- Choose a folding board (bi-fold, quad-fold, or 6-panel) when the unfolded play area exceeds the box footprint and requires a continuous printed surface with paper-wrapped or cloth-taped hinges.
- Choose interlocking board panels when modular layouts or variable table footprints are required, or when folded stack height on a multi-fold board would exceed the box depth.
- Choose a dual-layer recessed player board when tokens, cubes, or trackers must stay seated during play, using a die-cut top layer laminated over a solid backing board.
- Choose a GM screen when vertical standing rigidity is required across 3 or 4 portrait or landscape panels, using thicker 2.5–3 mm (0.098–0.118 in) greyboard and wider hinge gaps so panels stand without tipping or binding.
Boxed games and board tooling follow project and component minimums rather than the 200-deck starting tier used for standard offset cards.
Core Material and Thickness Specifications
Game boards and GM screens are built by laminating printed wrap sheets onto rigid greyboard cores. When specifying paper wraps and liners, state weight in gsm; if referencing US basis weights, distinguish US Text LB (measured on a 25 × 38 in / 635 × 965 mm basis sheet) from US Cover LB (measured on a 20 × 26 in / 508 × 660 mm basis sheet), because identical pound numbers represent different sheet weights and calipers.
| Material / Component | Metric Specification | Imperial Equivalent | Structural Role and Notes |
|---|---|---|---|
| Greyboard core (light) | 1.5 mm | 0.059 in | Top die-cut layer of dual-layer recessed boards; compact or light player mats |
| Greyboard core (standard) | 2.0 mm | 0.079 in | Standard folding boards, backing layers for recessed boards, light interlocking tiles |
| Greyboard core (heavy) | 2.5 mm | 0.098 in | Large quad-fold or 6-panel boards, heavy interlocking panels, standard GM screens |
| Greyboard core (extra-heavy) | 3.0 mm | 0.118 in | Heavy-duty GM screens and oversized boards requiring maximum warp resistance |
| Wrap margin allowance | 15–20 mm per side | 0.591–0.787 in per side | Turned over the greyboard edge and glued to the underside or liner |
| Lamination film (double-sided) | +0.03–0.05 mm total | +0.001–0.002 in total | Anti-scuff matte lamination recommended for dark artwork to prevent rub marks |
| Interlocking die gap | 3–4 mm | 0.118–0.157 in | Minimum spacing between die-cut panel edges on a press sheet |
| Box cavity clearance (W / H) | 1.5–2.5 mm | 0.059–0.098 in | Required gap between folded board outer dimensions and inner box walls |
| Box cavity clearance (stack) | 1.5–3.0 mm | 0.059–0.118 in | Vertical clearance above the folded board stack and companion components |
Structure, Fold Counts, and Thickness Combinations
Folded boards and GM screens require deliberate hinge spacing between adjacent greyboard panels so the wrap paper bridges the joint without tearing when closed or buckling when opened flat.
| Board / Screen Type | Typical Panel / Fold Count | Recommended Greyboard Combination | Hinge / Joint Construction | Key Fit & Alignment Requirement |
|---|---|---|---|---|
| Bi-fold board | 2 panels (1 fold) | 2.0 mm or 2.5 mm (0.079 or 0.098 in) | Single wrapped paper hinge; optional inner liner over the joint | Folded height = 2 × board caliper + wrap/film thickness |
| Quad-fold board | 4 panels (2 folds, 2 × 2) | 2.0 mm (0.079 in) standard; 2.5 mm (0.098 in) max | Primary center hinge plus secondary cross-fold hinge with wider gap | Secondary fold must accommodate double-panel thickness inside the crease |
| 6-panel board | 6 panels (3 folds, 2 × 3) | 1.5 mm or 2.0 mm (0.059 or 0.079 in) | Multi-stage accordion or gate-fold hinges | Keep caliper at 1.5–2.0 mm to prevent excessive folded stack height |
| Interlocking board | 2 to 8+ separate panels | 2.0 mm or 2.5 mm (0.079 or 0.098 in) | Die-cut puzzle tabs and slots across matching panel edges | Maintain 3–4 mm (0.118–0.157 in) die gap on sheet; verify tab clearance after wrap |
| Dual-layer recessed board | 1 solid base + 1 die-cut top | 1.5 mm (0.059 in) top + 1.5–2.0 mm (0.059–0.079 in) base | Full-face adhesive lamination of die-cut frame onto solid backing | Registration of top cut-outs to base artwork within tight visual tolerance |
| GM screen | 3 or 4 panels (2 or 3 folds) | 2.5 mm or 3.0 mm (0.098 or 0.118 in) | Wide-gap wrapped hinges allowing 90°–135° standing angles | Center panels and wings must balance upright without bowing or tipping |
Prepress, Wrap Allowances, and Box Fit
Board wraps and liners are supplied as print-ready AI, PDF, or PSD files exported to PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Color and Resolution: Build artwork in CMYK with separate spot layers for any foil, spot UV, or die-line indicators, at ≥300 DPI at final print size.
- Black Ink Formulation: Use 100% K for fine text and thin rules. Use rich black (C40–60 M30–40 Y30–40 K100) for large solid areas while keeping Total Area Coverage (TAC) at ≤280%–300%.
- Bleed and Safety: Include 3 mm (0.118 in) bleed beyond the outer wrap trim or die-cut edge, and keep critical text and graphics ≥3 mm (0.118 in) inside all panel edges, fold lines, and recessed cut-outs.
- Wrap and Cavity Formulas (plain text):
Wrap Sheet Width = Unfolded Board Width + (2 × Greyboard Thickness) + (2 × Wrap Margin [15–20 mm / 0.591–0.787 in])Wrap Sheet Height = Unfolded Board Height + (2 × Greyboard Thickness) + (2 × Wrap Margin [15–20 mm / 0.591–0.787 in])Folded Board Stack Height = (Panel Layers Stacked × (Greyboard Thickness + Wrap/Film Allowance))Minimum Inner Box Width or Height = Folded Board Width or Height + 1.5 to 2.5 mm (0.059 to 0.098 in) clearanceMinimum Inner Box Depth = Folded Board Stack Height + Companion Component Height + 1.5 to 3.0 mm (0.059 to 0.118 in) clearance
Production Steps and Sign-Off Criteria
Card Deck Press coordinates board and screen builds with specialist offset and tabletop manufacturing partners through four controlled stages:
- Prepress and Dieline Verification: Verify CMYK separation, TAC ≤280%–300%, 3 mm (0.118 in) bleed, ≥3 mm (0.118 in) safety around fold lines and recesses, and exact hinge-gap positioning on the master dieline.
- Sheet Printing and Surface Finishing: Print wrap and liner sheets at ≥300 DPI and apply lamination (anti-scuff matte for dark artwork). Verify sheet flatness and ink curing before mounting.
- Core Cutting, Wrapping, and Assembly: Cut greyboard panels to caliper spec, position panels with the required hinge gaps, wrap the outer sheet over the 15–20 mm (0.591–0.787 in) margin, and apply the inner liner. For dual-layer boards, die-cut the top frame and laminate it under pressure onto the backing board; for interlocking boards, die-cut after wrapping or align pre-cut panels.
- Dry-Fit and Cavity Sign-Off:
- Flatness and Hinge Action: Opened board lies flat without tenting at the spine; GM screen panels stand cleanly across intended angles without binding.
- Recess and Joint Registration: Dual-layer cut-outs align cleanly with printed base wells; interlocking tabs seat firmly without forcing or tearing wrap edges.
- Box Fit: Folded board slides into the target box cavity within the 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3.0 mm (0.059–0.118 in) stack-height clearance.
Concrete Failure Modes
- Board Warping or Cupping: Caused by unbalanced moisture absorption between the outer wrap and inner liner, or by pairing a heavy wrap/lamination with an undersized 1.5 mm (0.059 in) greyboard across a large span.
- Hinge Splitting or Crease Cracking: Caused by an undersized hinge gap between greyboard panels, folding across the grain of the wrap paper, or omitting protective lamination over dark solid ink at the fold line.
- Interlocking Tab Bind or Loose Fit: Caused by failing to account for wrap paper and lamination thickness (+0.03–0.05 mm / +0.001–0.002 in film) inside the die-cut slot profile, or by breaching the 3–4 mm (0.118–0.157 in) die gap during cutting.
- Dual-Layer Recess Misalignment: Caused by artwork shifting relative to the top die-cut frame during lamination, or by placing critical well borders closer than 3 mm (0.118 in) to the cut edge.
- Wrap Corner Lift: Caused by a wrap margin narrower than 15 mm (0.591 in) or insufficient adhesive coverage at the mitered corners of 2.5–3.0 mm (0.098–0.118 in) greyboard.
- Dark-Ink Scuffing: Caused by shipping or rubbing unlaminated or standard-matte dark covers (high TAC near 280%–300%) without anti-scuff matte film.
- Box-Fit Interference: Caused by calculating box dimensions from nominal panel size without adding hinge-gap growth, wrap thickness, and the required 1.5–2.5 mm (0.059–0.098 in) side clearance.
Guides in this section
Parent guide Tabletop Game Component Manufacturing