Core Material Specifications

Card Deck Press produces custom boxes with specialist offset and tabletop manufacturing partners. While standard offset card runs start at 200 decks (typical tiers of 200, 300, 500, and 1,000+), boxed games and custom box tooling follow project and component minimums.

Material Layer Standard Options & Calipers Basis Weight & Sizing Notes Best-Fit Application
Folding paperboard Single-ply coated board (typically 200–300 gsm+ cover grades) Specified in gsm or US Cover LB (20 × 26 in / 508 × 660 mm basis sheet) Lightweight tuck boxes, inner dividers, booster outer sleeves
Rigid greyboard core 1.5 / 2.0 / 2.5 / 3.0 mm (0.059 / 0.079 / 0.098 / 0.118 in) Selected by box span and total load in kg (lb) Two-piece lid-and-base boxes, magnetic clamshells, heavy board game boxes
Wrap paper & inner liner Thin coated art paper (typically 80–120 gsm; ~0.08–0.13 mm / 0.003–0.005 in per sheet) Distinguish US Text LB (25 × 38 in / 635 × 965 mm) from US Cover LB (20 × 26 in / 508 × 660 mm); requires 15–20 mm (0.591–0.787 in) wrap margin Exterior printed wrap and balanced interior lining on rigid greyboard
Clear plastics Transparent window film or 0.30 mm (0.012 in) rigid PVC sheet Rigid clear sheet holds form without a paperboard core Die-cut box windows, clear two-piece cases, retail slipcases
Closure hardware Concealed magnets, ribbon pulls, friction-fit steps, tuck tabs Recessed into greyboard cavities or die-cut directly into paperboard Magnetic book-style boxes, heavy-lid lift assists, standard tuck closures

Paperboard vs. Rigid Greyboard

  • Folding paperboard scores and folds in a single pass. It suits compact decks where total contents weight stays low in kg (lb) and the box relies on tight internal geometry rather than wall thickness.
  • Rigid greyboard provides compression resistance against stacking loads in transit. Use 1.5 mm (0.059 in) or 2.0 mm (0.079 in) greyboard for compact card boxes, and step up to 2.5 mm (0.098 in) or 3.0 mm (0.118 in) for large game boxes, wide lids, or heavy multi-component sets.

Wrap Papers, Grain Direction, and Basis Weight

  • Grain orientation: Align wrap paper grain parallel to the primary spine or long fold axis so the sheet wraps cleanly around 90-degree greyboard edges without cracking.
  • Wrap margin: Leave a 15–20 mm (0.591–0.787 in) turn-in margin around all outer edges of the rigid board flat so the wrap anchors securely inside the box walls.
  • Basis weight distinction: Always verify paper weight in gsm alongside US basis weights. US Text LB is measured on a 25 × 38 in (635 × 965 mm) basis sheet, whereas US Cover LB is measured on a 20 × 26 in (508 × 660 mm) basis sheet; identical pound numbers represent very different sheet thicknesses.
  • Surface finish: Pair dark, ink-heavy box wraps with an anti-scuff matte lamination to prevent rub marks during packing and handling.

Clear Plastics and Closure Hardware

  • Clear windows and sleeves: Thin clear films bond behind die-cut paperboard or wrapped greyboard apertures to display card backs. Full clear plastic boxes use rigid sheet stock such as 0.30 mm (0.012 in) PVC scored along fold lines.
  • Hardware integration: Concealed magnets sit inside routed recesses within 2.0–3.0 mm (0.079–0.118 in) greyboard walls before the wrap paper and inner liner are applied. Ribbon pulls anchor beneath the inner tray liner so the pull tab does not tear free under deck weight.

Clearance and Stack Fit Tolerances

Box internal dimensions must account for the finished deck caliper—including any 0.03–0.05 mm (0.001–0.002 in) added per card by double-sided lamination—plus operational clearance:

  • Width and height clearance: 1.5–2.5 mm (0.059–0.098 in) total clearance across internal width and height.
  • Stack height clearance: 1.5–3.0 mm (0.059–0.118 in) clearance above the card stack height (for example, when housing 300 gsm art/blue-core cards at 0.28–0.31 mm / 0.011–0.012 in, 310 gsm black-core linen at 0.30–0.32 mm / 0.012–0.013 in, 330 gsm black core at 0.32–0.34 mm / 0.013 in, 350 gsm art stock at 0.34–0.38 mm / 0.013–0.015 in, 400 gsm at 0.40–0.44 mm / 0.016–0.017 in, or 0.30 mm / 0.012 in PVC).

Plain-text cavity sizing formula: Internal Cavity Dimension = Finished Component Stack Dimension + Box Clearance (1.5–2.5 mm X/Y or 1.5–3.0 mm Z)

Production Steps

  1. Prepress and Die-Line Setup: Build box wraps and folding cartons in AI, PDF, or PSD, exported as PDF/X-1a or PDF/X-4 at ≥300 DPI with outlined or embedded fonts. Include 3 mm (0.118 in) bleed per side and keep critical text and logos inside ≥3 mm (0.118 in) safety margins. Use CMYK with separate spot layers for foil or UV, 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for large dark areas, and keep total area coverage (TAC) at ≤280%–300%.
  2. Core Cutting and Grooving: Die-cut folding paperboard with crease rules, or die-cut and V-groove rigid greyboard (1.5–3.0 mm / 0.059–0.118 in) to create crisp 90-degree corners. Route magnet pockets if using magnetic closures.
  3. Printing and Surface Lamination: Offset print the folding carton or exterior wrap sheet, cure inks, and apply anti-scuff matte or protective film before die-cutting or wrapping.
  4. Wrapping, Window Patching, and Hardware Assembly: Bond clear window film over apertures, seat magnets or ribbon pulls, and wrap the printed paper around the rigid core with a 15–20 mm (0.591–0.787 in) turn-in. Apply a balanced inner liner to counteract moisture pull.
  5. Curing and Fit Check: Press finished rigid boxes flat or in jigs until adhesive moisture equalizes, then test-load the actual laminated deck or game components.

Sign-Off Criteria

  • Structural rigidity: Box walls resist bowing under expected stack weight in kg (lb) and corner seams meet cleanly at 90 degrees without exposed greyboard.
  • Wrap adhesion and grain: Wrap paper lies flat across all panels with no edge lift along the 15–20 mm (0.591–0.787 in) turn-ins and no fiber cracking along scored folds.
  • Component fit: Finished cards and inserts slide in smoothly within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3.0 mm (0.059–0.118 in) stack height clearances without forcing or excessive rattle.
  • Print and finish: Ink coverage stays within TAC ≤280%–300%, fine text prints cleanly in 100% K, and dark wraps show no scuffing after handling.

Failure Modes

  • Panel warp (bowing lids or bases): Caused by gluing a damp printed wrap to one side of rigid greyboard without a grain-matched, balanced inner liner.
  • Corner crush and split wraps: Caused by pairing heavy decks in kg (lb) with under-spec greyboard (below 2.0 mm / 0.079 in on wide spans) or running wrap paper cross-grain over tight 90-degree folds.
  • Turn-in edge lift: Caused by an insufficient wrap margin (under 15 mm / 0.591 in) or weak adhesive bond against unprimed laminated edges.
  • Crushed card corners or stuck lids: Caused by calculating box depth from raw card gsm without adding 0.03–0.05 mm (0.001–0.002 in) per card for double-sided film and the required 1.5–3.0 mm (0.059–0.118 in) stack clearance.
  • Ink cracking and scuffing on folds: Caused by exceeding 300% TAC on score lines or omitting anti-scuff matte lamination on dark solid wraps.

Regulatory and Packaging Compliance Records

When boxes or packaged games enter regulated consumer markets, maintain material declarations, test reports, and packaging weight records in kg (lb) aligned with the destination market's official procedures:

  • Toy safety assessment (EU): If the boxed card or tabletop game is intended for children's play, follow applicable EU Toy Safety / EN 71 assessment and testing procedures and retain laboratory test records for paperboard, inks, coatings, and closure hardware.
  • Packaging producer registration (Germany): For boxed products placed on the German market, record packaging material weights and complete German Packaging Act (VerpackG / LUCID) data reporting.
  • Sorting and recycling markings (France): For household packaging sold in France, prepare artwork with the required French Triman sorting information based on the box's paperboard, plastic window, and hardware material split.