Profile Geometry and Use Cases
| Profile | Lid Wall Coverage | Opening & Release Behavior | Best-Fit Layout | Key Trade-off |
|---|---|---|---|---|
| Full-Telescope | Covers 100% of base outer height | Slow, damped air release; often needs thumb notches on tall, tight boxes | Flat boxed games, multi-layer inserts, heavy component loads | Maximum double-wall crush resistance, but hardest to grip if walls are flush-wrapped |
| Partial-Telescope | Covers ~50%–75% of base outer height | Exposes base tray below the lid rim for direct finger grip | Standard card-deck boxes, lighter tabletop sets, quick-open retail boxes | Faster opening without thumb notches, but leaves the lower base wall single-ply |
| Shoulder-Neck | Lid meets base flush against an inner collar | Controlled friction fit on the exposed neck step; clean flush exterior seam | Upright collector decks, premium rigid sets requiring an aligned exterior graphic | Flush outer wall alignment, but adds a third greyboard collar and tighter assembly tolerances |
- Flat game layouts vs. upright card decks: Flat layouts distribute component weight across a large base area, so lid friction is governed mainly by perimeter length and wall parallelism. Upright card decks stack cards vertically or edge-on, placing concentrated lateral pressure on the base walls and increasing height-to-footprint ratios; these require thicker greyboard or an internal divider/insert to keep walls from bowing outward and binding the lid.
Specifications and Clearances
Boxed games and custom box tooling follow project and component minimums rather than the 200-deck starting tier used for standard offset card decks.
Board, Paper, and Structural Tolerances
- Greyboard thickness: 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in). Use 1.5–2 mm (0.059–0.079 in) for compact single-deck or light card boxes under ~0.5 kg (1.1 lb), and 2.5–3 mm (0.098–0.118 in) for large flat game boxes or dense upright multi-deck loads exceeding ~1.5–2 kg (3.3–4.4 lb).
- Wrap paper stock: Typically 128–157 gsm coated art paper or specialty textured paper. Always specify paper by gsm; when referencing US basis weights, distinguish US Text LB (weighed on a 25 × 38 in / 635 × 965 mm basis sheet) from US Cover LB (weighed on a 20 × 26 in / 508 × 660 mm basis sheet), as the same pound number represents a much lighter sheet in Text than in Cover.
- Wrap turn-in margin: 15–20 mm (0.591–0.787 in) folded over the top rim of the lid and base greyboard walls for secure interior adhesion.
- Internal component clearance: 1.5–2.5 mm (0.059–0.098 in) across internal width and length/height, and 1.5–3 mm (0.059–0.118 in) for internal stack height above the top card, board, or insert.
- Lid-to-base sizing formulas (plain text):
Base Inner Width = Component Width + 1.5 to 2.5 mm (0.059 to 0.098 in)Base Inner Length = Component Length + 1.5 to 2.5 mm (0.059 to 0.098 in)Base Inner Height = Component Stack Height + 1.5 to 3 mm (0.059 to 0.118 in)Base Outer Width = Base Inner Width + (2 * Base Greyboard Thickness) + (2 * Wrap Paper Thickness)Lid Inner Width = Base Outer Width + Lid-to-Base Fit Clearance (typically 0.5 to 1.0 mm / 0.020 to 0.039 in total, adjusted for lamination)- For shoulder-neck boxes,
Lid Outer Width = Base Outer Width, while the inner neck collar steps inward byLid Greyboard Thickness + Neck Fit Clearance.
Artwork, Prepress, and Surface Finish
- File formats and color: Supply print-ready files in AI, PDF, or PSD using PDF/X-1a or PDF/X-4 standards, with all fonts outlined or embedded. Use CMYK with separate spot layers for metallic foils, spot UV, or embossing.
- Resolution and bleed: Minimum 300 DPI for all raster artwork, with 3 mm (0.118 in) bleed per outer wrap edge and ≥3 mm (0.118 in) safety margin inside fold/creased panel boundaries.
- Black ink and coverage: Use 100% K only for fine text and thin rules. Use rich black (
C40–60 M30–40 Y30–40 K100) for large solid black areas, keeping Total Area Coverage (TAC) at ≤280%–300% to prevent ink set-off and cracking along greyboard folds. - Lamination: Anti-scuff matte lamination suits dark artwork by resisting handling marks across high-friction lid-and-base contact zones. Account for wrap lamination thickness when setting lid-to-base clearance, as thick film adds friction along overlapping walls.
Job-Specific Production Steps
- Stack-up and dieline engineering: Measure the physical stack of cards, boards, punchboards, and inserts (including any plastic or paperboard tray), add the 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3 mm (0.059–0.118 in) height clearance, and generate separate dielines for the base greyboard, lid greyboard (plus neck greyboard if shoulder-neck), and outer paper wraps including the 15–20 mm (0.591–0.787 in) turn-in margins.
- Greyboard cutting and V-grooving: Die-cut or V-groove the greyboard blanks. V-grooved corners produce crisp 90-degree outer edges for flush wraps and shoulder-neck joints; standard scored/taped corners leave slightly softer exterior radii.
- Tray and lid forming: Fold the greyboard walls upward and stay-tape or hot-melt the four corners square. For shoulder-neck boxes, glue the pre-wrapped inner neck collar inside the base tray so the exposed step height matches the lid drop.
- Wrap printing, finishing, and wrapping: Print the wraps in CMYK (plus any spot layers), apply anti-scuff matte or gloss lamination, and die-cut the outer wrap sheets with corner reliefs. Glue and wrap the printed sheets onto the formed greyboard trays, folding the 15–20 mm (0.591–0.787 in) margins cleanly over the inner rim.
- Fit calibration and dry assembly: Test the wrapped lid over the wrapped base with a full dummy component load inside to verify glide resistance before full production gluing.
Sign-Off Criteria
- Structural fit and drop test: On an empty or loaded box held vertically by the lid, a full-telescope or partial-telescope base slides downward smoothly under gravity within a few seconds without binding or dropping instantly; a shoulder-neck lid seats flush against the base seam with no visible gap.
- Dimensional and squareness check: Internal width, length, and stack height meet the 1.5–2.5 mm (0.059–0.098 in) and 1.5–3 mm (0.059–0.118 in) clearance targets with no wall bowing when components are seated.
- Wrap and corner integrity: All four corners sit square with no exposed greyboard, glue squeeze-out, bubbling, or ink cracking along 90-degree V-grooved folds; the 15–20 mm (0.591–0.787 in) inner turn-in adheres flat to the interior wall.
- Print and regulatory records: Verify TAC ≤280%–300%, crisp 100% K fine text, and accurate bleed/safety alignment across lid-to-base wrap transitions. Where boxes are sold as part of a toy or consumer packaged good in regulated markets, maintain applicable material and packaging compliance documentation—such as EN 71 toy safety assessment and testing records (EU Toy Safety), German packaging registration (VerpackG / ZSVR), or French sorting labeling (Triman / Info-tri)—according to destination market requirements.
Concrete Failure Modes
- Vacuum-locked or binding lid: Caused by zero or negative lid-to-base clearance, uncompensated thick lamination on both mating surfaces, or tall full-telescope walls without air-relief channels or thumb notches.
- Loose, slipping lid: Caused by excessive lid-to-base clearance, out-of-square corner taping, or base walls bowing inward when an oversized box lacks an internal insert.
- Bowed walls and crushed corners: Caused by pairing 1.5 mm (0.059 in) greyboard with heavy flat game loads or tall upright card stacks exceeding 1.5–2 kg (3.3–4.4 lb), or by omitting internal dividers that transfer vertical stack load to the outer walls.
- Wrap cracking or peeling at edges: Caused by exceeding 280%–300% TAC on dark folds without lamination, grain direction running perpendicular to the main fold, or turn-in margins shorter than 15 mm (0.591 in) losing adhesion inside the rim.
- Scuffing on dark matte boxes: Caused by omitting anti-scuff matte lamination on dark C40–60 M30–40 Y30–40 K100 wraps, leading to burnished rub marks where the lid repeatedly slides over the base tray.
Guides in this section
Parent guide Card Box and Game Box Structures