Specifications and Paper Grades
Standard sheeted paper sticker face stocks use 80–120 gsm coated paper, paired with a backing liner and pressure-sensitive adhesive. When comparing North American paper specs against metric gsm, distinguish US Text LB (basis sheet size 25 × 38 in / 635 × 965.2 mm) from US Cover LB (basis sheet size 20 × 26 in / 508 × 660.4 mm): an 80–120 gsm face stock falls in the lightweight Text range (roughly 54–80 lb Text), whereas Cover LB measures stiffer board weights on a smaller basis sheet (weight conversion: 1 kg = 2.205 lb).
| Face Stock Finish | Typical Face Weight | Ink Holdout & Surface Behavior | Best-Fit Application | Moisture & Scuff Sensitivity |
|---|---|---|---|---|
| Semi-gloss coated paper | 80–100 gsm | High ink holdout, bright color contrast, smooth sheen | Full-color game tokens, seals, label sheets | Absorbs moisture at cut edges; light rub needs varnish |
| Matte coated paper | 80–120 gsm | Low glare, sharp fine text, slightly higher ink absorption | Writable labels, dark-toned graphics, muted finishes | Scuffs easily on dark solids without anti-scuff matte coat |
Prepress and Artwork Rules
- File format and color: Submit AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts, CMYK process colors, and separate spot layers for any die-cut or kiss-cut lines.
- Resolution and ink limits: Keep raster artwork at ≥300 DPI. Set fine text to 100% K, build rich black at C40–60 M30–40 Y30–40 K100, and cap total area coverage (TAC) at ≤280%–300%.
- Bleed and safety: Extend full-bleed artwork 3 mm (0.118 in) past each cut edge and keep critical text or borders ≥3 mm (0.118 in) inside the cut line.
Production Steps and Offset Ink Drying
- Press conditioning and sheeted offset printing: Acclimate coated sticker sheets to pressroom humidity before feeding so the paper face and backing liner stay flat during registration. Run CMYK and any spot layers within the ≤280%–300% TAC ceiling to prevent excess ink film on the coated surface.
- Offset ink drying: Allow printed sheets to dry in controlled lifts before mechanical handling. Semi-gloss coatings hold ink on top of the clay surface, which sharpens dots but slows absorption; matte coatings absorb vehicle faster yet still require full set-up before kiss-cutting to avoid roller marking.
- Protective coating: Apply an inline overprint varnish or anti-scuff matte film when designs carry heavy dark solids or rich black backgrounds.
- Kiss-cutting and sheeting: Die-cut through the coated face stock down to the release liner without scoring the liner fibers, then trim sticker sheets to final size and pack flat in moisture-barrier wraps.
Sign-Off Criteria
- Ink cure and rub check: Printed sheets show zero ink transfer onto adjacent sheets or die-cut tooling after drying, and dark solids resist finger scuffing.
- Flatness and registration: Sheeted stickers lie flat with no edge lift or curl, and kiss-cut lines clear all safety elements by ≥3 mm (0.118 in).
- Prepress compliance: Production PDFs pass PDF/X-1a or PDF/X-4 preflight with TAC ≤280%–300%, 3 mm (0.118 in) bleed, and ≥300 DPI images.
- Regulatory records (when applicable): For stickers packed into children's games or toys destined for the EU, maintain EU Toy Safety (EN 71) assessment and testing documentation covering the ink, adhesive, and paper stock as part of the game's technical file.
Failure Modes
- Humidity curl on sheeted stickers: Because coated paper face stocks expand and contract with ambient moisture at a different rate than the release liner, unsealed sheets exposed to high humidity curl toward or away from the liner along the cut edges.
- Ink set-off and roller scuffing: Stacking heavy lifts or feeding sheets into the kiss-cutter before offset ink cures transfers wet ink onto the back of the next sheet and leaves track marks across dark artwork.
- Scuffing and edge-wear on dark solids: Uncoated or unprotected matte paper face stocks show bright rub marks along rich black areas during collation and shipping; adding an anti-scuff matte finish prevents surface burnishing.
- Liner score-through: Excessive die pressure cuts into the backing liner beneath the 80–120 gsm paper face, causing sheets to snap along kiss-cut lines when peeled.
Parent guide Sheeted Sticker Face Stocks