Conditions that change this setup:

  • Bordered card backs: Increase the inward safe margin from 3 mm (0.118 in) to 4–5 mm (0.157–0.197 in) so minor cutting shifts do not produce visibly uneven borders on narrow cards.
  • Dark artwork or gilded edges: Heavy dark solids require anti-scuff matte film to resist rub marks, whereas thick lamination can conflict with gilded-edge finishing.
  • Other tabletop formats: Alternative card sizes require their own trim dies and tooling; review the tabletop card sizes overview when selecting a different format for your deck.

Dimensions and Template Specifications

All inch values are derived from the assigned millimetre dimensions at 25.4 mm per inch, and pixel counts are calculated at 300 DPI.

Parameter Millimetres (mm) Inches (in) 300 DPI Pixels (px) Notes
Trim Size (Finished Card) 41 × 63 mm 1.61 × 2.48 in 484 × 744 px Final die-cut card dimensions
Bleed Allowance 3 mm per side 0.118 in per side 35 px per side Full-bleed artwork extension
Bleed Canvas (Artboard) 47 × 69 mm 1.85 × 2.72 in 555 × 815 px Required export file size
Safe Area (Standard) 35 × 57 mm 1.38 × 2.24 in 413 × 673 px ≥3 mm (0.118 in) inward from trim
Safe Area (Bordered Backs) 31–33 × 53–55 mm 1.22–1.30 × 2.09–2.17 in 366–390 × 626–650 px ≥4–5 mm (0.157–0.197 in) inward from trim
Corner Radius R3–R3.5 mm 0.118–0.138 in — Keep corner graphics clear of arc

Bleed and Pixel Formulas

Bleed Canvas Width  = Trim Width + (2 × Bleed) = 41 + (2 × 3) = 47 mm
Bleed Canvas Height = Trim Height + (2 × Bleed) = 63 + (2 × 3) = 69 mm
Inches              = Millimetres / 25.4
Pixels (300 DPI)    = (Millimetres / 25.4) × 300

Stock, Finish, and Prepress Parameters

  • Run minimums: Standard offset card production starts at 200 decks (typical tiers: 200, 300, 500, 1,000+).
  • Card stock and caliper: Specify stock in gsm rather than US Text LB or Cover LB, as Text and Cover pound weights use different basis sheet sizes. Approximate single-card calipers:
    • 300 gsm art or blue core: 0.28–0.31 mm (0.011–0.012 in)
    • 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in)
    • 330 gsm black core: 0.32–0.34 mm (0.013 in)
    • 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in)
    • 400 gsm stock: 0.40–0.44 mm (0.016–0.017 in)
    • PVC: 0.30 mm (0.012 in)
    • Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card.
  • Box clearance: When pairing Mini US decks with a box, allow 1.5–2.5 mm (0.059–0.098 in) clearance across width and height, and 1.5–3 mm (0.059–0.118 in) for total deck stack height.
  • File and color setup: Supply AI, PDF, or PSD files exported to PDF/X-1a or PDF/X-4 in CMYK with separate spot layers, ≥300 DPI raster resolution, and outlined or embedded fonts. Set fine text to 100% K, use rich black at C40–60 M30–40 Y30–40 K100, and keep total area coverage (TAC) at ≤280%–300%.

Job-Specific Production Steps

  1. Build the template canvas: Create a 47 × 69 mm (1.85 × 2.72 in) document at ≥300 DPI in CMYK color mode, marking the 41 × 63 mm (1.61 × 2.48 in) trim line and R3–R3.5 mm (0.118–0.138 in) corner curves on a non-printing guide layer.
  2. Extend full-bleed artwork: Pull all background colors, textures, and edge-to-edge illustrations out to the 47 × 69 mm (1.85 × 2.72 in) canvas edge so every side carries a 3 mm (0.118 in) bleed.
  3. Position safe-zone elements: Keep all typography, icons, and critical frames inside the 35 × 57 mm (1.38 × 2.24 in) safe area, or inside 31–33 × 53–55 mm (1.22–1.30 × 2.09–2.17 in) for bordered backs.
  4. Separate ink and spot plates: Convert small text to 100% K, verify rich-black builds stay within TAC ≤280%–300%, isolate foil or spot-UV masks on dedicated spot layers, and outline or embed all fonts.
  5. Export and verify imposition: Export press-ready PDF/X-1a or PDF/X-4 files and review die-line overlays on the proof before sheet imposition and cutting.

Sign-Off Criteria

  • Exported artboard measures 47 × 69 mm (1.85 × 2.72 in) / 555 × 815 px at ≥300 DPI with no upscaled low-resolution images.
  • All critical text and graphics sit at least 3 mm (0.118 in) inside the 41 × 63 mm trim line—or 4–5 mm (0.157–0.197 in) for bordered backs—and clear the R3–R3.5 mm (0.118–0.138 in) corner arcs.
  • Fonts are outlined or embedded, fine text uses 100% K only, and rich-black areas do not exceed 280%–300% TAC.
  • Spot-finish layers are separated from CMYK process plates.

Concrete Failure Modes

  • Lopsided card-back borders: Placing decorative borders closer than 4–5 mm (0.157–0.197 in) to the 41 × 63 mm trim makes minor die-cut registration shifts immediately noticeable across the narrow 41 mm width.
  • White slivers along card edges: Stopping background fills at the 41 × 63 mm trim line instead of extending them to 47 × 69 mm (1.85 × 2.72 in) leaves unprinted paper visible when the die cuts through the sheet.
  • Clipped corner indices: Aligning corner symbols strictly to a square 3 mm margin without accounting for the R3–R3.5 mm (0.118–0.138 in) corner radius causes the rounded die to slice into corner details.
  • Fuzzy micro-text: Printing small card text with four-color rich black instead of 100% K produces color-registration halos on a compact 41 × 63 mm layout.
  • Scuffed dark faces or edge-gilding conflicts: Omitting anti-scuff matte film on dark full-bleed artwork leads to visible handling rub, while applying thick lamination over cards intended for gilded edges causes edge-adhesion failures.