When to Change the Default Build
- Switch from linen to smooth stock when card faces carry fine-line engravings, small corner indices, or multi-line caption banners that lose edge crispness over an embossed crosshatch texture.
- Step up from a folding tuck box to a pocket rigid box when pairing the deck with a 16-page saddle-stitched booklet, adding gilded edges, or targeting gift-grade shelf durability.
- Choose 330 gsm black core over 300 gsm art/blue core when cards feature dark, full-bleed backs or require maximum snap and opacity during repeated overhand shuffling.
- Adjust internal box depth whenever adding double-sided protective film (+0.03–0.05 mm / 0.0012–0.0020 in per card) or inserting an 8-panel leaflet or 16-page booklet, rather than forcing the companion insert into a bare-deck cavity.
Bill of Materials and Default Specifications
Every Sibilla production file should lock the 52-card deck, packaging, and companion paper tolerances into one unified bill of materials (BOM). In US paper specifications, card stocks are measured on the Cover basis sheet (20 x 26 in), whereas interior booklet and leaflet papers are measured on the Text basis sheet (25 x 38 in).
| Component | Default Specification | Caliper / Thickness | Weight / Basis Equivalent |
|---|---|---|---|
| 52-Card Deck | 57 x 89 mm (2.24 x 3.50 in), R3–R3.5 mm (0.118–0.138 in) corners | 0.28–0.34 mm (0.0110–0.0134 in) per card | 300–330 gsm (approx. 111–122 lb Cover, 20 x 26 in basis); bare deck ~0.079–0.087 kg (0.17–0.19 lb) |
| Tuck Box | Folding cartonboard with thumb notch and locking tabs | 0.34–0.44 mm (0.0134–0.0173 in) board | 350–400 gsm (approx. 129–148 lb Cover, 20 x 26 in basis) |
| Pocket Rigid Box | Two-piece lid-and-base or magnetic clamshell | 1.5–2.0 mm (0.059–0.079 in) greyboard core; 15–20 mm (0.59–0.79 in) wrap margin | Printed wrap on 120–150 gsm (81–101 lb Text, 25 x 38 in basis); finished boxed deck ~0.12–0.16 kg (0.26–0.35 lb) |
| 8-Panel Leaflet | Accordion or roll-fold, trimmed inside box footprint | 0.08–0.13 mm (0.0031–0.0051 in) per sheet | 80–120 gsm (approx. 54–81 lb Text, 25 x 38 in basis) |
| 16p Saddle-Stitched Booklet | 4 interior signatures + separate cover (multiples of 4 pages) | Interior 0.08–0.13 mm (0.0031–0.0051 in); cover 0.20–0.31 mm (0.0079–0.0122 in) | Interior 80–120 gsm (54–81 lb Text); cover 200–300 gsm (approx. 74–111 lb Cover, 20 x 26 in basis) |
Card Stock Selection and Smooth vs. Linen Legibility
- 300 gsm art / blue core (0.28–0.31 mm / 0.0110–0.0122 in): Delivers a flexible parlor feel and clean ink holdout on smooth surfaces, keeping the 52-card stack compact.
- 310 gsm black-core linen (0.30–0.32 mm / 0.0118–0.0126 in): Adds a tactile crosshatch emboss that reduces surface friction for shuffling and hides minor handling scuffs. However, the linen peaks scatter light across 6–8 pt caption text, serif numerals, and fine-line borders. Use linen only when typography is bold and illustrations rely on clear tonal blocks.
- 330 gsm black core (0.32–0.34 mm / 0.0126–0.0134 in): Provides higher stiffness and opaque light-blocking for high-contrast backs. Paired with a smooth matte varnish or anti-scuff matte film, it preserves fine caption legibility on traditional Sibilla layouts.
- Surface coatings and edge gilding: Anti-scuff matte lamination suits dark artwork without glossy glare. Adding double-sided film increases card caliper by 0.03–0.05 mm (0.0012–0.0020 in) per card. When specifying gilded edges, avoid thick film lamination, which can peel or delaminate under foil-stamping heat and edge-sanding.
52-Card Stack Thickness and Box-Plus-Leaflet Fit
Calculate bare-deck stack height and internal box cavity using plain-text tolerances:
Bare Stack Height = 52 x Card Caliper (plus +0.03 to +0.05 mm per card if double-sided film is applied)
Internal Box Depth (Bare Deck) = Bare Stack Height + 1.5–3.0 mm (0.06–0.12 in) stack clearance
Internal Box Width / Height = Card Trim + 1.5–2.5 mm (0.06–0.10 in) lateral clearance
- Unfilmed 52-card stack: 14.56–16.12 mm (0.57–0.63 in) on 300 gsm; 15.60–16.64 mm (0.61–0.66 in) on 310 gsm linen; 16.64–17.68 mm (0.66–0.70 in) on 330 gsm. Adding 1.5–3.0 mm (0.06–0.12 in) stack clearance yields 16.5–20.5 mm (0.65–0.81 in) internal depth for the bare deck.
- Filmed 52-card stack: Double-sided film raises the 52-card stack by 1.56–2.60 mm (0.061–0.102 in), pushing total stack height to 16.12–20.28 mm (0.63–0.80 in). Verify the upper end of the 16.5–20.5 mm (0.65–0.81 in) cavity or expand depth to 21.5–23.0 mm (0.85–0.91 in) so cards do not bind.
- Width and height clearance: For a 57 x 89 mm (2.24 x 3.50 in) deck, set internal box dimensions to 58.5–59.5 x 90.5–91.5 mm (2.30–2.34 x 3.56–3.60 in) so cards drop in cleanly without corner rattle.
- Companion insert allowance: An 8-panel folded leaflet on 80–120 gsm stock adds roughly 0.64–1.04 mm (0.025–0.041 in) of flat paper plus fold springback; reserve 1.5–2.0 mm (0.06–0.08 in) of extra internal depth. A 16-page saddle-stitched booklet (4 interior sheets plus 1 cover sheet and wire-stitch crown) requires 2.0–3.0 mm (0.08–0.12 in) of extra internal depth, plus a trimmed footprint slightly smaller than the internal box width and height so pages lie flat without curling at the corners.
Prepress and Print File Specifications
- Trim, bleed, and safety: 57 x 89 mm (2.24 x 3.50 in) trim; 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) inner safety margin for faces, increasing to ≥4–5 mm (0.157–0.197 in) for bordered card backs.
- Color and ink limits: CMYK with separate spot layers (for metallic inks, foil, or spot UV) at ≥300 DPI. Set fine caption text and hairlines to 100% K (no four-color black). Use rich black (C40–60 M30–40 Y30–40 K100) for solid dark backgrounds, keeping Total Area Coverage (TAC) at ≤280%–300%.
- File formats: Print-ready AI, PDF, or PSD exported to PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
Production Workflow and Sign-Off Criteria
- Prepress and imposition: Partner prepress imposes the 52 card faces and backs onto a single press sheet (leaving spare slots for title/extra cards if needed) alongside the box dieline and 8-panel leaflet or 16-page booklet signatures.
- Proofing sign-off: Approve a hard-copy wet proof or calibrated color proof and an unprinted white dummy of the box-plus-insert assembly. Confirm 100% K caption sharpness, TAC limits on dark borders, and smooth-vs.-linen legibility before plating.
- Offset press and finishing: Print CMYK + spot layers, cure inks, apply aqueous varnish or anti-scuff matte film, and die-cut cards with R3–R3.5 mm (0.118–0.138 in) rounded corners.
- Box and insert assembly: Wrap 1.5–2.0 mm (0.059–0.079 in) greyboard with 15–20 mm (0.59–0.79 in) wrap margins (or die-cut and glue folding tuck cartons), fold 8-panel leaflets or saddle-stitch 16-page booklets, and collate into the finished box.
- Final physical sign-off: Verify 52-card stack caliper against the internal box depth, check that the lid closes or the tuck flap locks flush with the leaflet/booklet inside, and inspect narrow 57 mm (2.24 in) bordered backs for die-cut centering.
Regulatory and Packaging Compliance Records
When distributing decks into regulated markets, maintain the applicable assessment and packaging records with your compliance files:
- Toy safety (EU): If the product is marketed for children or falls under toy classification, compile EN 71 assessment and third-party lab testing records per the European Commission Toy Safety framework.
- Packaging EPR (Germany & France): Register retail packaging weights under Germany's VerpackG in the LUCID Packaging Register, and print required sorting marks on consumer boxes sold in France per France Info-Tri / Triman.
Concrete Failure Modes
- Broken captions on linen stock: Fine-line illustrations and small caption banners printed on 310 gsm linen lose stroke continuity across the embossed texture. Fix: Switch to 300 gsm or 330 gsm smooth stock with matte varnish, or increase caption weight and size before plating.
- Box bowing or crushed tuck flaps: Designing the box cavity to the bare-deck 16.5–20.5 mm (0.65–0.81 in) range without adding 1.5–3.0 mm (0.06–0.12 in) for an 8-panel leaflet or 16-page booklet causes lids to sit proud and tuck tabs to pop open. Fix: Lock the insert type before cutting box tooling and test a weighted white dummy.
- Visible border drift on narrow trim: On a 57 mm (2.24 in) wide card, a 0.5 mm (0.020 in) die-cut shift makes thin outer frames look lopsided. Fix: Keep bordered backs at ≥4–5 mm (0.157–0.197 in) safety or use borderless full-bleed artwork.
- Lamination conflict with gilded edges: Thick double-sided film lifts or scorches along the card perimeter during metallic edge gilding. Fix: Use uncoated varnish instead of thick film when specifying gilded edges.
- Scuffing and ink set-off on dark backs: Over-inked dark backgrounds (>300% TAC) or 4-color black caption text scuff during collating and shuffling. Fix: Cap TAC at ≤280%–300%, use 100% K for fine text, and specify anti-scuff matte coating.