Choosing between C1S and C2S SBS:
- C1S (Coated One Side): Pairs a smooth clay-coated outer print face with an uncoated, porous inner surface. Use C1S for standard tuck boxes and outer sleeves where graphics sit on the outside only and the side seam relies on fast, high-bond glue penetration into raw fibers.
- C2S (Coated Two Sides): Coats both faces for ink holdout inside and out. Use C2S for two-sided tuck boxes, interior-printed flaps, or reversible sleeves. Because both surfaces are sealed by coating, glue-flap zones require coating knockout or adhesives formulated for coated board.
- Caliper selection: Higher ordered caliper grades increase panel rigidity and crush resistance for heavier deck masses (kg/lb) or wider box spans, while requiring wider creasing channels and adjusted fold allowances to prevent outer-coating cracking.
Specifications and Physical Properties
| Property | C1S SBS | C2S SBS | Production Impact |
|---|---|---|---|
| Core & Edge | Bleached virgin pulp | Bleached virgin pulp | Clean white die-cut and scored edges with no grey or kraft fiber show-through |
| Print Surface | Coated outer face only | Coated outer and inner faces | High ink holdout for CMYK, separate spot layers, and dense rich black |
| Glue-Flap Bond | Uncoated inner back | Coated inner back | C1S accepts standard cold glue directly; C2S requires glue-area varnish/coating knockout or specialized adhesive |
| Basis Weight Convention | Specified in gsm and Cover LB | Specified in gsm and Cover LB | US Cover LB uses a 20 × 26 in (508 × 660 mm) basis sheet; US Text LB uses a 25 × 38 in (635 × 965 mm) basis sheet |
| Minimums & Tooling | Project/component minimums | Project/component minimums | Tuck boxes and sleeves require custom dielines and cutting/creasing tooling |
Prepress and Structural Tolerances
- File & Color Setup: Supply AI, PDF, or PSD files in PDF/X-1a or PDF/X-4 at ≥300 DPI with outlined or embedded fonts. Use CMYK with separate spot layers, 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and Total Area Coverage (TAC) ≤280%–300%.
- Bleed & Safety: Provide 3 mm (0.118 in) bleed per side and ≥3 mm (0.118 in) safety margin from all cut and score lines.
- Surface Protection: Anti-scuff matte lamination suits dark artwork on SBS tuck boxes and sleeves, preventing rub marks during handling and transit.
- Box Clearance: Size tuck and sleeve dielines with 1.5–2.5 mm (0.059–0.098 in) clearance across width and height, and 1.5–3 mm (0.059–0.118 in) clearance for stack height. Account for actual deck stack thickness, including double-sided card film lamination that adds 0.03–0.05 mm (0.001–0.002 in) per card.
Production Steps
- Stock and Grain Matching: Select C1S or C2S in an ordered caliper grade matched to the total deck weight (kg/lb) and box dimensions. Orient board grain to balance panel stiffness against fold resistance along primary score lines.
- Dieline and Prepress Preparation: Place artwork on the approved tuck or sleeve dieline with 3 mm (0.118 in) bleed, ≥3 mm (0.118 in) safety margins, and varnish/lamination knockouts over the glue-flap zone (essential on C2S).
- Offset Printing and Finishing: Print CMYK and spot layers onto the coated face(s), allow ink curing, and apply aqueous coating or anti-scuff matte lamination before die-cutting.
- Creasing, Die-Cutting, and Gluing: Set creasing rule width and channel depth to the ordered caliper grade, die-cut thumb notches and tuck tabs cleanly, and fold-glue the side seam under compression until set.
Sign-Off Criteria
- Print & Ink Holdout: Solid fills and rich black panels exhibit uniform density without mottling; fine 100% K text is sharp with no ink spread.
- Cut & Crease Quality: Die-cut edges are clean white without feathering; 90-degree and 180-degree folds on tuck flaps and sleeve corners show intact coating with no fiber cracking.
- Fit & Clearance: The finished deck inserts and slides out smoothly within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack height allowances without bowing the box walls.
- Seam Integrity: Glued side seams hold under normal tuck-flap opening force and full deck mass (kg/lb).
Concrete Failure Modes
- Score Cracking on Heavy Ink: Exceeding TAC ≤280%–300% or folding high-caliper SBS over an undersized crease channel fractures the clay coating along the spine, exposing white fibers. Keep TAC within limits, apply anti-scuff matte film, and match crease tooling to the ordered caliper.
- Glue-Seam Pop-Open on C2S: Applying standard glue over a coated or varnished inner flap prevents fiber penetration, causing sleeve or tuck seams to split. Knock out coating/varnish in the glue zone and pair the adhesive to C2S.
- Scuffing on Dark Artwork: Unprotected dark CMYK or rich black surfaces abrade against adjacent cartons during transit. Use anti-scuff matte lamination or protective coating.
- Tight Sleeve Fit or Tuck Bulging: Failing to include card film thickness (0.03–0.05 mm / 0.001–0.002 in per card) or reducing clearances below 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack height causes binding and distorted box panels.
- Fuzzy Die-Cut Edges: Worn cutting rules or improper makeready pressure crush the bleached core rather than shearing it cleanly, leaving frayed white edges on thumb notches and closure tabs.
Parent guide Folding Carton Paperboard for Card Boxes