• Cavity molding suits uniform, high-repeatability runs where rigid multi-part tooling controls face flatness, parting-line alignment, and consistent pip depth across every die.
  • Silicone casting suits layered or suspended internal inclusions and sharp-edge profiles that require multi-stage pouring and hand-finished gate removal, though flexible molds wear faster and require closer dimensional checks.

Partner-sourced game pieces and custom dice tooling follow project and component minimums rather than standard offset card deck tiers.

Structural Specifications

Construction Element Cavity Molding Silicone Casting Primary Control Target
Mold-cavity architecture Rigid multi-part cavity with fixed parting lines and gate channels Flexible split or cap silicone mold with pour spouts Face-to-face parallelism and flash control
Internal inclusion layering Single-shot or two-stage core-and-overmold Multi-stage pour with timed gel intervals Centered mass and bubble-free suspension
Pip and numeral engraving Machined into cavity walls with draft angles Cast from master pattern with recessed faces Clean ink retention and sharp character edges
Edge-finishing workflow Mechanical gate trim and bulk tumbling Hand-trimmed sprue and staged wet polishing Uniform corner radius or crisp flat-edge geometry

When dice are packed inside a custom game box or tray alongside cards and boards, allow 1.5–2.5 mm (0.059–0.098 in) clearance across box width and height and 1.5–3 mm (0.059–0.118 in) clearance for stack height.

Production Steps

  1. Tooling or master preparation: Machine rigid mold cavities with recessed pip/numeral geometry and draft angles, or finish a dimensionally true master pattern for silicone mold making.
  2. Molding or staged casting: Inject or pour base resin into the cavity. For layered designs, pour a base layer, position inclusions once the first layer supports them without sinking, and complete the fill to encase the inclusions centrally.
  3. Demolding and gate removal: Release cured dice from the cavity or split silicone mold and trim sprues, vents, and parting-line flash flush with the surrounding face.
  4. Edge finishing: Tumble rounded-edge dice in finishing media to smooth edges uniformly, or lap and polish sharp-edge dice face by face to preserve crisp intersections.
  5. Ink filling and wipe-down: Flood recessed pips and numerals with pigment ink, wipe excess cleanly from the flat face, and cure the ink fill.
  6. Regulatory documentation (when applicable): For dice marketed as toys or for children, complete EN 71 assessment and testing records under the EU Toy Safety framework before release.

Sign-Off Criteria

  • Geometric symmetry: Opposite faces are parallel and adjacent faces meet squarely without warpage or sunken faces.
  • Centered weight distribution: No visible air pockets, voids, or shifted inclusions that pull the center of mass toward one face.
  • Recessed ink readability: High-contrast ink fills every pip and numeral completely with crisp edges and no surface smear or haloing on the surrounding face.
  • Clean edge and parting-line finish: Gate marks and parting lines are flush and match the gloss or matte texture of the rest of the die.

Concrete Failure Modes

  • Shifted inclusions or trapped air voids: Pouring before the base layer reaches sufficient viscosity lets dense inclusions sink, while trapped air creates voids near upper faces; both skew roll fairness.
  • Over-sanded faces during gate removal: Aggressive trimming or uneven hand lapping flattens one face more than others, breaking symmetry and altering roll balance.
  • Ink pull-out or smudged faces: Shallow engraving, missing draft angles, or wiping before partial ink set lifts pigment out of the recess or leaves haze across textured surfaces.
  • Parting-line flashing and edge chipping: Worn mold seams leave raised ridges that catch during tumbling, while brittle sharp edges chip if agitated in bulk media instead of hand-polished.