Switch to another binding when the pad faces heavy handling in a loose bag before play, when sheets are printed on coated cover stock that resists PVA penetration, or when players need a stub to remain bound for record-keeping.
Specifications and Material Choices
| Component / Parameter | Typical Specification | Production Notes |
|---|---|---|
| Sheet stock | 80–120 gsm (about 0.08–0.13 mm / 0.003–0.005 in per sheet) | Uncoated offset paper accepts pen and pencil cleanly and absorbs PVA at the head edge. |
| Weight basis distinction | US Text LB (25 × 38 in / 635 × 965 mm) vs. US Cover LB (20 × 26 in / 508 × 660 mm) | Always specify gsm alongside Text LB; an 80 lb Text sheet is far lighter than an 80 lb Cover board. |
| Chipboard backer | 1.5–2.0 mm (0.059–0.079 in) greyboard/chipboard, or 200–300 gsm cover backer | 1.5–2.0 mm board gives handheld rigidity during scoring; thin cover stock suits pads resting inside a rigid game box. |
| Head-edge adhesive | Flexible PVA padding compound | Remains pliable after curing so sheets flex upward and release from the glue film without tearing. |
| Bleed and safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety margin | Keep score boxes, headers, and fine 100% K text clear of the head-edge glue line and three trimmed edges. |
| Box fit clearance | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height | Account for total pad caliper when sizing the surrounding game box or tray cavity. |
Total pad thickness follows a simple stack calculation:
Pad thickness (mm) = (Sheet count × Sheet caliper in mm) + Backer caliper in mm + 0.1–0.2 mm glue film
Prepress files use AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 at ≥300 DPI in CMYK (with separate spot layers if needed), outlined or embedded fonts, 100% K for fine grid lines and text, rich black (C40–60 M30–40 Y30–40 K100) only for heavy solids, and total area coverage (TAC) ≤280%–300%. Because scorepad trim dimensions vary by box cavity and table footprint, size the sheet footprint to match the game's insert or box clearance rather than forcing a standard card trim. Project minimums follow the broader boxed-game or component run rather than the 200-deck card tier.
Production Steps
- Print and condition sheets: Run the uncoated scorepad sheets in CMYK, allowing ink to dry flat so moisture imbalance does not curl the stack before jogging.
- Collate with backers: Place the chipboard or heavy cover backer at the bottom of each sheet count, matching the exact pad count per unit.
- Jog and clamp the head edge: Vibrate-jog stacks against a square fence so all head edges sit flush, then clamp under even downward pressure with a rigid weighting block or hydraulic clamp. Unaligned sheets create stepped recesses where PVA cannot bridge.
- Apply flexible PVA padding compound: Brush or roller-coat two thin, even passes of flexible PVA along the clamped head edge, allowing the first coat to tack before applying the second. Avoid pooling compound onto the face of the top sheet or past the side corners.
- Cure and separate pads: Air-dry clamped stacks until the PVA turns clear and flexible, then slice between backers with a sharp padding knife to separate individual pads cleanly without pulling fibers from the bottom sheet.
- Three-side trim (when run multi-up): Guillotine-trim the foot, left, and right edges after padding—or trim before padding with a final micro-skim—keeping the padded head edge untouched so the glue film remains intact.
- Pack for transit: Shrink-wrap or band pads in tight bundles and pack cartons under 10–15 kg (22–33 lb) with snug dunnage so shifting stacks do not shear the glued head edge during shipping.
Sign-Off Criteria
- Clean peel-force balance: Lifting a sheet from a bottom corner at a steady angle releases the sheet smoothly at the head edge without tearing the sheet margin, lifting the next sheet, or leaving a paper stub.
- Intact glue spine: The cured PVA film flexes without cracking when the pad is bent slightly, and holds the remaining stack together when held upside down by the last sheet.
- Backer stiffness and flatness: The chipboard backer supports writing on a lap or uneven table without bowing, and the pad lies flat with zero corner curl.
- Registration and clearance: Grid lines and headers sit inside the ≥3 mm (0.118 in) safety margin, and finished pad dimensions fit the target box cavity within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) height clearances.
Failure Modes
- Transit edge-splitting: Heavy cartons, loose void fill, or brittle glue formulations cause pads to split mid-stack along the head edge under vibration or drop impact. Prevent this by using flexible PVA, shrink-wrapping pads tightly in small bundles, and limiting carton weight.
- Sheet tearing and stubbing (over-gluing): Applying rigid bookbinding adhesive or flooding excessive PVA onto porous uncoated stock wicks compound 1–2 mm (0.039–0.079 in) between sheets, causing the paper to tear across the top line instead of peeling cleanly.
- Premature sheet detachment (under-gluing or poor jogging): Starved glue coats, single-pass application, or recessed sheets from uneven jogging leave dry spots along the head edge so sheets fall loose during packing or first use.
- Curled or floppy pad base: Pairing a high sheet count with a thin cover backer instead of 1.5–2.0 mm (0.059–0.079 in) chipboard causes the pad to warp under ambient humidity changes and flex uncomfortably when held in one hand.
- Clipped headers at the head edge: Placing borders or titles closer than 3 mm (0.118 in) to the top edge traps ink under the glue film or exposes raw white paper edges if the stack is trimmed unevenly.
Parent guide Tear-Off Scorepads and Campaign Pads