Both materials run on standard offset presses starting at 200 decks (usual tiers of 200, 300, 500, and 1,000+ decks) through specialist offset and tabletop manufacturing partners. The decision comes down to how ink sits on the sheet, whether the deck needs protective film, and whether players or users will write directly on the cards. For broader material pairings across cores and plastics, see the card comparison hub.

When to Switch Between Coated and Uncoated

  • Choose coated art cardstock when artwork relies on saturated photography, fine detail, deep dark solids, or protective finishes such as aqueous coating, gloss lamination, or anti-scuff matte lamination.
  • Choose uncoated cardstock when the deck functions as a writable score card, prompt card, or note card that must take ballpoint pen, marker, or pencil without smearing, or when an exposed, non-reflective paper tooth is required.
  • Switch from uncoated to coated if the design uses heavy full-bleed dark backgrounds—uncoated fibers absorb ink and show edge wear quickly without film protection.
  • Switch from coated to uncoated if end-users need to stamp, sign, or write on the card face, because clay coating and plastic lamination repel standard ink and graphite.

Material Specifications

Coated art paperboard uses a smooth clay-coated surface that holds ink on top of the sheet for sharp halftone dots. Uncoated offset cardstock leaves the cellulose fibers exposed, increasing ink absorption and surface friction.

Specification Coated Art Cardstock Uncoated Cardstock
Surface structure Clay-coated, smooth, low porosity Exposed paper grain, porous, matte tooth
Ink holdout & color High holdout; crisp edges and vibrant CMYK density Lower holdout; softer contrast and higher dot gain
Scuff resistance Moderate raw; high with varnish or anti-scuff matte film Lower on heavy ink coverage; edges show fiber wear sooner
Writability Poor; ink smears on clay coating and lamination High; accepts pencil, ballpoint pen, and stamps
Typical weight & caliper 300 gsm art/blue core: 0.28–0.31 mm (0.0110–0.0122 in); 350 gsm art stock: 0.34–0.38 mm (0.0134–0.0150 in); 400 gsm: 0.40–0.44 mm (0.0157–0.0173 in) Commonly specified in 300–400 gsm ranges matching target stiffness and bulk
Lamination allowance Compatible; double-sided film adds 0.03–0.05 mm (0.0012–0.0020 in) per card Generally left unlaminated to preserve grain and writability

Weight Units and Basis Sheet Distinctions

Cardstock weight is specified in grams per square meter (gsm) alongside caliper in mm (in), because US pound (lb) ratings depend on the uncut basis sheet size:

  • US Cover LB uses a 20 × 26 in (508 × 660 mm) basis sheet.
  • US Text LB uses a 25 × 38 in (635 × 965 mm) basis sheet.

Because the Cover basis sheet is smaller than the Text basis sheet, a 100 lb Cover stock is substantially thicker and heavier per square meter than a 100 lb Text stock. Always confirm both gsm and target caliper in mm (in) rather than relying on pound weight alone. Higher gsm stocks and added lamination also increase total deck stack height and shipping mass in kg (lb)—for example, moving from 300 gsm to 400 gsm increases paper mass by one-third per sheet across a multi-kilogram (multi-pound) production carton.

Job-Specific Production Steps

  1. Prepress and Color Separation
    • Supply print-ready files in AI, PDF, or PSD format exported as PDF/X-1a or PDF/X-4 at ≥300 DPI with outlined or embedded fonts.
    • Set 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin (or ≥4–5 mm / 0.157–0.197 in for bordered backs), and plan for R3–R3.5 mm (0.118–0.138 in) die-cut corners.
    • Keep fine text at 100% K. Build large dark areas with rich black (C40–60 M30–40 Y30–40 K100) and keep Total Area Coverage (TAC) at ≤280%–300%.
    • Place any spot treatments on separate spot layers rather than flattening them into CMYK artwork.
  2. Press Calibration by Stock
    • For coated art, calibrate ink limits to stay within ≤280%–300% TAC so sheets dry cleanly before coating or lamination.
    • For uncoated cardstock, adjust curves for higher dot gain and avoid heavy ink saturation; excess ink soaks into the open fibers and causes set-off onto the back of adjacent press sheets.
  3. Coating, Lamination, and Finishing
    • Apply protective varnish or lamination to coated art decks. Use anti-scuff matte lamination when cards feature dark artwork that is handled frequently.
    • If a coated deck specifies gilded edges, coordinate film thickness early—thick lamination can conflict with edge-gilding adhesion.
    • Leave uncoated decks unlaminated and unvarnished wherever writing or stamping is required.

Sign-Off Criteria

Verify the following measurable conditions on pre-production or press proofs before full production:

  • Caliper and stack height: Single-card thickness matches the target stock range in mm (in), accounting for +0.03–0.05 mm (+0.0012–0.0020 in) if double-sided film is applied.
  • Ink density and registration: Fine 100% K text is sharp without color haloing, and dark rich-black panels show even tone without mottling.
  • Surface function: Coated anti-scuff matte cards resist dry-rub marking on dark solids; uncoated cards accept standard pen and pencil without skipping or smudging.
  • Trim and corner geometry: Card borders remain symmetrical within the ≥4–5 mm (0.157–0.197 in) bordered-back safety zone, and corners die-cut cleanly to R3–R3.5 mm (0.118–0.138 in).

Concrete Failure Modes

  • Muddy artwork and ink set-off on uncoated stock: Exceeding 280%–300% TAC on porous uncoated board causes fibers to wick ink, flattening midtones and transferring wet ink onto stacked sheets.
  • Scuffing on dark coated cards: Running dark, high-coverage coated art cardstock without anti-scuff matte lamination results in visible rub marks and white edge-cracking during shuffling and packing.
  • Gilding failure over thick lamination: Applying heavy lamination film to coated cards prior to edge gilding can prevent metallic foil from bonding cleanly to the trimmed card edges.
  • Blocked writability: Applying an overall aqueous seal or laminate onto an uncoated deck seals the paper tooth, causing pen ink to bead and smear.