Within the components production scope, board gauge, nick geometry, and slot width change based on part size and mechanical stress:
- Small tokens and counters run on 1.5–2.0 mm (0.059–0.079 in) greyboard so steel rules cut cleanly through tight curves without crushing narrow bridges.
- Map tiles, standees, and slot-together structures use 2.0–3.0 mm (0.079–0.118 in) greyboard for rigidity, requiring slot widths matched to the finished mounted caliper (greyboard plus face/back sheets and film).
- Riveted dials and multi-layer trackers combine 1.5–2.0 mm (0.059–0.079 in) layers so total stack height stays compact while keeping die-cut windows and center rivet holes concentric.
- Boxed game integration requires 1.5–2.5 mm (0.059–0.098 in) clearance across sheet width and height and 1.5–3 mm (0.059–0.118 in) for total stack height inside the box or insert.
Material and Dimensional Specifications
Tooling and production minimums follow project and component requirements. Paper weight comparisons use grams per square meter (gsm), distinguishing US Text LB (based on a 25 × 38 in / 635 × 965 mm sheet) from US Cover LB (based on a 20 × 26 in / 508 × 660 mm sheet) when specifying wrap or card stocks alongside mounted greyboard.
Greyboard Gauges and Component Applications
| Greyboard Gauge (mm) | Greyboard Gauge (in) | Wrap Margin | Primary Applications | Mechanical Trade-Off |
|---|---|---|---|---|
| 1.5 mm | 0.059 in | 15–20 mm (0.591–0.787 in) | Small tokens, dial layers, compact chits | Cuts cleanly on tight radii; lower bending stiffness on wide tiles |
| 2.0 mm | 0.079 in | 15–20 mm (0.591–0.787 in) | Standard tokens, tiles, light standees | Balances edge rigidity with clean steel-rule penetration |
| 2.5 mm | 0.098 in | 15–20 mm (0.591–0.787 in) | Heavy tiles, player boards, standees | Resists warping on larger spans; requires wider die spacing |
| 3.0 mm | 0.118 in | 15–20 mm (0.591–0.787 in) | Structural standees, slot-together terrain | Maximum rigidity; higher die pressure increases bevel at cut edges |
Die-Cut, Retention, and Assembly Tolerances
| Feature | Specification (mm) | Specification (in) | Physical Requirement |
|---|---|---|---|
| Die-cut gap between parts | 3–4 mm minimum | 0.118–0.157 in | Prevents steel-rule compression from crushing or delaminating the waste matrix |
| Bleed per side / per cut edge | 3 mm | 0.118 in | Extends artwork past every outer and inner cut line |
| Standard safety margin | ≥3 mm | ≥0.118 in | Keeps text and icons clear of edge bevel and registration shift |
| Bordered part safety margin | ≥4–5 mm | ≥0.157–0.197 in | Hides minor die-to-print shift on framed tiles and tokens |
| Double-sided film caliper | +0.03–0.05 mm | +0.001–0.002 in | Added to base sheet thickness when calculating slot fit and stack height |
| Box width/height clearance | 1.5–2.5 mm | 0.059–0.098 in | Allows full punchboard sheets to drop into the box without bowed corners |
| Box stack height clearance | 1.5–3 mm | 0.059–0.118 in | Accommodates sheet caliper stack-up and lid closure |
Prepress and Surface Finish Rules
- File formats and color: Supply print-ready AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 at ≥300 DPI in CMYK, with outlined or embedded fonts.
- Spot layers: Place all die-cut outlines, internal windows, slots, and rivet holes on dedicated spot layers set to overprint, separate from CMYK artwork.
- Ink density: Use 100% K for fine text, rich black C40–60 M30–40 Y30–40 K100 for solid black fills, and keep Total Area Coverage (TAC) at ≤280%–300% to prevent ink set-off during mounting and pressing.
- Surface coating: Use anti-scuff matte lamination on dark artwork to reduce rub marks during die-cutting and transit.
Production Steps and Sign-Off Criteria
Manufacturing Sequence
- Prepress and die-line engineering: Separate CMYK print layers from vector cut, slot, and hole paths. Verify 3 mm (0.118 in) bleed around every punch-out shape and 3–4 mm (0.118–0.157 in) spacing between adjacent parts.
- Sheet printing and lamination: Print face and back wraps offset in CMYK, apply protective film or varnish, and verify ink cure before mounting.
- Greyboard mounting and wrapping: Laminate printed sheets onto the specified greyboard gauge using a 15–20 mm (0.591–0.787 in) wrap margin where edges fold over, then press flat to stabilize moisture and prevent curl.
- Steel-rule die-cutting and nicking: Cut mounted sheets with custom steel-rule dies. Leave small physical nicks (unbroken tabs along the cut line) positioned on straight edges or low-detail areas so parts stay locked in the waste matrix during packing.
- Riveting and dial assembly: Punch center holes through stacked dial faces and backboards, insert metal or plastic rivets, and set tension so layers rotate smoothly without wobble.
- Sorting and box packing: Stack finished punchboard sheets with 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3 mm (0.059–0.118 in) height clearance inside the game box.
Sign-Off Criteria
- Retention vs. release: Parts remain seated in the sheet when shaken or stacked in transit, then pop out with thumb pressure without tearing the printed face paper or leaving oversized burrs.
- Irregular die-cut alignment: Custom silhouettes, interior windows, and bordered tiles maintain visual centering within the ≥3 mm (0.118 in) standard or ≥4–5 mm (0.157–0.197 in) bordered safety zone.
- Slot-together fit: Interlocking tabs and standee bases seat firmly into slots without forcing, bowing the slot walls, or splitting the greyboard plies.
- Concentric dial alignment: Multi-layer dials rotate smoothly around the rivet axis with indicator windows framing the underlying values cleanly across a full 360-degree turn.
- Compliance documentation: Where small punch-out tokens or child-oriented components require regulatory assessment, record age-grade and small-parts testing under the European Commission Toy Safety (EN 71) framework alongside applicable packaging registration records such as LUCID / VerpackG and Triman info-tri.
Concrete Failure Modes
- Crushed or delaminated waste bridges: Placing cut lines closer than 3–4 mm (0.118–0.157 in) compresses the narrow strip of greyboard between steel rules, causing edges to flake or collapse before punch-out.
- Torn artwork during punch-out: Oversized nicks, too many nicks on small tokens, or nicks placed across sharp corners or fine text pull the laminated face sheet away from the greyboard core when removed.
- Loose or split slot-together joints: Designing slot widths around nominal greyboard thickness without accounting for mounted wrap paper and 0.03–0.05 mm (0.001–0.002 in) double-sided film causes parts either to jam and split the board edge or to wobble loosely.
- Eccentric dial windows and binding rivets: Registration drift between the print sheet, window cutout, and center rivet hole clips text inside dial apertures or causes layers to rub against the outer edge of the backing board.
- White edge slivers and off-center borders: Omitting the 3 mm (0.118 in) bleed around internal die cuts or placing borders inside the 4–5 mm (0.157–0.197 in) safety zone exposes unprinted paper along beveled cut edges.