Structural Specifications and Tolerances
Because deck formats vary by project, trench dimensions are derived directly from the trimmed deck and the inner box cavity rather than a fixed card trim.
| Parameter | Specification | Notes |
|---|---|---|
| Insert board weight | 300–400 gsm | Measured in gsm; US Cover LB (20 × 26 in basis sheet) is distinct from US Text LB (25 × 38 in basis sheet) |
| Board caliper (uncoated) | 300 gsm: 0.28–0.31 mm (0.011–0.012 in) 350 gsm: 0.34–0.38 mm (0.013–0.015 in) 400 gsm: 0.40–0.44 mm (0.016–0.017 in) |
Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) |
| Lateral trench clearance | 1.5–2.5 mm (0.059–0.098 in) | Added to trimmed deck width and length |
| Vertical stack clearance | 1.5–3.0 mm (0.059–0.118 in) | Added to deck stack height inside the box cavity |
| Outer box wall brace (if rigid box) | 1.5, 2.0, 2.5, or 3.0 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard | Rigid box walls resist outward splay from friction-locked U-channels |
| Prepress & print files | AI, PDF, or PSD; PDF/X-1a or PDF/X-4 | CMYK + separate spot layers for cut/crease/glue-free zones; ≥300 DPI |
| Bleed & safety | 3 mm (0.118 in) bleed per side; ≥3 mm (≥0.118 in) safety | Keep critical text and borders clear of fold creases |
| Ink & black builds | 100% K fine text; rich black C40–60 M30–40 Y30–40 K100 | TAC ≤280%–300%; anti-scuff matte lamination suits dark artwork |
Sizing Formulas
Trench inner width = Deck trimmed width + (1.5 to 2.5 mm) [+ 0.059 to 0.098 in]
Trench inner length = Deck trimmed length + (1.5 to 2.5 mm) [+ 0.059 to 0.098 in]
Trench wall height = Box inner depth (or Deck stack height + 1.5 to 3.0 mm [0.059 to 0.118 in])
For friction-locked U-channels, the outer return wings span the full inner width of the box cavity so the box walls hold the insert in compression. For glued center-trench inserts, the outer footprint is sized to sit cleanly inside the box walls with 1.5–2.5 mm (0.059–0.098 in) total clearance, because the glued anchor flaps carry the lateral load independently.
Production and Construction Steps
- Align paperboard grain with the primary trench creases. Run the sheet grain parallel to the longitudinal channel folds so the vertical walls resist buckling under downward deck weight (kg/lb) and fold cleanly without cracking.
- Design load-transferring shoulders and return legs. Form horizontal top shoulders that bridge from the trench rim to the outer box wall, then fold down into full-depth vertical outer legs. This transfers vertical deck mass (kg/lb) to the box floor instead of suspending the deck solely on crease stiffness.
- Select the wall-locking mechanism.
- Friction-locked U-channel: Size the outer return legs to contact the inner box walls snugly so the box tray prevents the trench walls from splaying outward.
- Glued anchor-flap center-trench: Add bottom fold-in or fold-out anchor flaps along the base of the trench walls, or die-cut tab-and-slot returns that lock beneath the trench floor.
- Mask glue zones and set tooling. Keep varnish and film lamination off all adhesive anchor flaps on a separate spot layer. Cut and crease on custom steel-rule tooling (subject to boxed-game and tooling minimums), using double-score channels where 350–400 gsm (0.34–0.44 mm / 0.013–0.017 in) board makes tight 90-degree or 180-degree turns.
- Pre-break creases and assemble. Pre-fold the shoulders and anchor flaps, bond glued seams under pressure until set, and seat the finished insert into the box tray.
Sign-Off Criteria
- Deck fit and extraction: The trimmed deck drops into the trench with 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3.0 mm (0.059–0.118 in) vertical clearance, sliding out without corner snagging.
- Wall stability under load: Vertical trench walls remain square at 90 degrees with no outward splay, shoulder sag, or floor lift when carrying the full deck weight (kg/lb).
- Crease and lamination integrity: Folded shoulders show no ink cracking or film delamination along the top edges; glued anchor flaps hold firmly along unvarnished board fibers.
- Prepress verification: Die-lines and glue-free masks sit on separate non-printing spot layers, bleed extends 3 mm (0.118 in) past cut lines, and total area coverage stays at or below 280%–300%.
Concrete Failure Modes
- Outward wall splay and trench collapse: Un-glued U-channel walls bow outward when the outer box span is too wide or the outer tray walls flex, causing the deck to drop to the box floor. Resolve by adding glued bottom anchor flaps or bracing the insert against rigid greyboard walls (1.5–3.0 mm / 0.059–0.118 in).
- Shoulder cracking and springback: Folding across the paperboard grain or under-scoring 350–400 gsm (0.34–0.44 mm / 0.013–0.017 in) stock fractures the outer printed surface and creates upward springback that pushes the deck against the box lid.
- Adhesive delamination on coated flaps: Extending flood varnish or film lamination onto anchor flaps prevents glue penetration, causing the trench base to pop open under deck weight (kg/lb) during transit.
- Corner binding during insertion: Omitting the 1.5–2.5 mm (0.059–0.098 in) lateral allowance causes card corners—including standard R3–R3.5 mm (0.118–0.138 in) rounded corners—to catch on the vertical trench walls and fray card edges.
Parent guide Folded Paperboard Insert Structures