Structural Specifications and Clearances
- Paperboard Stock and Basis Weight: Specify 350 gsm art stock (0.34–0.38 mm / 0.013–0.015 in caliper) for light, narrow decks, or 400 gsm stock (0.40–0.44 mm / 0.016–0.017 in caliper) for wider platforms and heavier token trays. In US basis weights, these heavy boards are rated in Cover LB (20 × 26 in basis sheet size) rather than Text LB (25 × 38 in basis sheet size). When single-ply folded struts cannot support dense component loads, replace the folded riser with 1.5 mm (0.059 in) or 2.0 mm (0.079 in) greyboard support blocks.
- Box Fit and Stack-Height Clearance: Maintain 1.5–2.5 mm (0.059–0.098 in) total clearance across the box width and length so the riser slides into the base without bowing the outer walls. Set the riser step height to leave 1.5–3.0 mm (0.059–0.118 in) of vertical clearance between the top of the elevated deck or tray and the inner lid plane.
- Grain Direction: Align the paperboard grain vertically down the load-bearing struts (perpendicular to the horizontal shelf crease) to maximize column compression resistance.
- Prepress and Print (Printed Risers): Supply CMYK artwork with separate spot layers if required at ≥300 DPI in PDF/X-1a or PDF/X-4, with outlined or embedded fonts, 3 mm (0.118 in) bleed per side, and ≥3 mm (0.118 in) safety margin from trim and crease lines. Use 100% K for fine text, rich black (C40–60 M30–40 Y30–40 K100) for dark solids, and keep total area coverage (TAC) at ≤280%–300%. Apply anti-scuff matte lamination or varnish on dark artwork to prevent rub marks from sliding card edges; double-sided film adds 0.03–0.05 mm (0.001–0.002 in) to sheet thickness.
Fold-Lock Struts and Gusset Geometries
Stepped paperboard risers resist crushing under stacked boxes only when vertical loads travel straight into the box floor rather than bending the side skirts:
- Fold-Lock Vertical Struts: Die-cut internal support legs fold 90 degrees beneath the elevated shelf and engage with locking slots cut into the base flange or side wall. Unpinned 90-degree flaps splay outward under top load, whereas tab-locked struts form closed vertical columns.
- Gusseted Corner Webs: Continuous 45-degree diagonal creases connect the vertical riser wall to the horizontal step shelf. These triangular gussets fold inward as the platform erects, resisting sideways shear (parallelogram racking) when boxes shift during shipping.
- Double-Laminated Step Edges: Folding the vertical riser wall back 180 degrees against itself doubles the load-bearing thickness along the step front (reaching 0.80–0.88 mm / 0.031–0.035 in on 400 gsm stock) where deck and tray weight concentrates.
- Span-Matched Sub-Frames: Narrow shallow decks can sit on a central stepped bridge flanked by open side wells. Wide trays require an intermediate center strut or perimeter-braced cross-rib so the horizontal shelf does not dish downward in the middle.
Production Steps
- Dieline and Step-Height Engineering: Calculate the riser elevation from the box interior depth minus the shallow deck or tray height and the 1.5–3.0 mm (0.059–0.118 in) lid clearance. Position fold-lock tabs, base slots, and 45-degree gusset creases with vertical grain orientation locked on the layout. Custom box tooling and insert dies follow project and component minimums (standard offset card decks start at 200 decks across 200/300/500/1,000+ tiers).
- Offset Printing and Coating: Print sheets on 350–400 gsm stock and apply anti-scuff matte coating where dark ink meets moving cards or trays.
- Flatbed Die-Cutting and Creasing: Cut the perimeter, locking slots, and internal strut reliefs while channeling the 90-degree, 45-degree, and 180-degree fold lines so heavy coated stock folds cleanly without outer-ply splitting.
- Erection and Box Loading: Fold the corner gussets inward, seat every vertical strut tab into its matching base slot, drop the assembled platform into the box base within the 1.5–2.5 mm (0.059–0.098 in) lateral tolerance, and place the shallow deck or token tray on the step.
Sign-Off Criteria
- White Dummy Fit Check: Assemble an unprinted die-cut sample on the production stock and grain direction inside the target box with the actual card stack or tray. Verify smooth insertion without wall bowing and confirm 1.5–3.0 mm (0.059–0.118 in) clearance below the closed lid.
- Static Top-Load Compression: Place stacked boxes or an equivalent dead weight (for example, 5–15 kg / 11–33 lb matching master-carton stacking height) on the closed lid. Open the box and inspect struts for buckling, tab pull-out, or shelf dishing.
- Crease Integrity Inspection: Check 90-degree strut folds, 45-degree gussets, and 180-degree double-wall returns under raking light for fiber cracking or coating delamination.
Concrete Failure Modes
- Strut Splay and Pancaking: Vertical support legs that lack locking tabs or rely solely on friction against smooth inner box walls slide outward under stacked carton weight, collapsing the platform flat.
- Cross-Grain Column Buckling: Nesting the dieline with paperboard grain running horizontally across the riser width rather than vertically down the struts reduces column stiffness, causing the riser wall to kink mid-height under load.
- Gusset Cracking on Heavy Coated Stock: Folding 400 gsm board across 45-degree gussets or 180-degree return walls without properly matched crease channels splits the outer clay coat and weakens corner shear resistance.
- Center-Span Dish: Supporting a wide tray or deck only at its outer edges leaves the center of the horizontal shelf unsupported, causing it to sag downward and drop the deck below the lid plane.
- Lateral Wall Bind: Exceeding the 1.5–2.5 mm (0.059–0.098 in) perimeter clearance wedges the riser against the box walls, bowing the base outward and obstructing telescoping lid closure.
Parent guide Folded Paperboard Insert Structures