The exact mold split, trimming allowance, and polishing sequence shift based on four conditions:
- Mold architecture: Single-face cap (squish) molds isolate cleanup to one face, whereas two-piece split molds require seam blending across multiple edges.
- Resin cure hardness: Harder cured resin holds a sharper vertex under lapping but chips more easily if trimmed aggressively.
- Inclusion load: Heavy glitter, foil, or solid inserts near the surface can snag during coarse leveling and leave micro-pits on the polished face.
- Numeral engraving depth: Shallow engravings risk being ground away if thick mold flash forces heavy stock removal on the sprue face.
Specifications and Structural Parameters
| Parameter | Sharp-Edge Cast Resin Requirement | Operational Impact |
|---|---|---|
| Mold cavity material | Platinum-cure silicone cast from a lapped master | Transfers optical face flatness and crisp edge angles before polishing begins |
| Parting-line placement | Routed to a single designated face (cap mold) or controlled edge | Limits primary sprue and flash removal to one plane, preserving adjacent vertices |
| Flashing / sprue allowance | Kept thin, typically 0.1–0.3 mm (0.004–0.012 in) at the cap seam | Prevents excessive coarse-grit grinding that can dish the face or shallow out numbers |
| Polishing platen | Rigid flat lap (glass or precision plate), not foam-backed pads | Maintains planar geometry right up to the edge without rounding vertices |
| Engraving depth | Sufficiently recessed below the raw face plane | Allows full sprue-face leveling and multi-stage polishing without losing number walls |
| Post-polish handling | Separated into individual foam or tray cells | Prevents vertex-to-vertex impact chipping during inspection and packing |
When sharp-edge dice are included in products intended for younger players, sharp points and small-part geometry require formal mechanical-hazard and age-grading assessment under applicable frameworks such as the European Commission toy safety rules rather than assuming standard component clearance.
Production Steps
Master Preparation and Parting Placement Masters are finished to target flatness and edge crispness before silicone pouring. For polyhedral sets, cap-mold parting is positioned on a single flat face (often the highest-value face) so the remaining faces demold near-finished and only require light final buffing.
Pressure Casting and Full Cure Resin is mixed, degassed, and cured inside a pressure chamber so trapped air collapses away from acute mold vertices and recessed numeral walls. Dice remain in the mold until the resin reaches full cross-linked hardness; demolding early causes edges to flex or smear during trimming.
Manual Sprue and Flash Trimming Once demolded, raised flashing or gate stubs on the parting face are pared back using a fresh precision blade or flush-cut nipper. Cuts are made parallel to the face rather than levered against an adjoining edge, leaving a slight proud margin to be leveled on the lap rather than gouging below the face plane.
Progressive Flat-Lap Polishing The trimmed face is worked wet on a rigid flat lap using sequential abrasive films or papers—moving from coarse leveling grits down through fine micro-abrasives and a final polishing compound. Each stage removes the scratch pattern of the previous grit while keeping downward pressure centered over the face so edges stay square. Adjacent un-sprued faces receive light high-grit finishing only as needed to match gloss.
Numeral Inking and Surface Wipe Recessed numbers are filled with acrylic or enamel paint, then wiped clean across the flat face with a lint-free cloth and mild solvent that does not craze the cured resin.
Sign-Off Criteria
Pre-production and lot sign-off samples are checked under raking light and magnification before bulk assembly:
- Vertex and edge integrity: Points meet cleanly with no chips, fractured corners, or softened "pillow" bevels.
- Face planarity: Reflections across every face remain undistorted, with no dishing or tilted planes on the sprue face.
- Optical clarity: No milky haze, swirl marks, or leftover coarse-grit scratches from skipped polishing steps.
- Seam invisibility: No raised ridge or step along the mold parting face or edges.
- Numeral definition: Crisp, uniform paint fill with clean edges and consistent depth on the polished sprue face.
Concrete Failure Modes
- Chipped vertices during trimming or packing: Caused by biting too close to a corner with dull nippers, prying against an edge, or bulk-tumbling finished dice together in bags instead of compartmentalized trays.
- Rounded ("pillowed") edges: Caused by polishing on compressible foam-backed abrasives or rocking the die by hand, which wears down the outer perimeter faster than the face center.
- Dished or out-of-flat sprue face: Caused by uneven finger pressure during coarse leveling when removing thick cap-mold flash.
- Pinholes at tips and numbers: Caused by insufficient degassing or pressure during cure, leaving micro-voids that trap white polishing compound.
- Cloudy faces or persistent scratch lines: Caused by jumping too far between grit sizes or failing to rinse coarse abrasive residue before moving to finer films.
- Shallow or erased numerals: Caused by heavy mold flash forcing excessive material removal on the sprue face, grinding down into the engraved number recess.
Parent guide Molded and Cast Dice Construction