Specifications and Materials
Rigid shell performance depends on matching greyboard thickness to the span of the box walls and keeping outer wraps thin enough to fold cleanly over 90-degree corners without cracking. When specifying paper wraps or liners, use gsm rather than pound weight alone, because US Text LB (measured on a 25 × 38 in / 635 × 965 mm basis sheet) and US Cover LB (measured on a 20 × 26 in / 508 × 660 mm basis sheet) represent different actual paper thicknesses at the same numerical pound rating.
| Parameter | Standard Specification | Metric (mm) | Imperial (in) | Notes |
|---|---|---|---|---|
| Greyboard core | Rigid chipboard / greyboard | 1.5 / 2 / 2.5 / 3 mm | 0.059 / 0.079 / 0.098 / 0.118 in | Thicker board increases wall rigidity and requires deeper V-grooves |
| Wrap turn-in margin | Continuous outer paper flap | 15–20 mm | 0.591–0.787 in | Folds over the top rim into the interior wall |
| Width / height clearance | Interior cavity allowance | 1.5–2.5 mm | 0.059–0.098 in | Prevents tight binds around decks, trays, or inserts |
| Stack height clearance | Interior depth allowance | 1.5–3 mm | 0.059–0.118 in | Accommodates deck thickness and liner buildup |
| Bleed (outer wrap) | All exterior trim edges | 3 mm per side | 0.118 in per side | Extends past the turn-in cut edge |
| Safety margin | Interior & face artwork | ≥3 mm | ≥0.118 in | Keeps text and borders clear of fold lines and creases |
Prepress and Surface Finishes
- File standards: Supply wrap artwork in AI, PDF, or PSD format exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Color and resolution: Build artwork in CMYK with separate spot layers where required, at ≥300 DPI.
- Ink density: Use 100% K for fine text, build rich black solids at C40–60 M30–40 Y30–40 K100, and keep total area coverage (TAC) at ≤280%–300% to prevent ink cracking along wrapped edges.
- Surface protection: Anti-scuff matte lamination suits dark artwork by resisting friction marks during mechanical wrapping and folding.
Job-Specific Production Steps
- Board cutting: Sheet greyboard (1.5–3 mm / 0.059–0.118 in) is slit and die-cut or guillotine-trimmed to the flat net blank dimensions of the base or lid.
- V-grooving or scoring: Fold lines are cut into the board. V-grooving removes a V-shaped channel from the exterior face to leave a thin hinge of uncut board, producing sharp 90-degree corners. Standard die-scoring compresses the board along the fold without removing material, which leaves a slightly softer edge radius.
- Corner-staying: The four side walls are folded upward at 90 degrees and locked together at each corner using heat-activated kraft or polyester stay tape to hold the shell square before wrapping.
- Outer paper wrapping: Adhesive is applied to the printed wrap sheet, and the stayed greyboard shell is positioned onto the wet sheet. The wrap is pressed onto the base panel, folded up the side walls, and turned over the top rim by the 15–20 mm (0.591–0.787 in) wrap margin onto the inside face.
- Interior lining: A separate interior liner sheet is glued into the bottom and inner walls (or wrapped prior to assembly) to cover the exposed greyboard and the turn-in edges of the outer wrap.
Sign-Off Criteria
- Dimensional fit: Interior cavity measurements meet the 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3 mm (0.059–0.118 in) stack height clearance for the intended contents.
- Squareness and corner integrity: Stayed corners sit flush at 90 degrees with no bowing along the side walls and no visible split in the outer wrap at the corner folds.
- Turn-in adhesion: The 15–20 mm (0.591–0.787 in) wrap margin bonds flat to the interior wall with no air bubbles, lifting edges, or exposed greyboard at the rim.
- Artwork registration: Face graphics, spine text, and borders align within the ≥3 mm (≥0.118 in) safety zone without drifting onto the wrapped edges.
- Surface finish: Dark CMYK or rich black areas show no scuffing, rub-off, or cracking along the V-grooved folds.
Concrete Failure Modes
- Over-deep V-grooving: Cutting too far through the greyboard weakens the hinge, causing the wall to tear off during corner-staying or under drop impact.
- Shallow V-grooving or under-scoring: Leaving too much uncut board thickness prevents a crisp 90-degree fold, resulting in rounded, bulging corners and poor lid fit.
- Insufficient wrap margin (<15 mm / <0.591 in): Short turn-in flaps lack enough glue surface area on the inner wall and peel back over time, especially when the interior liner is omitted or tight.
- Excessive ink coverage (TAC >300%): Heavy ink buildup combined with unlaminated dark solids cracks along the sharp V-grooved edges or scuffs against the wrapping machine's pressure brushes.
- Undersized interior clearance (<1.5 mm / <0.059 in): Ignoring liner thickness or board tolerances causes card decks, trays, or punchboards to jam inside the shell or bow the side walls outward.
Compliance and Material Records
When a finished boxed game or rigid packaging assembly requires regulatory assessment—such as European toy safety assessment and testing under EN 71, German packaging registration under VerpackG, or French sorting labeling under Triman—maintain batch records for greyboard, adhesives, inks, and laminations so material declarations and lab testing match the exact production build.
Guides in this section