Choose a five-sided rigid slipcase when a multi-deck set or card-and-book bundle needs a closed rear spine for shelf display and a single front opening for slide-out access. Compared with an open-ended sleeve box, the closed fifth wall prevents inner boxes from pushing out the back and keeps wide sets square under handling. Switch to thicker greyboard as total set weight (kg/lb) and cavity span increase, and size the opening clearances from the measured finished tuck boxes or bound books rather than unmounted card dimensions.

Wall Construction and Material Specifications

A five-sided slipcase uses rigid greyboard panels joined at 90 degrees across the top, bottom, two sides, and rear wall, leaving the front face open.

  • Greyboard core thickness: 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in). Light two-deck sets can use 1.5–2 mm (0.059–0.079 in) board; wider multi-deck sets and heavy book-plus-deck bundles (higher total kg/lb mass) require 2.5–3 mm (0.098–0.118 in) walls so the top and bottom panels do not bow inward.
  • Wrap margin and liner: The outer printed paper wrap folds over the open front lip and thumb notches with a 15–20 mm (0.591–0.787 in) turn-in margin, and an interior liner sheet covers the raw greyboard walls.
  • Paper weight basis: Specify wrap and liner stocks in gsm. When referencing North American weights, distinguish US Text LB (25 x 38 in / 635 x 965 mm basis sheet) from US Cover LB (20 x 26 in / 508 x 660 mm basis sheet) because identical LB numbers represent different sheet thicknesses and gsm values.
  • Protective finish: Anti-scuff matte lamination suits dark artwork across large exterior panels and exposed front edges.
  • Minimums: Custom slipcase tooling and boxed components follow project and component minimums, while standard offset card decks inside the set start at 200 decks (usual tiers 200/300/500/1,000+).
Specification Target Range Production Role
Greyboard thickness 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) Controls wall rigidity and prevents span bowing
Wrap turn-in margin 15–20 mm (0.591–0.787 in) Anchors outer wrap inside the open front face
Width and height clearance 1.5–2.5 mm (0.059–0.098 in) Prevents side-wall binding across grouped items
Stack or depth clearance 1.5–3 mm (0.059–0.118 in) Absorbs cumulative tuck-box or book thickness variance
Exterior bleed 3 mm (0.118 in) per side Covers trim and wrap-edge registration
Artwork safety >= 3 mm (0.118 in) Keeps type and borders clear of creases and thumb notches

Opening Constraints, Clearances, and Thumb Notches

Multi-unit cavities accumulate thickness variance across every enclosed tuck box or book, so internal dimensions must be calculated from the full loaded group:

Internal Width  = Sum of enclosed box or book widths + 1.5 to 2.5 mm (0.059 to 0.098 in)
Internal Height = Max enclosed box or book height + 1.5 to 2.5 mm (0.059 to 0.098 in)
Internal Depth  = Max enclosed box or book depth + 1.5 to 3 mm (0.059 to 0.118 in)
  • Inner deck and box measurement: Measure the finished, filled tuck boxes before locking the slipcase dieline. For non-standard deck formats, base the cavity on the physical loaded box and card stack rather than a default trim assumption.
  • Book-bundle allowances: When grouping a rulebook or guidebook alongside decks, account for bound spine swell. Interior book stock of 80–120 gsm adds about 0.08–0.13 mm (0.003–0.005 in) per sheet, paired with 200–300 gsm covers. Bound signatures run in multiples of four: saddle stitch for 12–40 pages, perfect binding for 28+ pages, and sewn binding recommended for 80–100+ pages.
  • Thumb-notch geometry: Die-cut matching semi-circular or U-shaped thumb notches into the open front edges of the top and bottom (or side) panels. Without front notches, flush-seated tuck boxes cannot be gripped individually and must be shaken out.
  • Notch wrap relief: Keep notch curves smooth enough for the 15–20 mm (0.591–0.787 in) wrap margin to fold cleanly into the cavity without wrinkling or exposing raw greyboard.

Prepress and Production Steps

  1. Confirm physical stack dimensions: Measure the assembled tuck boxes and any bound books together to lock the internal width, height, and depth clearances.
  2. Prepare print files: Supply AI, PDF, or PSD artwork exported as PDF/X-1a or PDF/X-4 at >= 300 DPI in CMYK with separate spot layers. Outline or embed all fonts, set fine text to 100% K, build rich black at C40–60 M30–40 Y30–40 K100, and keep total area coverage (TAC) at <= 280%–300%.
  3. Set bleed and safety around openings: Add 3 mm (0.118 in) bleed per side outside the 15–20 mm (0.591–0.787 in) wrap margin, and keep logos, rules, and text >= 3 mm (0.118 in) inside every 90-degree crease, rear spine edge, and thumb-notch curve.
  4. Cut and V-groove the greyboard: Mill or score the 1.5–3 mm (0.059–0.118 in) greyboard for crisp 90-degree corners, and die-cut the front thumb notches before wrapping.
  5. Print, laminate, and wrap: Print the outer sheet, apply anti-scuff matte lamination on dark designs, die-cut wrap relief tabs at the thumb notches, wrap the five-sided shell, and line the interior walls.

Sign-Off Criteria

Verify the white dummy and first printed sample against the following physical checks before full production:

  • Slide fit: Every tuck box or book slides in and out smoothly with 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) depth clearance—neither jamming against the front lip nor dropping out freely under light tilt.
  • Thumb-notch finish: Front cutouts align symmetrically, expose enough spine to grip a single box or book, and show continuous wrap coverage with zero split paper or raw greyboard edges.
  • Corner squareness and wrap adhesion: The closed rear wall holds 90-degree corners without racking, and the wrap sits flat along the spine and 15–20 mm (0.591–0.787 in) interior turn-ins.
  • Print and rub resistance: Fine text prints in clean 100% K, dark solids stay within TAC <= 280%–300%, and front-lip edges resist scuffing during repeated box insertion.

Failure Modes

  • Cumulative stack jam: Calculating cavity width from single-box nominal dimensions instead of the combined loaded group leaves insufficient clearance, forcing the last tuck box or book to bind or crush.
  • Unreachable flush boxes: Omitting front thumb notches or cutting them too shallow forces users to tip and shake the slipcase to remove inner decks.
  • Split wrap at the thumb notch: Tight notch radii or missing die-cut relief tabs prevent the 15–20 mm (0.591–0.787 in) wrap margin from seating smoothly, leaving torn paper or exposed greyboard along the grip edge.
  • Wall bowing on wide spans: Using 1.5 mm (0.059 in) greyboard on wide or heavy multi-deck sets (higher kg/lb load) lets the top and bottom walls sag inward, pinching the middle tuck boxes.
  • Edge scuffing on dark spines: Omitting anti-scuff matte lamination or exceeding 300% TAC causes visible ink rub along the open front lip and rear corners during transit and shelf handling.