This compact cut is the right choice when cards must fit small-format sleeves, compact tabletop trays, or tight tuckboxes. Switch to Standard Euro if your artwork or sleeve ecosystem depends on the extra 6 mm (0.236 in) of vertical height, or choose Poker when card layouts need a wider canvas for dense rules text—see Tabletop Card Sizes to compare sibling formats. For bordered card backs, expand the interior safe-area inset from 3 mm (0.118 in) to 4–5 mm (0.157–0.197 in) so die-cut tolerance never produces uneven borders.

Template Dimensions and 300 DPI Specifications

Specification Millimetres (mm) Inches (in) Pixels at 300 DPI Notes
Trim Size 59 × 86 mm 2.32 × 3.39 in 697 × 1,016 px Final die-cut card size
Bleed Canvas 65 × 92 mm 2.56 × 3.62 in 768 × 1,087 px Adds 3 mm (0.118 in) bleed per side
Standard Safe Area 53 × 80 mm 2.09 × 3.15 in 626 × 945 px 3 mm (0.118 in) inset from trim
Bordered-Back Safe Area 49–51 × 76–78 mm 1.93–2.01 × 2.99–3.07 in 579–602 × 898–921 px 4–5 mm (0.157–0.197 in) inset from trim
Corner Radius R3–R3.5 mm 0.118–0.138 in — Keep corner graphics clear of arc

All inch and pixel equivalents derive from 25.4 mm per inch using the following plain-text formulas:

  • Bleed width (mm) = Trim width (mm) + (2 × 3 mm) = 59 + 6 = 65 mm
  • Bleed height (mm) = Trim height (mm) + (2 × 3 mm) = 86 + 6 = 92 mm
  • Inches = Dimension (mm) / 25.4
  • Pixels at 300 DPI = round((Dimension (mm) / 25.4) × 300)

Format Distinction: Small Trading Card vs. Standard Euro and Poker

  • Versus Standard Euro: Small Trading Card shares the narrow profile of Standard Euro but trims 6 mm (0.236 in) shorter vertically. That 6 mm difference changes the cutting die, tuckbox height, and sleeve fit. Artwork built for Standard Euro cannot simply be cropped at the top or bottom without shifting visual balance, and 59 × 86 mm cards require matching small-format sleeves rather than Euro sleeves that leave excess headroom.
  • Versus Poker: Poker decks provide a wider, larger surface suited to multi-line text boxes and broader illustrations. Moving a Poker layout onto a 59 × 86 mm template requires re-typesetting and adjusting element proportions rather than uniform scaling, which shrinks body copy and compresses inner margins.
  • Box and Insert Impact: Because deck width, height, and thickness determine packaging tooling, size any tuckbox or rigid box around the 59 × 86 mm trim plus 1.5–2.5 mm (0.059–0.098 in) clearance across width and height, and 1.5–3 mm (0.059–0.118 in) clearance for total stack height.

Prepress, Stock, and Finishing Specifications

Card Deck Press produces custom decks through specialist offset and tabletop manufacturing partners, with standard offset card runs starting at 200 decks (usual production tiers: 200, 300, 500, and 1,000+ decks).

  • File Format and Color: Supply print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4. Build artwork in CMYK with separate spot layers for foil, spot UV, or die-lines. Outline or embed all fonts, and keep raster imagery at ≥300 DPI at final print size.
  • Black Ink and Coverage: Use 100% K for fine text and thin rules. For solid black backgrounds, use rich black (C40–60 M30–40 Y30–40 K100) while keeping total area coverage (TAC) at ≤280%–300%.
  • Card Stock and Caliper: Specify stock by gsm (distinguishing US Cover LB from US Text LB by their different basis sheet sizes). Typical card calipers are:
    • 300 gsm art / blue core: 0.28–0.31 mm (0.011–0.012 in)
    • 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in)
    • 330 gsm black core: 0.32–0.34 mm (0.013 in)
    • 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in)
    • 400 gsm stock: 0.40–0.44 mm (0.016–0.017 in)
    • PVC: 0.30 mm (0.012 in)
  • Lamination and Edge Finishes: Double-sided film adds 0.03–0.05 mm (0.001–0.002 in) per card to stack height. Anti-scuff matte lamination suits dark artwork with heavy ink coverage. Avoid pairing thick lamination with gilded edges, as the two finishes can conflict during edge application.

Production Steps and Sign-Off Criteria

  1. Set Up the Bleed Canvas: Create the document at 65 × 92 mm (2.56 × 3.62 in)—or 768 × 1,087 px at 300 DPI—with trim guides at 59 × 86 mm (2.32 × 3.39 in).
  2. Establish Safe Zones: Place text, icons, and frame borders inside 53 × 80 mm (2.09 × 3.15 in) for full-bleed cards, or 49–51 × 76–78 mm (1.93–2.01 × 2.99–3.07 in) for bordered backs. Keep corner details clear of the R3–R3.5 mm (0.118–0.138 in) corner arc.
  3. Separate Non-Printing Layers: Put die-lines, corner-radius guides, and spot finishes on dedicated spot layers set to overprint or non-printing as required, never merged into the CMYK artwork.
  4. Verify Color and Export: Confirm 100% K on small text, rich black values on dark solids, TAC ≤280%–300%, and outlined/embedded fonts before exporting PDF/X-1a or PDF/X-4.

Sign-off criteria before press:

  • Bleed canvas measures exactly 65 × 92 mm (768 × 1,087 px at 300 DPI) with artwork extending fully to the outer edge.
  • All live type and critical artwork sit inside the 3 mm (or 4–5 mm bordered-back) safe area.
  • All raster links are ≥300 DPI in CMYK, with TAC ≤280%–300% and spot layers separated.
  • Card stock gsm, core type, finish, and box clearances match the confirmed deck count.

Failure Modes

  • Uneven or Clipped Card Back Borders: Placing a printed border within 3 mm of the trim line exposes normal die-cut shift; use a 4–5 mm (0.157–0.197 in) safe margin on bordered backs or switch to full-bleed backs.
  • White Edge Slivers: Designing at 59 × 86 mm without the 3 mm (0.118 in) bleed per side leaves unprinted paper along edges when the die cuts slightly outside the nominal line.
  • Cropped Corner Badges: Square corner frames or pip icons placed near the outer corners get sliced by the R3–R3.5 mm (0.118–0.138 in) corner-rounding die.
  • Cramped Layouts from Direct Resizing: Scaling a Poker or Standard Euro file down to 59 × 86 mm without re-typesetting produces illegible micro-text and distorted aspect ratios.
  • Scuffing, Set-Off, or Gilding Peeling: Exceeding 300% TAC causes slow drying and ink transfer, dark uncoated/standard-matte backs show abrasion without anti-scuff matte, and thick lamination interferes with gilded-edge adhesion.