The choice between a full-width wraparound sleeve and a narrower belly band changes with inner-box rigidity, surface friction, and handling weight:

  • Full-width wraparound sleeves cover most or all of the inner box length, distributing friction across four full panels so the sleeve resists skewing on heavier boxed games.
  • Belly bands leave the ends of the inner box exposed, lowering material cost and highlighting box texture, but have less contact area and slide off more easily if the inner box is heavy (e.g., 1.0 kg / 2.2 lb or more) or wrapped in low-friction film.
  • When to switch: If both the inner box and sleeve use smooth film lamination and the band cannot be tensioned tightly without bowing the side walls, add a thumb-notch or switch to a closed-end sleeve structure.

Specifications

Paperboard Stock and Weight

Select paperboard by gsm and US Cover LB (based on the 20 × 26 in / 508 × 660 mm Cover basis sheet, rather than the 25 × 38 in / 635 × 965 mm Text basis sheet used for interior 80–120 gsm / ~54–81 lb Text sheets):

Component Recommended Stock Approximate Caliper Basis Weight Distinction
Standard belly band 200–300 gsm art card 0.20–0.31 mm (0.008–0.012 in) ~74–111 lb Cover (20 × 26 in)
Rigid wraparound sleeve 350 gsm art stock 0.34–0.38 mm (0.013–0.015 in) ~129 lb Cover (20 × 26 in)
Heavy-duty structural sleeve 400 gsm art stock 0.40–0.44 mm (0.016–0.017 in) ~148 lb Cover (20 × 26 in)
Double-sided film lamination Matte or anti-scuff matte +0.03–0.05 mm (+0.001–0.002 in) Added total thickness

Dimensional Fit, Clearances, and Overlap

  • Inner box baseline: Rigid inner boxes built from 1.5, 2.0, 2.5, or 3.0 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard with wrapped paper have slight corner radiusing and surface thickness that must be measured on the finished wrapped box before finalizing the sleeve dieline.
  • Clearance vs. tension: Unlike slip-on two-piece lids that use 1.5–2.5 mm (0.059–0.098 in) total clearance across width and height, open-ended sleeves and belly bands rely on controlled friction. The internal sleeve perimeter should match the finished inner box perimeter plus only minimal assembly clearance (typically 0.5–1.0 mm / 0.020–0.039 in total across each axis, depending on stock stiffness and lamination).
  • Underside glue flap: 15–20 mm (0.591–0.787 in) overlap positioned on the bottom panel, hidden from the primary display face.
  • Flat dieline calculation (plain text): Flat Width = (2 × Inner Box Width) + (2 × Inner Box Height) + Axis Clearances + Fold Allowances + Glue Flap Overlap

Prepress and Finishing

  • File setup: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts.
  • Color and ink limits: CMYK with separate spot layers, ≥300 DPI raster artwork, 100% K for fine text, rich black C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) ≤280%–300%.
  • Bleed and safety: 3 mm (0.118 in) bleed per side on all exterior edges and the outer edge of the glue flap; keep critical text and logos ≥3 mm (0.118 in) away from trim lines and corner score lines.
  • Surface finish: Use anti-scuff matte lamination on dark artwork to prevent rub marks during shipping and retail handling. Leave the underside glue-flap bonding zone free of lamination or varnish (glue knock-out) so adhesive bonds directly to paper fibers.

Production Steps

  1. Dieline engineering and grain alignment: Align the paperboard grain parallel to the four corner score lines. Running grain parallel to the wrap axis lets the board bend cleanly around 90-degree corners with minimal spring-back.
  2. Offset printing and lamination: Print the flat press sheet, cure inks, and apply film lamination or coating. Verify the glue-flap strip remains uncoated.
  3. Die-cutting and creasing: Die-cut the outer perimeter and press four parallel crease rules at the panel boundaries. Match crease rule width and counter-channel depth to the exact caliper (0.28–0.44 mm / 0.011–0.017 in) so the outer printed liner stretches without cracking.
  4. Pre-folding, gluing, and compression: Pre-break the four corner scores on the folder-gluer, apply adhesive along the 15–20 mm (0.591–0.787 in) underside flap, fold closed, and hold under belt compression until the bond sets.
  5. Fit verification: Slide finished sleeves onto actual wrapped and laminated inner-box samples before bulk assembly.

Sign-Off Criteria

  • Corner fold integrity: All four 90-degree scores fold crisply with zero ink cracking or fiber splitting on the outer face.
  • Seam strength: The underside glue overlap lies flat with full edge-to-edge adhesion and no adhesive squeeze-out that could stick to the inner box.
  • Seated tension: The sleeve slides onto the inner box smoothly by hand without bowing the side panels or crushing box corners, and stays seated without slipping when the boxed unit is held vertically or inverted.
  • Prepress accuracy: Bleed extends 3 mm (0.118 in) past cut edges, and panel artwork centers cleanly between score lines without drifting onto adjacent faces.

Failure Modes

  • Sleeve slides off in handling or transit: Caused by excessive perimeter clearance, low-friction film-on-film contact between a laminated sleeve and a laminated inner box, or shallow corner scores that cause the panels to bow outward (spring-back) and lose contact pressure.
  • Binding, bowing, or crushed inner-box corners: Caused by omitting the 0.03–0.05 mm (0.001–0.002 in) double-sided lamination thickness or inner-box wrap thickness from the dieline calculation.
  • Cracked ink along corner scores: Caused by grain running perpendicular to the fold lines, heavy ink coverage exceeding 300% TAC across a score, or creasing 350–400 gsm (0.34–0.44 mm / 0.013–0.017 in) board without an anti-scuff matte film or proper channel depth.
  • Underside seam pops open: Caused by gluing directly over film lamination or UV coating without a glue knock-out, or insufficient compression time before releasing tension on stiff 400 gsm (0.40–0.44 mm / 0.016–0.017 in) board.
  • Panel artwork wraps around corners: Caused by failing to subtract board fold take-up across the four 90-degree bends when positioning spine or side-panel graphics.