For component construction, core materials, and format options, see game boards.
Core Tolerance Specifications
| Tolerance Area | Governing Condition | Specification / Relationship | Physical Effect |
|---|---|---|---|
| Greyboard Core | Board rigidity and fold bulk | 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) | Sets minimum hinge gap, corner wrap draw, and folded stack height |
| Wrap Turn-In | Paper wrap adhesion over board edge | 15–20 mm (0.59–0.79 in) past board trim onto reverse face | Anchors wrap tension against edge peel and corner exposure |
| Prepress Bleed & Safety | Wrap registration and trim shift | 3 mm (0.118 in) bleed per side; >= 3 mm (0.118 in) safety (>= 4–5 mm / 0.157–0.197 in for bordered backs) | Prevents white edge slivers and clipped border frames |
| Stepped Hinge Gaps | Multi-panel folding geometry | Outer fold gaps exceed inner fold gaps proportional to folded stack thickness | Allows outer panels to wrap over inner panels without pinching or tearing |
| Recess Cutout Clearances | Dual-layer die-cut wells | Artwork kept >= 3 mm (0.118 in) from cutout edges; die gap allowances follow 3–4 mm (0.118–0.157 in) spacing rules where applicable | Prevents registration drift from exposing unprinted board or binding tokens |
| Interlocking Tab Fit | Modular die-cut board joints | Matched tab-and-slot die profile accounting for board caliper and edge wrap | Balances snug table assembly against tear-out during disassembly |
| Flatness Bounds | Moisture and tension symmetry | Balanced face wrap and back liner across aligned grain direction | Prevents cupping, bowing, and rocking on flat surfaces |
| Box Interior Clearance | Folded board or GM screen in box | 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3 mm (0.059–0.118 in) stack height | Ensures smooth insertion and removal without crushing board corners |
Wrap Allowances and Prepress Margins
Paper wraps are printed on coated text-weight stock rather than heavy cover stock—measured in gsm, where US Text LB uses a 25 x 38 in basis sheet and US Cover LB uses a 20 x 26 in basis sheet—so the sheet folds cleanly around 90-degree board edges without cracking.
- Turn-in margin: The printed wrap extends 15–20 mm (0.59–0.79 in) beyond each edge of the greyboard core, folding over the board thickness and adhering to the back face before the back liner is applied.
- Artwork bleed and safety: Supply 3 mm (0.118 in) bleed per side beyond the full unwrapped sheet dimension (board size + board thickness + turn-in). Keep critical text and borders >= 3 mm (0.118 in) inside fold lines and board edges, increasing to >= 4–5 mm (0.157–0.197 in) on bordered backs.
- Print setup: Export CMYK files (with separate spot layers if specified) at >= 300 DPI in PDF/X-1a or PDF/X-4 (AI, PDF, or PSD source), with fonts outlined or embedded, 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for solids, and total area coverage (TAC) <= 280%–300%. Anti-scuff matte lamination suits dark artwork where fold friction occurs.
Stepped Hinge Gaps
Single-fold (bi-fold) boards use one centered hinge gap sized to let the two halves close face-to-face without stressing the outer wrap. Multi-fold boards (quad-fold, six-fold) and 3- or 4-panel GM screens stack panels on top of one another when folded, which requires stepped hinge gaps:
folded stack thickness = (folded panel layers * greyboard caliper) + wrap and film thickness
outer hinge gap > inner hinge gap
Each outward fold wraps around the combined thickness of the panels already folded inside it. If all hinges use the same narrow gap, the outer spine stretches when closed, lifting the wrap or splitting the hinge paper.
Recess Cutout Clearances and Interlocking Tab Fit
- Recess cutouts: Dual-layer boards laminate a die-cut top board onto a solid backing board. Die registration shifts relative to print, so keeping borders and labels >= 3 mm (0.118 in) clear of cutout edges prevents clipped graphics. Cutout openings must exceed the nominal token or tile footprint enough to accommodate die bevel and adhesive squeeze-out.
- Interlocking tabs: Modular boards with puzzle-cut edges rely on consistent die-cut kerf across 1.5–3 mm (0.059–0.118 in) greyboard. Unwrapped die-cut edges compress slightly during cutting for a tighter friction fit; wrapped edges add paper and adhesive thickness inside the joint and require wider slot clearance so tabs seat without delaminating the corner wrap.
Flatness and Box Clearance
Flatness depends on opposing tension: the adhesive moisture and film tension on the front wrap must be counterbalanced by a matching back liner and aligned paper grain direction. Once folded, the closed board or GM screen must clear the box walls by 1.5–2.5 mm (0.059–0.098 in) in width and length and 1.5–3 mm (0.059–0.118 in) in stack height.
Production Steps and Sign-Off Criteria
- Dieline and Step-Gap Engineering: Confirm greyboard caliper (1.5, 2, 2.5, or 3 mm / 0.059, 0.079, 0.098, or 0.118 in), fold sequence, stepped hinge widths, and 15–20 mm (0.59–0.79 in) wrap turn-in before placing artwork.
- Prepress Verification: Check 3 mm (0.118 in) bleed, >= 3 mm (0.118 in) safety (>= 4–5 mm / 0.157–0.197 in for bordered backs), TAC <= 280%–300%, and hinge-line artwork alignment across separate panels.
- Printing and Lamination: Print CMYK/spot sheets, cure ink, and apply protective film (such as anti-scuff matte on dark solids) on both the face wrap and balancing liner where required.
- Board Cutting and Mounting: Die-cut or guillotine greyboard panels, mount the wrapped face sheet with 15–20 mm (0.59–0.79 in) turn-ins, apply the back liner, and crease or assemble stepped hinges.
- Pressing and Conditioning: Stack finished boards under flat, weighted press plates until adhesive moisture stabilizes, then verify closed stack height against the 1.5–3 mm (0.059–0.118 in) box clearance allowance.
Physical Sign-Off Criteria
- Fold cycle check: Open and close the board or GM screen flat across all hinges; the outer wrap remains adhered with no whitening, cracking, or spring-back tension.
- Flatness check: Lay the opened board on a level surface; all corners and hinge seams sit flush without rocking or upward cupping.
- Fit check: Seat tokens in recessed wells, join interlocking tabs without forcing, and slide the folded unit into its box within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack clearances.
Concrete Failure Modes
- Corner Split or Wrap Lift: Turn-in margin falls below 15 mm (0.59 in) or heavy cover-weight paper is used instead of flexible text-weight wrap, causing edges to pull away from 2.5–3 mm (0.098–0.118 in) greyboard corners.
- Hinge Tearing or Spring-Back: Equal-width hinge gaps on a multi-fold board or GM screen fail to account for stacked panel thickness, over-stretching the outer wrap when folded shut.
- Board Cupping and Warping: Laminated face wrap is paired with an unlaminated or mismatched-grain back liner, or boards are packed before adhesive moisture equilibrates.
- Recess Misalignment: Graphics placed within 3 mm (0.118 in) of a die-cut recess edge show clipped borders or exposed greyboard after mounting registration variance.
- Tab Delamination or Binding: Interlocking slots cut without allowance for wrap or film thickness pinch during assembly, peeling the surface paper back from the tab neck.
- Box Pinch: Closed stack height exceeds target due to uncalibrated lamination and hinge bulk, eliminating the 1.5–3 mm (0.059–0.118 in) vertical box clearance and crushing board edges during packing.
Guides in this section