Choose the opening geometry based on how many layers protect the card, how the deck sits inside its box, and whether cards are handled repeatedly or sealed for storage. For seam welding and base sleeve construction, see card sleeve welding and openings.

Opening Specifications and Trade-Offs

Opening Type Aperture Placement Primary Use Case Air Evacuation & Fit Closure & Retention
Top-loading Short top edge Single sleeving and outer sleeves Vents straight out during single-layer insertion; traps air if used as an inner sleeve inside another top-loading sleeve Open mouth; relies on sleeve friction and depth
Side-loading Long side edge Inner sleeves for double sleeving Vents trapped air perpendicular to a top-loading outer sleeve's mouth as the card slides down Friction fit inside the outer sleeve
Resealable flap Short top edge with extended fold-over lip Archival storage and multi-card packs Traps air if sealed before compressing the stack Pressure-sensitive adhesive strip on the sleeve body or flap

Deck fit depends on the combined thickness of the sleeve wall, trapped air, and card stock—such as 300 gsm art or blue core at 0.28–0.31 mm (0.011–0.012 in), 400 gsm at 0.40–0.44 mm (0.016–0.017 in), or PVC at 0.30 mm (0.012 in), plus 0.03–0.05 mm (0.0012–0.0020 in) per card if double-sided film is applied. Total sleeved deck height and width must stay within box clearances of 1.5–2.5 mm (0.059–0.098 in) across width and height and 1.5–3 mm (0.059–0.118 in) for stack height.

Production and Assembly Mechanics

  1. Aperture placement and slitting: Leave one edge unwelded while sealing the remaining perimeter as covered in card sleeve welding and openings. Slit the opening mouth cleanly without nicking the adjacent side welds. For any deck format, size the aperture and lip allowance to the finished card trim and caliper so cards enter without catching.
  2. Inner-sleeve air evacuation: When producing double-sleeve sets, pair a side-loading inner sleeve with a top-loading outer sleeve. Placing the inner opening along the long edge creates an escape path perpendicular to the outer sleeve's closed bottom, allowing air to vent along the side seam during insertion.
  3. Resealable flap-strip mechanics: Extend one panel past the mouth to form a fold-over lip, score the fold line, and apply a release-lined adhesive strip. Mounting the adhesive strip on the sleeve body rather than the flap keeps exposed adhesive away from card edges during insertion and removal.

Sign-Off Criteria

  • Target cards insert and withdraw smoothly without edge-buckling or snagging on the adhesive strip.
  • A side-loading inner sleeve inside a top-loading outer sleeve expels air during insertion and keeps the stacked deck within the 1.5–3 mm (0.059–0.118 in) box stack-height clearance.
  • Aperture slits are square and clean, with intact corner welds at both ends of the mouth.
  • Resealable flaps fold flat without skewing, and release liners peel cleanly without lifting the adhesive layer.

Failure Modes

  • Air pillowing and stack swell: Using a top-loading inner sleeve inside a top-loading outer sleeve seals air at the closed bottom, inflating the stack past box clearance.
  • Adhesive snagging: Placing the adhesive strip on the fold-over flap exposes glue directly to the card corner as the card passes through the mouth.
  • Mouth weld tearing: Misaligned slitting or weak corner termination at the open edge causes the sleeve to split down the side seam under insertion force.
  • Flap skew or premature release: Uneven fold scoring or surface contamination prevents the adhesive strip from staying sealed during handling or transit.