Forming Methods and Structural Specifications
| Structure / Method | Best-Fit Geometry | Physical Characteristics | Primary Constraint |
|---|---|---|---|
| Bar Milling and Cross-Cut Slicing | Flat-faced 2.5D silhouettes (cubes, discs, meeples, hexagonal tokens) | Constant cross-section along the extrusion axis; parallel front and back faces | Cannot form undercuts, waisted necks, or domed tops |
| Individual CNC Turning / Routing | 3D contoured parts (pawns, tapered pegs, spherical heads, grooved cylinders) | Variable diameter along the axis; smooth rotational symmetry | Higher cycle time per blank; curved faces limit flat printing |
| Tumble-Sprayed Lacquer | Single-color pieces of any geometry | Even base color across faces and edges | Sharp internal corners and deep recesses receive thinner coverage |
| Pad Printing (Tampo) | Flat or gently curved faces on sliced or turned blanks | Silicone pad transfers spot ink from an etched plate | Small print area; requires separate plates and jigs per spot color |
| Screen Printing | Wide, flat, uniform-thickness wooden tokens and blocks | Thick, opaque spot ink deposit through mesh | Requires flat registration surface; unsuitable for curved sides |
| Heat Transfer / Foil Stamping | Sealed flat faces needing multi-color detail or metallic accents | Film or foil bonded under heat and pressure | Requires smooth, sealed grain to prevent lifting or pitting |
| Laser Engraving | Monochrome recessed detail on raw or coated wood | Etched mark with no ink layer thickness | Natural grain density varies contrast between pieces |
Surface Preparation and Graphic Prepress
Raw wood grain is porous and absorbs liquid ink unevenly, causing feathered edges and patchy coverage. After slicing or turning, blanks are tumble-sanded to knock down sharp burrs and round fragile edges, then sealed with a primer or base lacquer before graphic application.
- File Format and Color Separation: Supply vector artwork in AI, PDF, or PSD (PDF/X-1a or PDF/X-4) with outlined or embedded fonts. Use separate spot layers for each pad-print, screen-print, or foil pass rather than process halftones on small wooden faces, and keep fine text in 100% K or a single solid spot color. For heat-transfer films carrying full-color rasters, provide ≥300 DPI artwork and keep total area coverage (TAC) at ≤280%–300%.
- Fit and Box Clearance: Account for wood blank variation and paint or lacquer build-up when sizing insert cavities and trays. Standard boxed-game clearance of 1.5–2.5 mm (0.059–0.098 in) across width and height and 1.5–3 mm (0.059–0.118 in) for stack height prevents painted wooden pieces from binding inside rigid compartments.
Job-Specific Production Steps
- Geometry Review and Tooling Split: Assign constant-profile pieces to bar milling and slicing, and assign contoured or axially symmetric pieces to individual CNC turning. Confirm custom cutter profiles and print-registration jigs against project minimums.
- Blank Forming and Deburring: Mill and slice profiled bars or turn individual blanks, then tumble-sand to remove cross-cut fuzz, sharp corners, and machining marks.
- Sealing and Base Coating: Apply a pore-filling sealer and base coat (by spray or tumble-coating) and cure fully so the surface is uniform before printing.
- Graphic Application and Curing: Seat blanks in dedicated jigs for pad printing, screen printing, heat transfer, or laser engraving. Cure inks or lacquers completely before bulk bagging to prevent sticking.
- Sorting, Fit Check, and Compliance Records: Cull split or misregistered pieces, verify cavity fit in the target insert or tray, and complete applicable assessment and testing—such as EN 71 toy safety assessment and testing where the product falls under toy or child-accessible scopes—logging test reports alongside required market records.
Sign-Off Criteria
- Blank Integrity: Cross-cut faces and turned contours match the approved physical sample with smooth, deburred edges and no splintering or tear-out.
- Coating Uniformity: Sealer and base lacquer cover grain evenly without pinholes, orange-peel texture, or uncured tackiness.
- Graphic Registration and Adhesion: Printed, foiled, or engraved marks sit centered within the face boundary, remain legible at actual size, and resist rubbing during normal handling.
- Component Fit: Sample pieces drop cleanly into their assigned tray or box cavities within the specified clearance.
- Compliance Documentation: Applicable safety assessment and test records (such as EN 71 documentation where relevant) are verified before bulk shipment.
Concrete Failure Modes
- Grain Raise and Ink Feathering: Skipping or under-applying the wood sealer lets pad or screen ink wick into open wood fibers, blurring fine lines and text.
- Cross-Cut Tear-Out: Dull slicing blades or unchamfered 90-degree corners chip along the grain during bar cutting or bulk tumbling.
- Jig Registration Drift: Minor thickness or width variation between sliced blanks causes pad-printed or screen-printed graphics to shift off-center on small faces.
- Coating Tackiness and Rub-Off: Insufficient cure time or incompatible topcoats over base lacquer cause painted pieces to stick together in bulk bags or scuff in transit.
- Cavity Binding: Unaccounted paint build-up or blank swell pushes piece dimensions past tray clearance, preventing smooth seating or removal.
Guides in this section
Parent guide Non-Paper Component Construction and Structures