Both formats sit within the broader family of booklet and paper structures, but they behave like consumable tabletop boards rather than bound books. The production choice depends on sheet count, double-sided vs. single-sided writing, whether players write in-hand or on the table, and the available cavity height inside the game box.


Material and Structural Specifications

Sheet Stock and Basis Weight

Writing sheets require uncoated paper so pencil, ballpoint pen, and fine-liner ink absorb cleanly without smearing.

  • Interior writing stock: 80–120 gsm uncoated offset paper, measuring approximately 0.08–0.13 mm (0.003–0.005 in) per sheet. In US paper sizing, this corresponds to roughly 54–81 lb Text based on a 25 × 38 in (635 × 965 mm) basis sheet.
  • Single-sided vs. double-sided sheets: Use 80–100 gsm (54–68 lb Text) for single-sided scorepads. Step up to 100–120 gsm (68–81 lb Text) for double-sided campaign trackers to reduce ink show-through.
  • Optional top cover sheet: When a pad includes a protective front cover, use 200–300 gsm stock—roughly 74–111 lb Cover based on a 20 × 26 in (508 × 660 mm) basis sheet—scored at the head edge so it folds back cleanly during play.

Backing Board and Head-Edge Binding

  • Rigid backing board: Pair the sheet stack with greyboard or chipboard at 1.5 mm (0.059 in), 2.0 mm (0.079 in), 2.5 mm (0.098 in), or 3.0 mm (0.118 in). Use 1.5 mm (0.059 in) for compact table-rested scorepads and 2.0–3.0 mm (0.079–0.118 in) for large pads or pads held in one hand while writing.
  • Head padding glue: Clean-release EVA/PVA padding compound applied to the top edge. For thick pads (over 80–100 sheets), add a backing strip of cheesecloth or crash beneath the glue coat to prevent the stack from splitting.
  • Stapled perforations: Two or more wire staples driven through a top stub above a micro-perforation line. Keep the staple stub at least 10–12 mm (0.394–0.472 in) tall so the perforation sits clear of the staple clinch.

Prepress and Box-Fit Tolerances

  • File format and color: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 in CMYK with separate spot layers if needed, at ≥300 DPI, with all fonts outlined or embedded.

  • Black ink and ink limits: Set fine grid lines, checkboxes, and small score numbers in 100% K only to prevent multi-plate registration blur. Use rich black (C40–60 M30–40 Y30–40 K100) only for heavy solid fills, and keep Total Area Coverage (TAC) at ≤280%–300%.

  • Bleed and safety margins: Add 3 mm (0.118 in) bleed per side. Keep all live text, score boxes, and writing lines ≥3 mm (0.118 in) inside trim edges and ≥3 mm (0.118 in) below any glue line or perforation line.

  • Stack thickness and box clearance: Calculate finished pad thickness before locking sheet counts against a box cavity:

    Total pad thickness = (Sheet count × Single-sheet caliper) + Backing board thickness + Cover thickness

    Leave 1.5–2.5 mm (0.059–0.098 in) clearance across the box cavity width and height, and 1.5–3 mm (0.059–0.118 in) clearance for stack height. Boxed games and custom tooling follow project and component minimums set with specialist offset and tabletop manufacturing partners.


Production Steps

  1. Sheet imposition and offset printing: Impose single-design or multi-design sheets on uncoated offset stock with paper grain running parallel to the bound head edge so sheets lie flat and resist edge curl. Print 100% K rules and low-TAC fills, then allow ink to set before stacking.
  2. Collation and jogging: For multi-design campaign pads with rotating or numbered sheets, collate pages in exact play sequence. Jog the sheet stack flush to the head edge so every sheet sits even with the binding plane.
  3. Backing board pairing and clamping: Place the trimmed greyboard or chipboard backing under each stack (plus any optional top cover). Clamp stacks together under even hydraulic pressure along the head edge to eliminate air gaps between sheets.
  4. Head-edge binding or perforation and stitching:
    • Glued pads: Brush or roll padding compound across the clamped head edge in even coats, let cure completely, and slice individual pads apart along the backing-board boundaries.
    • Stapled pads: Micro-perforate sheets offline or inline, collate onto the backing board, and drive wire staples through the top stub above the perforation line.
  5. Final three-side trim and pack-out: Guillotine-trim the remaining three edges after adhesive cure or stitching so all sheet edges align flush with the backing board. Shrink-wrap or band pads in small bundles, keeping master shipping cartons within safe handling limits (typically under 15 kg / 33.1 lb) to prevent crushed corners.

Sign-Off Criteria

  • Clean sheet release: A single sheet peels away from a glued head edge or tears along a stapled perforation without lifting the sheet underneath, tearing into the grid, or leaving tacky residue on the writing face.
  • Staple and perforation alignment: On stapled pads, staples sit squarely within the top stub and the micro-perforation runs parallel to the head edge, at least 3 mm (0.118 in) clear of live score fields.
  • Backing rigidity and flatness: The pad lies flat on a table without bowing, and the backing board does not flex excessively when held in one hand.
  • Print sharpness and writeability: 100% K grid lines and small numbers show no color fringing; pencil and ballpoint ink mark cleanly without skipping or bleeding through to the reverse side.
  • Box cavity fit: Finished width, height, and total stack thickness fall within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height box clearances.

Failure Modes

Failure Mode Physical Cause Production Outcome
Multi-sheet tearing or glue bleed Insufficient clamping pressure lets padding compound wick between sheets Peeling one sheet rips the top edge of the next sheet or fuses pages together
Premature sheet shedding Too little adhesive, un-jogged sheets, or dust on the clamped head edge Sheets detach in transit or mid-game before players intend to remove them
Torn score fields on stapled pads Score grids placed closer than 3 mm (0.118 in) to the perforation line, or overly coarse perforation teeth Sheets dog-ear or rip straight through active checkboxes and point columns
Ink smearing and show-through Coated stock specified for scorepads, or 80 gsm (54 lb Text) used for heavy double-sided ink coverage Pen ink smudges on the surface or bleeds through to obscure the back-side tracker
Box lid lift or jammed insert Stack height calculated from sheet count alone without adding 1.5–3 mm (0.059–0.118 in) backing board and clearance Pads bow inside the tray or prevent the game box lid from closing flush
Pad curl after trimming Paper grain or backing board grain oriented perpendicular to the head edge in humid storage Sheets lift away from the backing board along the unbound bottom edge