For overall sheet registration, bleed, and cutting-rule placement across multi-up layouts, see postcard trim and perforation tolerances.
Stock Thickness, Basis Weight, and Ratio Mechanics
Perforation performance shifts directly with board caliper and internal core construction. When specifying paper weight, distinguish US Cover LB (based on a 20 x 26 in / 508 x 660 mm basis sheet) from US Text LB (based on a 25 x 38 in / 635 x 965 mm basis sheet), as the same gsm translates to a much lower Cover LB number than Text LB number.
| Stock Construction | Weight (gsm / approx. US Cover LB, 20 x 26 in basis) | Approximate Caliper (mm / in) | Perforation Rule & Ratio Behavior |
|---|---|---|---|
| Art / blue-core stock | 300 gsm (~111 lb Cover) | 0.28–0.31 mm (0.0110–0.0122 in) | Standard fine-tooth micro-perf; balanced cut-to-tie ratio holds multi-card sheets flat while snapping cleanly |
| Black-core linen stock | 310 gsm (~115 lb Cover) | 0.30–0.32 mm (0.0118–0.0126 in) | Textured surface and dense core require clean rule penetration so embossed valleys do not leave uncut fibers |
| Black-core stock | 330 gsm (~122 lb Cover) | 0.32–0.34 mm (0.0126–0.0134 in) | Higher fiber density resists tearing; requires slightly longer cut segments relative to tie width |
| Heavy art stock | 350 gsm (~129 lb Cover) | 0.34–0.38 mm (0.0134–0.0150 in) | Thicker caliper increases lateral tear resistance; lower TPI with wider cuts prevents ragged edge delamination |
| Extra-heavy art stock | 400 gsm (~148 lb Cover) | 0.40–0.44 mm (0.0157–0.0173 in) | High board stiffness stresses small ties in transit; requires deeper bevel penetration and calibrated tie strength |
| Double-sided film lamination | Added over base stock | +0.03–0.05 mm (+0.0012–0.0020 in) per card | Film stretches across uncut ties; requires full cut penetration through both film layers to avoid stringing |
The mechanical balance between sheet retention and tear cleanliness is governed by the open-cut ratio:
Open-Cut Ratio (%) = Cut Length / (Cut Length + Tie Length) * 100
Teeth Per Inch (TPI) = 25.4 mm / (Cut Length in mm + Tie Length in mm)
- Higher open-cut ratio (longer cuts, narrower ties): Reduces the force needed to separate cards and leaves fewer visible fiber tufts on 350–400 gsm (0.34–0.44 mm / 0.0134–0.0173 in) boards, but reduces sheet rigidity during packing and transit.
- Lower open-cut ratio (shorter cuts, wider ties): Increases sheet durability for heavy multi-card layouts and cross-grain perforations, but raises the risk of surface coating tear on 300–330 gsm (0.28–0.34 mm / 0.0110–0.0134 in) stocks if ties are too wide for the board caliper.
- Grain direction effect: Perforations running parallel to the paper grain split along natural fiber lines with less force and cleaner edges than perforations running across the grain, which cut through fiber bundles and benefit from a slightly higher open-cut ratio.
Job-Specific Production Steps
- Prepress and Dieline Separation: Build print artwork in CMYK at ≥300 DPI using AI, PDF, or PSD source files exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded. Place perforation lines on a dedicated non-printing spot layer separate from outer trim lines.
- Safety and Ink Coverage Setup: Maintain 3 mm (0.118 in) bleed on outer edges and keep critical text and graphics at least 3 mm (0.118 in) away from perforation lines—increasing to ≥4–5 mm (0.157–0.197 in) on bordered backs so slight tear-edge roughness stays clear of frame lines. Use 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and keep total area coverage (TAC) at ≤280%–300% so heavy ink does not crack along the perforation. Apply anti-scuff matte lamination on dark artwork.
- Rule Selection and Die Make-Ready: Match the micro-perforation rule height, bevel angle, and tooth pitch to the total caliper (base stock plus 0.03–0.05 mm / 0.0012–0.0020 in when double-sided film is used). Calibrate die-cutting pressure on make-ready sheets so the rule cuts cleanly through both top and bottom coatings—and both film layers if laminated—without crushing adjacent board fibers.
- Sheet Handling and Transit Packing: Pack perforated multi-card sheets flat in rigid cartons, keeping individual carton weights within safe manual handling limits (typically under 15–20 kg / 33–44 lb) and avoiding slack space that lets sheets flex along perforation lines during shipping.
Sign-Off Criteria
- Transit Retention: Flexing a finished sheet gently along the perforated axis does not pop ties open prematurely, and bottom sheets in a packed stack show no crushed or split bridges.
- Clean Separation: Detaching a postcard along the rule separates the board along the intended line without pulling surface paper, cracking ink, or leaving ragged fiber tufts protruding beyond the tear edge.
- Film Severance (Laminated Jobs): On double-sided laminated sheets, every cut segment penetrates both film faces completely so the plastic film snaps at each tie rather than stretching or peeling away from the paper core.
- Registration Accuracy: The perforation line remains parallel to artwork margins and within the ≥3 mm (0.118 in) safety zone (or ≥4–5 mm / 0.157–0.197 in for bordered backs) across the sheet.
Concrete Failure Modes
- Premature Separation in Transit: Caused by an overly high open-cut ratio, ties nicked during die make-ready, or heavy 350–400 gsm (0.34–0.44 mm / 0.0134–0.0173 in) sheets flexing in under-filled cartons. Fix by widening tie bridges or reducing carton stack shift.
- Ragged Paper Fibers and Surface Peeling: Caused by ties that are too wide for the board's caliper, cross-grain tearing without ratio compensation, or dull perforation rule teeth crushing rather than slicing fibers. Fix by increasing the open-cut ratio or replacing worn rule.
- Film Bridging and Edge Delamination: Caused when double-sided film (+0.03–0.05 mm / 0.0012–0.0020 in) is not fully severed by the perforation rule, causing the laminate to stretch and lift the printed paper layer when pulled. Fix by increasing die-cutting penetration depth to clear the bottom film layer.
- Ink Cracking Along the Tear Line: Caused by exceeding 280%–300% TAC across the perforation path or placing borders closer than 4–5 mm (0.157–0.197 in) to the rule on unlaminated dark solids. Fix by reducing ink density at the fold/tear zone or adding anti-scuff matte lamination.
Parent guide Postcard Trim and Perforation Tolerances