Choose turned-edge wrapping over flush-cut construction when a single-panel board from the flat rigid boards family requires sealed edges, continuous wrap-around artwork or border color, and resistance to edge delamination during repeated handling. Switch to thicker grayboard cores as board span increases to maintain rigidity, and pair dark full-bleed artwork with anti-scuff matte lamination to prevent rub marks along the folded edges.


Specifications

Parameter Specification Notes
Grayboard Core Caliper 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) Selected by board span and rigidity requirements
Wrap Margin (Turn-In) 15–20 mm (0.59–0.79 in) per side Folds over the board edge onto the back face
Face & Counter-Liner Stock Coated art or specialty paper, 120–150 gsm (approx. 80–100 lb US Text, 25 × 38 in basis sheet) Distinct from US Cover LB (20 × 26 in basis sheet); Text weight folds cleanly around 90-degree edges
Counter-Liner Placement Inset from all four board edges Overlaps the turned-in face paper edges without extending past the board perimeter
Surface Finish Anti-scuff matte or standard matte/gloss film Anti-scuff matte suits dark artwork; lamination adds 0.015–0.025 mm (0.0006–0.0010 in) per laminated side
Color & Ink Limits CMYK with separate spot layers; rich black C40–60 M30–40 Y30–40 K100; 100% K for fine text Total Area Coverage (TAC) ≤280%–300%
Prepress Files & Resolution AI, PDF, or PSD (PDF/X-1a or PDF/X-4); ≥300 DPI Fonts outlined or embedded
Artwork Bleed & Safety ≥3 mm (0.118 in) interior safety from board edge; background/bleed extended across the full 15–20 mm (0.59–0.79 in) wrap margin plus 3 mm (0.118 in) outer trim bleed Prevents white paper showing on the folded edge or back turn-in

Sheet Sizing Formulas

Because the printed face sheet must cover the front face, the board edge thickness, and the 15–20 mm (0.59–0.79 in) turn-in on all four sides, calculate the untrimmed wrap sheet dimensions in plain text as:

  • Face Sheet Width = Board Width + (2 * Board Thickness) + (2 * Wrap Margin)
  • Face Sheet Height = Board Height + (2 * Board Thickness) + (2 * Wrap Margin)

For example, adding a 20 mm (0.79 in) wrap margin on each side adds 40 mm (1.57 in) plus twice the grayboard caliper to both width and height before corner notching.


Production Steps

Card Deck Press produces turned-edge wrapped flat boards through specialist offset and tabletop manufacturing partners:

  1. Offset Printing & Lamination: Print the face wrap sheet and the counter-liner sheet in CMYK (plus any spot layers) at ≥300 DPI. Apply surface lamination—such as anti-scuff matte film for dark designs—to the face sheet before die-cutting.
  2. Corner Notching: Die-cut or notch the four corners of the printed face sheet at 45-degree angles (or stepped mitered tabs) sized to the selected grayboard caliper (1.5–3 mm / 0.059–0.118 in) so adjacent turn-ins meet cleanly without overlapping bulk.
  3. Face Mounting: Coat the back of the face sheet with adhesive and register the cut grayboard core onto the center of the sheet.
  4. Edge Turning & Pressing: Fold the 15–20 mm (0.59–0.79 in) wrap margins tightly over all four grayboard edges and press them flat onto the back face of the board.
  5. Counter-Liner Application: Glue and mount the inset counter-liner over the back of the board so it bridges the turn-in seam and seals the exposed grayboard center.
  6. Weighted Conditioning: Stack and press the finished boards under controlled weight while adhesive moisture equalizes to lock in board flatness.

Sign-Off Criteria

Before approving a production run, verify the physical sample against these criteria:

  • Sealed Perimeter: All four edges are completely covered by the face wrap with no exposed grayboard fibers at the corners or along the sides.
  • Turn-In Adhesion: The 15–20 mm (0.59–0.79 in) wrap margins lie flat against the back face with no bubbling, tenting, or edge lift.
  • Corner Neatness: Mitered corners are tight and square without protruding paper ears or split lamination along the fold.
  • Counter-Liner Alignment: The inset counter-liner sits centered on the back face, overlapping the turn-in edges cleanly without overhanging any board edge.
  • Flatness & Print Registration: The board lies flat on a level surface, and key artwork stays at least 3 mm (0.118 in) inside the front edge while edge color wraps cleanly around the thickness of the board.

Failure Modes

  • Edge Lift or Bubbling: Occurs when the wrap margin is narrower than 15 mm (0.59 in), adhesive coverage is uneven along the perimeter, or stiff lamination pulls the turn-in away from the grayboard. Maintain the full 15–20 mm (0.59–0.79 in) turn-in and press edges immediately after folding.
  • Corner Dog-Ears or Cracking: Occurs when corner notches do not match the 1.5–3 mm (0.059–0.118 in) board caliper or when overly heavy Cover-weight stock is used instead of flexible Text-weight wrap paper. Adjust notch geometry to the exact board thickness and keep wrap paper in the 120–150 gsm range.
  • Board Warping (Cupping or Bowing): Occurs when moisture from the adhesive and face paper pulls the board concave before the back is balanced. Apply the inset counter-liner promptly after wrapping, align paper grain direction consistently, and condition stacks under weight.
  • Exposed Raw Board at the Fold: Occurs when artwork bleed stops at the front trim line instead of extending across the 15–20 mm (0.59–0.79 in) wrap zone, or when registration shifts during mounting. Extend background color across the entire wrap margin and keep critical graphics ≥3 mm (0.118 in) inside the front edge.
  • Scuffing Along Folded Edges: Occurs on dark, high-ink-coverage boards when unlaminated ink rubs during folding or packing. Keep Total Area Coverage ≤280%–300% and specify anti-scuff matte lamination.