To avoid blade splices and crushed tips in irregular contours, soften sharp inward notches into continuous curves and widen acute outward points in the die line before tooling. The exact geometric limit changes with the board construction: thicker greyboard requires deeper blade penetration and generates stronger lateral wedging from the steel-rule bevel, while tighter spacing between neighboring pieces weakens the surrounding waste matrix.
Specifications and Physical Tolerances
| Parameter | Specification (Metric) | Specification (Imperial) | Production Impact |
|---|---|---|---|
| Greyboard core thickness | 1.5 / 2.0 / 2.5 / 3.0 mm | 0.059 / 0.079 / 0.098 / 0.118 in | Thicker cores increase bevel wedging and tip crush risk |
| Punchboard die gap | 3–4 mm | 0.118–0.157 in | Minimum spacing between adjacent cuts to prevent web collapse |
| Artwork bleed | 3 mm per side | 0.118 in per side | Covers die-cut registration variance along irregular paths |
| Safety margin | >=3 mm | >=0.118 in | Keeps critical graphics clear of bevel compression at tight corners |
| Prepress cut-line format | AI, PDF, PSD (PDF/X-1a or PDF/X-4) | — | Cut, crease, and nick paths must sit on separate spot layers |
Job-Specific Production Steps
- Audit the vector die line against board thickness: Review all inward corners, tight concave curves, and narrow spikes on the spot cut layer before approving tooling. Replace dead-sharp inward vertices with small radii so a single steel rule can bend continuously around the contour, and verify that adjacent tokens maintain the 3–4 mm (0.118–0.157 in) die gap.
- Set artwork bleed and safety around tight points: Extend background artwork 3 mm (0.118 in) past the cut path and hold text or key borders >=3 mm (0.118 in) inside the contour so slight bevel compression on narrow projections does not clip visible design elements.
- Bend and seat the steel rule: Specialist tabletop manufacturing partners bend steel cutting rule to match the approved vector path and mount it into the die board. Where a contour turns tighter than the steel can bend without kinking, the diemaker must miter or splice two separate blade ends together.
- Apply ejection rubber and position nicks: Foam ejection rubber is placed alongside the rule to strip the board cleanly after the press stroke. Holding nicks are placed along straight or broad edges—never on narrow spikes or spliced corners—so punching out the piece does not tear a fragile tip.
- Die-cut on the flat-bed press: As the press drives the beveled rule through the wrapped greyboard, the bevel pushes the paperboard outward. Broad curves distribute that lateral force evenly, whereas narrow acute tips are pinched from both sides simultaneously.
Sign-Off Criteria
- Continuous cut edges: Inward corners and curve transitions show clean, uninterrupted cuts with no step marks, double-cut notches, or ragged paper fibers from blade joints.
- Intact tips and core plies: Outward points and narrow projections show crisp edges with no mushrooming, flattened corners, or split greyboard layers—especially on 2.5 mm (0.098 in) and 3.0 mm (0.118 in) boards.
- Clean matrix release: Tokens punch out cleanly without tearing the surrounding 3–4 mm (0.118–0.157 in) waste web or lifting the printed wrap at tight tips.
- Registration within safety: Printed borders and details remain clear of the >=3 mm (0.118 in) safety zone around every tight radius and corner.
Concrete Failure Modes
- Visible step marks and burrs at spliced joints: When an inward corner or curve exceeds the bend limit of continuous steel rule, two separate blade segments must be butted together. Any microscopic gap or height mismatch at the joint leaves a step mark, uncut fibers, or a snag point when punching out the token.
- Crushed or split tips on acute spikes: On narrow outward points, the converging bevels of the two cutting edges compress the paperboard from both sides. In thicker 2.5 mm (0.098 in) and 3.0 mm (0.118 in) greyboard, this lateral pressure crushes the tip flat or splits the core plies apart.
- Waste matrix collapse: Routing two acute corners closer than the 3–4 mm (0.118–0.157 in) die gap leaves a thin bridge of greyboard that tears during press ejection, jamming the die or damaging adjacent pieces.
- Wrap chipping on punch-out: Tight outward tips concentrate stress on the surface paper wrap when the token is pushed free of the sheet, causing the printed face to chip or peel away from the core.
Parent guide Irregular Contour Punchboard Silhouettes