the polymer wall.
- Corner-junction unzipping on thick decks: Sleeves sized for standard 300 gsm (0.28–0.31 mm / 0.011–0.012 in) cards split at the bottom corners when loaded with 350–400 gsm (0.34–0.44 mm / 0.013–0.017 in) or double-laminated cards.
- Cross-film brittle fracture: Tears jump out of the seam into the clear face or start at a minor edge nick, indicating aged resin, off-spec polymer formulation, or cold-brittle stock.