For full pigment coverage mechanics and edge-sticking behavior across colored edge treatments, see the colored edges specification. For broader finish trade-offs across card faces and edges, see finish comparisons.
When to Choose Matte vs. Gloss Colored Edges
- Handling frequency: Choose matte colored edges for decks that are shuffled, dealt, or fanned regularly, because flat pigment reduces edge-to-edge tackiness and hides minor handling scuffs.
- Display and shelf presence: Choose gloss colored edges for collector or lightly handled display decks where light-catching edge sheen is the priority.
- Face finish pairing: Matte colored edges pair cleanly with anti-scuff matte face lamination—especially on dark artwork—while gloss colored edges create a deliberate high-sheen contrast or match gloss face coatings.
- Color depth and glare: Matte edges read consistently from any viewing angle without specular glare; gloss edges deepen saturated pigments under direct light but highlight surface micro-scratches.
Specifications Comparison
Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+ decks). Both edge finishes apply to standard offset paper stocks and must account for card caliper, face lamination, and box clearances.
| Attribute | Matte Colored Edges | Gloss Colored Edges |
|---|---|---|
| Edge Appearance | Flat, non-reflective pigment with uniform tone across angles | High-sheen, light-reflective surface with deeper visual saturation |
| Edge-to-Edge Sticking | Lower risk of tackiness between adjacent cards | Higher risk of tackiness under heat, pressure, or incomplete cure |
| Handling & Scuff Resistance | Hides finger oils and light friction marks during shuffling | Shows micro-scuffs, fingerprints, and burnishing with frequent play |
| Compatible Card Stocks | 300 gsm art/blue core (0.28–0.31 mm / 0.011–0.012 in), 310 gsm black-core linen (0.30–0.32 mm / 0.012–0.013 in), 330 gsm black core (0.32–0.34 mm / 0.013 in), 350 gsm art stock (0.34–0.38 mm / 0.013–0.015 in), 400 gsm (0.40–0.44 mm / 0.016–0.017 in) | Same paper stock range; best reserved for stiffer, lightly handled display builds |
| Face Lamination Interaction | Pairs directly with anti-scuff matte film; double-sided film adds 0.03–0.05 mm (0.001–0.002 in) per card | Pairs with gloss or matte film; thick lamination can conflict with precision edge treatments |
| Recommended Use Case | Regularly played decks, dark-toned borders, tight stack storage | Showcase editions, static display sets, minimal-shuffle keepsakes |
Prepress and Deck Geometry Parameters
- Bleed and safety: Supply card faces with 3 mm (0.118 in) bleed per side, at least 3 mm (0.118 in) safety margin, and at least 4–5 mm (0.157–0.197 in) safety margin for bordered backs so trim variance does not expose unprinted white stock against the colored edge.
- Corner radius: Standard die-cut corners use R3–R3.5 mm (0.118–0.138 in).
- Files and color setup: Submit AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 at 300 DPI or higher, using CMYK with separate spot layers for edge pigment specifications, outlined or embedded fonts, 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100), and total area coverage (TAC) at or below 280%–300%.
- Box clearance: Size tuck or rigid boxes with 1.5–2.5 mm (0.059–0.098 in) clearance across width and height, and 1.5–3 mm (0.059–0.118 in) clearance for total stack height.
Production Steps
- Prepress and spot layer setup: Confirm the edge pigment color on a separate spot layer alongside the 3 mm (0.118 in) face bleed and R3–R3.5 mm (0.118–0.138 in) corner die line.
- Printing, lamination, and die-cutting: Print card sheets at 300 DPI or higher, apply double-sided film if specified (adding 0.03–0.05 mm / 0.001–0.002 in per card), and die-cut with clean blades so card edges stack flush without burrs.
- Deck clamping and edge coating: Clamp the trimmed deck tightly under uniform pressure across all cards, then apply the matte or gloss pigment evenly over all four sides and rounded corners.
- Curing and separation: Allow the clamped block to cure completely, then fan the deck in multiple directions to separate individual cards cleanly before boxing.
Sign-Off Criteria
- Uniform coverage: Solid, even pigment across all four straight edges and R3–R3.5 mm (0.118–0.138 in) corners with no bare paper core showing through.
- Clean card separation: Cards fan smoothly without sticking, tearing face lamination, or transferring pigment onto adjacent card faces.
- Consistent sheen: Matte edges show a uniform flat finish without glossy streaks; gloss edges show consistent reflection without dull patches.
- Box fit: The finished deck slides into its box within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack height clearances without scraping the colored edges against inner box walls.
Concrete Failure Modes
- Edge-to-edge sticking and face peeling: Gloss colored edges packed or flexed before full cure bond adjacent cards together, pulling pigment or face lamination off when separated.
- Pigment bleed onto card faces: Insufficient clamping pressure during coating allows liquid pigment to wick between cards, staining the outer 0.5–1 mm (0.020–0.039 in) of card faces.
- Corner gaps and rough edges: Dull die-cutting blades or uneven clamping leave stepped card edges at the R3–R3.5 mm (0.118–0.138 in) corners, causing thin or patchy pigment coverage.
- Handling scuffs and burnishing: Frequent shuffling dulls gloss edges into uneven hazy patches, while tight box walls rub matte edges into shiny burnished streaks.
- Trim-line color mismatch: Omitting the 3 mm (0.118 in) bleed or 4–5 mm (0.157–0.197 in) bordered safety margin leaves a visible white paper sliver between the card face artwork and the colored edge.
Parent guide Coating, Decoration, and Edge Finish Comparisons