This choice sits within card comparisons as a substrate decision between a pre-laminated holographic paperboard that requires opaque white-ink underbases and uncoated or coated white paperboard printed directly in CMYK.

Conditions that change the decision:

  • Choose holographic foil cardstock when the design relies on continuous iridescent refraction across borders, backgrounds, or focal illustrations, and the layout avoids ultra-fine body copy directly over bare foil.
  • Choose standard white cardstock when brand colors, skin tones, or neutral grays must match tightly, when rules text or stat blocks sit at small point sizes, or when the production schedule cannot accommodate white-ink mask proofing.
  • Hybrid edge cases: If metallic shine is limited to a small crest, border accent, or title rather than spanning the card face, standard white cardstock with a targeted metallic finish avoids masking the entire sheet with white ink.

Material and Prepress Specifications

Standard offset card runs start at 200 decks, with usual production tiers at 200, 300, 500, and 1,000+ decks. Card stocks are specified in gsm alongside US Cover LB (measured on a 20 x 26 in basis sheet) rather than US Text LB (measured on a 25 x 38 in basis sheet), because equal LB numbers represent much heavier board in Cover weight than in Text weight.

Specification Holographic Foil Stock Standard White Cardstock
Substrate construction White paperboard pre-laminated with a patterned holographic film layer Uncoated or coated white paperboard (art stock, blue core, or black core)
Base stock & caliper (mm / in) Built on standard board weights; pre-laminated film and protective double-sided film add 0.03–0.05 mm (0.0012–0.0020 in) per card 300 gsm art/blue core: 0.28–0.31 mm (0.0110–0.0122 in); 310 gsm black-core linen: 0.30–0.32 mm (0.0118–0.0126 in); 330 gsm black core: 0.32–0.34 mm (0.0126–0.0134 in); 350 gsm art stock: 0.34–0.38 mm (0.0134–0.0150 in); 400 gsm: 0.40–0.44 mm (0.0157–0.0173 in)
Color & spot layers CMYK plus a dedicated spot layer for the opaque white-ink underbase mask CMYK with optional spot ink or Pantone layers only where needed
Black ink & TAC 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; Total Area Coverage (TAC) ≤280%–300% 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; Total Area Coverage (TAC) ≤280%–300%
Resolution & file format ≥300 DPI; AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts ≥300 DPI; AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts
Bleed, safety & corners 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in for bordered backs); R3–R3.5 mm (0.118–0.138 in) corner radius 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in for bordered backs); R3–R3.5 mm (0.118–0.138 in) corner radius
Surface protection Protective varnish or film over ink; anti-scuff matte suits dark artwork; thick lamination can conflict with gilded edges Varnish, aqueous, or film lamination; anti-scuff matte suits dark artwork; thick lamination can conflict with gilded edges

Deck stack and box fit: Because pre-laminated holographic film and any topcoat film increase single-card caliper by 0.03–0.05 mm (0.0012–0.0020 in), a full deck stack grows noticeably compared to unlaminated standard white cardstock. Box dimensions must maintain 1.5–2.5 mm (0.059–0.098 in) clearance across width and height and 1.5–3 mm (0.059–0.118 in) clearance for total stack height.


Job-Specific Production Steps

  1. Prepress separation and white-ink masking:
    • Holographic foil stock: Build artwork in CMYK at ≥300 DPI, then create a separate spot channel or vector layer for the white-ink underbase. Areas left blank in the white layer allow bare holographic foil to show through or tint translucent CMYK inks; areas filled with 100% spot white block the metallic sheen so CMYK prints as opaque color.
    • Standard white cardstock: Build artwork in CMYK at ≥300 DPI with no white-ink mask required. Export both stock types as PDF/X-1a or PDF/X-4 with fonts outlined or embedded, 3 mm (0.118 in) bleed per side, and TAC ≤280%–300%.
  2. Proofing:
    • Holographic foil stock: Proof both the CMYK separations and the white-ink mask alignment on the actual pre-laminated holographic substrate to verify opacity under solid colors and contrast on exposed metallic zones.
    • Standard white cardstock: Proof CMYK color balance, 100% K fine text sharpness, and rich black density directly on the selected paperboard.
  3. Offset printing and curing:
    • Holographic foil stock: Lay down the opaque white underbase first, cure or dry sufficiently to prevent ink set-off, and overprint CMYK passes on top of the non-absorbent foil surface.
    • Standard white cardstock: Print CMYK passes directly onto the coated or uncoated paperboard, where ink absorbs and sets into the paper fibers.
  4. Surface finishing and die-cutting:
    • Apply protective varnish or film (using anti-scuff matte for dark artwork), avoiding thick lamination when gilded edges are specified.
    • Die-cut cards to the job's assigned trim format with R3–R3.5 mm (0.118–0.138 in) corners, keeping ≥3 mm (0.118 in) safety inside the trim (≥4–5 mm / 0.157–0.197 in for bordered backs).
    • Collate and pack decks into boxes sized with 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack-height clearance.

Sign-Off Criteria

Before approving full offset production (200+ decks), verify the following physical and prepress conditions on the proof:

  • White-ink opacity and registration (holographic stock): Solid white underbase blocks the holographic pattern cleanly where opaque color is intended, with no haloing or misregistration around fine edges.
  • Color accuracy and contrast: CMYK hues match target values on masked areas (holographic) or bare board (standard white), and dark solids use rich black (C40–60 M30–40 Y30–40 K100) within TAC ≤280%–300%.
  • Type legibility: Small text is set in 100% K only, remains sharp without ink spread or holographic pattern interference, and sits inside the ≥3 mm (0.118 in) safety zone.
  • Trim and border symmetry: Bleed extends 3 mm (0.118 in) past every trim edge, and bordered card backs maintain ≥4–5 mm (0.157–0.197 in) safety so R3–R3.5 mm (0.118–0.138 in) corner rounding and die tolerances do not create uneven borders.
  • Caliper and box clearance: Measured single-card caliper (including any 0.03–0.05 mm / 0.0012–0.0020 in film addition) multiplied by card count leaves 1.5–3 mm (0.059–0.118 in) vertical clearance inside the box.

Concrete Failure Modes

  • Translucent, muddy CMYK on holographic stock: Omitting the spot white-ink underbase under midtones or light colors lets the silver-rainbow foil bleed through the ink, shifting hues and dropping contrast.
  • White-ink haloing or choke mismatch: When the white-ink mask is not properly choked or trapped to the CMYK artwork, slight press-sheet shift exposes a thin white outline or bare metallic sliver along object edges.
  • Unreadable small text over foil: Placing multi-color or fine serif text directly over unmasked holographic film causes the shifting refraction pattern to break up letterforms; fine text requires 100% K over an opaque white underbase or standard white cardstock.
  • Ink scuffing and set-off on non-absorbent foil: Exceeding TAC 280%–300% or printing dark artwork without anti-scuff matte protection on pre-laminated holographic film leads to slow drying, back-to-front ink transfer in the stack, and visible surface scratches during shuffling.
  • Gilded-edge and box-fit failures: Adding thick protective lamination on top of pre-laminated holographic stock can peel or conflict with edge gilding, and failing to account for the extra 0.03–0.05 mm (0.0012–0.0020 in) per card causes the finished deck stack to bind in a box sized for unlaminated white cardstock.
  • Off-center bordered backs: Placing thin borders closer than 4–5 mm (0.157–0.197 in) to the trim line makes normal die-cut variance obvious on both holographic and standard white decks.