Two physical conditions govern the result: stack clamping uniformity (which prevents liquid pigment from wicking inward between card faces) and substrate/coating compatibility (which determines how evenly the pigment wets, cures, and resists rub-off during handling). Unlike stamped foil—which can conflict with thick surface lamination—sprayed or inked pigments bond across laminated or varnished card edges when the deck is clamped flat and cured before separation.
Specifications and Finish Compatibility
Standard offset card runs with edge finishing start at 200 decks (usual production tiers: 200, 300, 500, and 1,000+ decks). Because painted edges add virtually zero measurable thickness compared to stamped foil, decks maintain standard box clearance of 1.5–2.5 mm (0.059–0.098 in) across width and height and 1.5–3 mm (0.059–0.118 in) for stack height without requiring custom box allowances.
Card Stock, Caliper, and Basis Weight
Card stocks are specified in gsm (grams per square meter) and fall under US Cover LB (measured on a 20 x 26 in / 508 x 660 mm basis sheet), rather than US Text LB (measured on a 25 x 38 in / 635 x 965 mm basis sheet, which applies to 80–120 gsm / 0.08–0.13 mm / 0.003–0.005 in interior booklet sheets).
| Stock Type | Nominal Caliper (mm / in) | Edge Finishing Behavior |
|---|---|---|
| 300 gsm art / blue core | 0.28–0.31 mm (0.011–0.012 in) | Moderate fiber density; requires firm clamping to block wicking |
| 310 gsm black-core linen | 0.30–0.32 mm (0.012–0.013 in) | Textured face requires tight clamp pressure at linen valleys |
| 330 gsm black core | 0.32–0.34 mm (0.013 in) | Dense core resists inward bleed; clean edge for opaque pigment |
| 350 gsm art stock | 0.34–0.38 mm (0.013–0.015 in) | Thicker edge band increases visual border prominence |
| 400 gsm stock | 0.40–0.44 mm (0.016–0.017 in) | Wide edge profile; supports high-opacity matte and metallic-toned sprays |
| PVC | 0.30 mm (0.012 in) | Non-porous edge; requires specialty adhesion-promoting ink/pigment |
Double-sided film lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card. On dark artwork, anti-scuff matte lamination protects card faces from clamp-mark burnishing and scuffing during edge finishing and subsequent handling.
Prepress and Geometry Requirements
- Bleed and safety: Provide 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin for full-bleed art, and ≥4–5 mm (0.157–0.197 in) safety for bordered backs so minor trim variance does not create an uneven gap next to the painted edge.
- Corner radius: Standard die-cut corners of R3–R3.5 mm (0.118–0.138 in) allow spray passes to wrap smoothly around corners without bridging.
- Color and file setup: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts, ≥300 DPI raster art, 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and TAC ≤280%–300%. Specify the edge color as a separate spot layer or callout distinct from the CMYK card-face artwork.
Production Steps
- Prepress and Spot Color Separation: Confirm the edge pigment callout (matte, satin, gloss, or metallic-toned) on a separate spot layer alongside the CMYK card-face files, ensuring full 3 mm (0.118 in) bleed on all sides.
- Printing, Coating, and Cutting: Print sheets via offset, apply the specified surface coating or lamination (such as anti-scuff matte on dark faces), guillotine to final trim, and round corners to R3–R3.5 mm (0.118–0.138 in).
- Stacking and Clamping: Jog each deck flush and clamp the stack under uniform mechanical pressure. Eliminating air gaps between cards is critical to seal the face borders against liquid pigment.
- Spraying or Inking: Apply opaque pigment across the clamped edges in controlled passes. Spraying delivers uniform matte, satin, gloss, or metallic-toned coverage around curved corners; direct inking suits flat, solid-tone edges.
- Curing and Fanning: Allow the pigment layer to cure completely before releasing clamp pressure, then fan the deck to separate individual cards cleanly before boxing.
Sign-Off Criteria
- Coverage and Sheen Consistency: Uniform color density and sheen (matte, satin, gloss, or metallic-toned) across all four edges and R3–R3.5 mm (0.118–0.138 in) corners, with no bare paper core or core-tint show-through.
- Wicking Limit: Clean, sharp cutoff at the card perimeter with zero inward pigment bleed onto card faces or bordered backs.
- Handling Resistance and Separation: Cards fan apart smoothly without tearing edge pigment, and normal shuffling does not rub pigment onto fingers or adjacent card surfaces.
- Regulatory Documentation (Children's Games): When a deck is intended for children, edge pigments and surface coatings are subject to EN 71 assessment and testing procedures documented under the European Commission Toy Safety framework.
Concrete Failure Modes
- Edge Wicking (Inward Bleed): Light or uneven clamping—or textured linen stocks clamped with insufficient force—allows liquid ink to wick along paper fibers onto the card face. Prevent by verifying flush jogging, uniform clamp pressure, and fast-setting opaque pigment formulations.
- Card Blocking (Edge Sticking): Releasing the clamp or boxing decks before gloss or heavy pigment layers finish curing causes adjacent edges to bond, chipping the finish when cards are fanned. Prevent by applying thin passes, enforcing full cure time, and fanning decks prior to packaging.
- Corner Thinning or Bridging: Die-cut burrs or single-angle spraying leave thin coverage or pooled pigment on R3–R3.5 mm (0.118–0.138 in) corners. Prevent with sharp corner-rounding dies and multi-angle spray coverage.
- Rub-Off on Handling: Over-thick metallic-toned or unsealed pigment transfers onto hands or dark card faces during shuffling. Prevent by controlling film build and pairing dark card faces with anti-scuff matte lamination.
- Trim-to-Edge Contrast Mismatch: Narrow back borders under 4–5 mm (0.157–0.197 in) safety amplify minor cut tolerances against a high-contrast painted edge, making borders look off-center. Prevent by keeping bordered backs within the recommended safety zone or matching edge pigment to the outer bleed tone.