Stocks lighter than 128 gsm tear more easily under wet-glue tension and show underlying greyboard texture or adhesive strike-through, while stocks heavier than 157 gsm resist tight 90-degree bends and pull away from corner turn-ins. For full board and lining pairings, see Rigid Box Materials.
Conditions That Shift the Stock Choice
- 90-degree V-grooved corners: Sharp V-grooved greyboard walls require a pliable 128 to 157 gsm sheet with film lamination to bridge the outer score line without cracking the paper fibers or ink layer.
- Greyboard thickness: Thicker boards—2.5 mm (0.098 in) and 3 mm (0.118 in) compared with 1.5 mm (0.059 in) or 2 mm (0.079 in)—increase the outer wrap radius and require the full 15 to 20 mm (0.59 to 0.79 in) turn-in margin to anchor the sheet inside the box wall.
- Dark or heavy ink coverage: Dense solids and rich blacks require anti-scuff matte lamination so wrapping rollers and board edges do not burnish or scratch the printed face.
- Boxed game minimums: Rigid box wrapping and custom die tooling follow project and component minimums rather than the 200-deck starting tier used for standard offset cards.
Specifications
| Parameter | Specification | Notes |
|---|---|---|
| Wrap paper weight | 128–157 gsm | Sits in the US Text LB range (25 × 38 in / 635 × 965 mm basis sheet), distinct from heavier US Cover LB stocks (20 × 26 in / 508 × 660 mm basis sheet) |
| Greyboard core pairings | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) | Selected by box size and load; see Rigid Box Materials |
| Wrap turn-in margin | 15–20 mm (0.59–0.79 in) | Wraps over the board edge onto the interior face |
| Surface lamination | Anti-scuff matte or standard film | Reinforces 90-degree folds and protects dark artwork |
| Color & resolution | CMYK + separate spot layers, ≥300 DPI | Files supplied as AI, PDF, or PSD in PDF/X-1a or PDF/X-4 |
| Bleed & safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety | Keep critical elements clear of fold lines and turn-ins |
| Black & ink limits | 100% K fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% | Prevents ink cracking at folds and drying delays before lamination |
| Box fit clearance | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height | Accounts for wrapped wall buildup around internal contents |
Basis Weight Distinction
US Text LB and US Cover LB use different basis sheet sizes, so a pound rating alone does not specify sheet thickness or stiffness. Text weights are measured on a 25 × 38 in (635 × 965 mm) basis sheet, whereas Cover weights are measured on a 20 × 26 in (508 × 660 mm) basis sheet. Exterior rigid box wraps fall in the 128 to 157 gsm Text range rather than Cover stocks, which are too stiff to fold cleanly into 15 to 20 mm (0.59 to 0.79 in) turn-ins.
Production Steps
- Prepress and sheet offset printing: Set up artwork in PDF/X-1a or PDF/X-4 with outlined or embedded fonts, ≥300 DPI raster images, 3 mm (0.118 in) bleed per side, and ≥3 mm (0.118 in) safety from score and fold lines. Print the wrap sheet with specialist offset and tabletop manufacturing partners using CMYK and separate spot layers within the 280%–300% TAC limit.
- Surface finishing: Apply film lamination—using anti-scuff matte for dark solids—before die-cutting the wrap so the film reinforces the paper surface during folding.
- Wrap die-cutting: Cut the printed wrap sheet with corner reliefs sized to match the greyboard thickness and the 15 to 20 mm (0.59 to 0.79 in) turn-in depth.
- Board preparation: Cut and V-groove the 1.5 to 3 mm (0.059 to 0.118 in) greyboard flat, then fold the walls into a 90-degree shell.
- Gluing and wrapping: Apply a controlled, even adhesive film to the back of the wrap paper, register the greyboard shell to the sheet, press the side panels, and fold the 15 to 20 mm (0.59 to 0.79 in) turn-ins smoothly around the corners and over the top edges.
- Pressing and curing: Clamp or press the wrapped shell until adhesive moisture dissipates and the wrap bonds flat to the board without edge lift or panel bow.
Sign-Off Criteria
- 90-degree fold integrity: Exterior corners and V-grooved edges show continuous paper and lamination contact with zero fiber splitting, ink cracking, or white crease lines.
- Corner and turn-in bond: All four corners sit tight against the board with no dog-earing, and the 15 to 20 mm (0.59 to 0.79 in) interior turn-ins adhere flat from edge to edge.
- Surface flatness and cleanliness: No adhesive bleed-through, blistering, or rippling across flat panels, and no roller scuffing on dark solids.
- Graphic registration: Artwork aligns to the box faces within the ≥3 mm (0.118 in) safety zone without unintended wrap-around onto adjacent walls.
Failure Modes
- Corner splitting or white cracking: Caused by using wrap paper heavier than 157 gsm, omitting film lamination over heavy ink coverage, or folding across stiff grain over sharp V-grooves.
- Glue penetration and blistering: Caused by excessive adhesive volume or using paper lighter than 128 gsm, allowing moisture to soak through the sheet, soften fibers, and create ripples or dark blotches on the printed face.
- Turn-in edge lifting: Caused by turn-in margins narrower than 15 mm (0.59 in), insufficient pressing time, or spring-back from overly stiff paper resisting the 180-degree wrap over the board rim.
- Surface scuffing and burnishing: Caused by wrapping dark CMYK or rich-black solids without anti-scuff matte lamination, leaving shiny tracks where forming brushes and rollers press the corners.
- Panel warping after cure: Caused by unbalanced moisture expansion when wet glue pulls unevenly on the wrap sheet before the greyboard core stabilizes.
Guides in this section
Parent guide Card Box and Game Box Materials