Sheeted stickers sit alongside other flat paper and film extras within the materials hub. While the release liner and adhesive determine how flat a sheet stays in transit, the face stock controls print durability, color opacity, and die-cutting behavior.
Face-Stock Material Families and Thickness Grades
1. Paper Face Stocks (Uncoated Matte and Coated Art Paper)
- Ordered grades: Typically 80–120 gsm (approximately 0.08–0.13 mm / 0.0031–0.0051 in face thickness before adhesive and liner). In US paper weight terms, these sit in Text LB (measured on a 25 × 38 in basis sheet, roughly 54–81 lb Text) rather than Cover LB (measured on a 20 × 26 in basis sheet).
- Ink-curing system: Accepts conventional offset or UV/LED-UV inks. Uncoated matte papers absorb ink into the fibers, softening contrast and requiring strict total area coverage (TAC) control. Coated semi-gloss or matte art papers hold sharper halftone dots at ≥300 DPI.
- White-ink underbase: Not required; the opaque white paper base provides full color reflectance.
- Kiss-cut blade angle: 30°–45° standard steel or carbide blades cleanly sever paper fibers without crushing the release liner.
- Best fit: Indoor game-box extras, seal labels, and writable or matte-finish reward sheets where low unit weight and crisp folding or flat packing matter.
2. Synthetic Polyolefin Films (White Matte or Gloss PP / BOPP / PE)
- Ordered grades: Typically 0.05–0.10 mm (0.0020–0.0039 in) film caliper. Polyolefin films are ordered by thickness in millimetres or microns rather than gsm, though total sheet weight includes the adhesive and liner.
- Ink-curing system: Non-porous polyolefin requires UV, LED-UV, or compatible surface-treated (corona-treated or topcoated) ink systems. Conventional air-dry offset inks will scuff or rub off.
- White-ink underbase: White-pigmented polyolefin films do not require a white underbase for standard CMYK artwork, though high-opacity grades are used when stickers cover dark or patterned surfaces.
- Kiss-cut blade angle: 45°–60° acute blades with controlled downforce. Polyolefin stretches under dull or shallow blades, causing ragged edges or "stringing" during matrix stripping.
- Best fit: Water-resistant, tear-resistant crowdfunding rewards, deck-box decals, and curved surfaces (PE conforms better to tight curves; BOPP stays flatter on rigid panels).
3. Clear and Metallic Sticker Films (Clear BOPP/PET, Brushed or Mirror Metallic Film)
- Ordered grades: Typically 0.05–0.08 mm (0.0020–0.0031 in) face film. Polyester (PET) films are stiffer and more dimensionally stable than BOPP, making them less prone to stretching during kiss-cutting.
- Ink-curing system: UV or LED-UV curing over adhesion-promoting topcoats. High-gloss clear and metallic surfaces show micro-scratches easily if under-cured or stacked without protective overprint varnish or lamination.
- White-ink underbase: Mandatory separate spot white layer behind any CMYK element that must remain opaque. Printing CMYK directly onto clear film produces translucent colors; printing directly onto metallic film creates a tinted foil effect.
- Kiss-cut blade angle: 45°–60° micro-bevel carbide blades. Metallic laminates and rigid PET dull cutting edges faster than paper and require tight depth calibration to sever the face film without delaminating the metallic layer or scoring the liner.
- Best fit: Premium collector sheets, window/transparent overlays, and foil-effect reward tiers.
Face-Stock Comparison Table
| Material Family | Typical Face Caliper | Ink-Curing System | White-Ink Underbase | Kiss-Cut Blade Angle | Primary Tradeoff |
|---|---|---|---|---|---|
| Paper (Uncoated / Coated) | 0.08–0.13 mm (0.0031–0.0051 in); 80–120 gsm | Offset or UV/LED-UV | None | 30°–45° | Lowest tear and moisture resistance; cleanest fiber cut |
| Synthetic Polyolefin (PP/BOPP/PE) | 0.05–0.10 mm (0.0020–0.0039 in) | UV/LED-UV on topcoated film | None (white film) / Spot white (clear PP) | 45°–60° | Stretch-prone if blade is dull; strong moisture resistance |
| Clear & Metallic Films (PET/BOPP) | 0.05–0.08 mm (0.0020–0.0031 in) | UV/LED-UV with adhesion topcoat | Mandatory spot white for opaque areas | 45°–60° (carbide) | Fastest blade wear; requires tight white-to-CMYK registration |
Prepress, File Setup, and Physical Tolerances
- File formats: Submit AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Color and resolution: Build artwork in CMYK at ≥300 DPI. Place the white underbase (
White) and kiss-cut path (CutContour) on separate, clearly named spot layers set to overprint where required. - Black and ink limits: Use 100% K for fine text and thin linework. Use rich black (C40–60 M30–40 Y30–40 K100) for solid dark fills, keeping TAC ≤280%–300% to prevent ink set-off on coated papers and curing failure on synthetic films.
- Bleed and safety: Provide 3 mm (0.118 in) bleed per side around every full-bleed sticker and sheet perimeter. Keep critical text and borders at least ≥3 mm (0.118 in) inside the kiss-cut line.
- Corner geometry: Specify R3–R3.5 mm (0.118–0.138 in) rounded corners on individual stickers to reduce corner-lift and catching during packing and handling.
- Fulfillment weight calculation: When estimating parcel weights for crowdfunding tiers, include the face stock, adhesive, and release liner together:
Total sheet mass (kg) = Sheet area (m2) * Combined gsm / 1,000Convert kilograms to pounds using1 kg = 2.205 lb(for example, a 10 kg carton equals 22.05 lb).
Job-Specific Production Steps and Sign-Off Criteria
- Material and Liner Pairing: Match the face stock to a glassine or PET release liner of sufficient caliper so sheets remain flat under stacking pressure.
- Prepress and Spot Separation Check: Verify separate spot layers for
Whiteunderbase (choked 0.1–0.2 mm / 0.004–0.008 in inside CMYK edges to prevent white halos) andCutContourpaths, plus 3 mm (0.118 in) bleed and TAC ≤280%–300%. - Print and Curing Calibration: Run a press check on the target face stock to confirm UV/LED-UV lamp energy cures the ink completely without heat-warping thin polyolefin or clear BOPP.
- Kiss-Cutting and Matrix Calibration: Set blade angle (30°–45° for paper; 45°–60° for synthetic/metallic films) and adjust cutting pressure so the blade penetrates the face stock and adhesive layer while leaving the release liner intact.
Sign-Off Criteria
- Clean peel release: Every sticker lifts from the sheet without tearing the face stock, splitting the paper backing, or pulling liner fibers.
- Spot white registration: No visible white edge protrudes beyond CMYK artwork on clear or metallic stocks.
- Ink adhesion and rub resistance: Cured ink resists dry rub and light fingernail abrasion on synthetic and metallic surfaces.
- Sheet flatness: Finished sheets lie flat without edge curl that could jam automated pack-out or lift inside game boxes.
Concrete Failure Modes
- Ink Scuffing or Flaking on Polyolefin and PET: Caused by using conventional air-dry ink or insufficient UV curing on low-surface-energy films. Fix by specifying UV/LED-UV curing and topcoated synthetic stocks.
- Muddy or Translucent Colors on Clear and Metallic Films: Caused by printing CMYK without a spot white underbase. Fix by adding a dedicated spot white layer behind all opaque artwork.
- Liner Cut-Through or Edge Stringing: Caused by using a shallow paper blade on ductile polyolefin or excessive downforce on thin liners. Fix by switching to a 45°–60° blade and verifying kiss-cut depth on press sheets before full-run cutting.
- Corner Lifting During Fulfillment: Caused by sharp 90° sticker corners or moisture mismatch between paper face stocks and liners. Fix by applying R3–R3.5 mm (0.118–0.138 in) corner radii and packing sheets flat in moisture-resistant wraps.
Compliance and Packaging Records (Conditional)
- Toy safety (EU): When sheeted stickers are packaged with games or products marketed for children under 14 in the EU, EN 71 assessment and testing procedures apply; see the European Commission Toy Safety framework.
- Packaging registration and sorting labels: When shipping packaged sticker sheets into Germany or France, producer registration and sorting-mark rules may require records under VerpackG / LUCID and France Info-Tri / Triman.
Guides in this section
Parent guide Jigsaw Puzzle and Crowdfunding Paper Extra Materials