Choose 330 gsm black-core cards when the set relies on crisp snap, opaque blockout, and standard offset finishing; switch to 0.30 mm (0.0118 in) PVC when the game faces wet tables, frequent flexing, or high-wear handling. Choose a stitched pocket wallet for flexible carry and repeat insertion, or a folded heavy-board folio when a flat, printable exterior spine and lower tooling complexity are priorities. Standard offset card production starts at 200 decks (typical tiers: 200, 300, 500, and 1,000+), while custom wallet stitching or folio die-cutting follows component minimums.
Default Bill of Materials and Stock Specs
Card trim dimensions vary by game layout; size the wallet pocket or folio panels directly from the finished card trim rather than forcing a single default card format. Distinguish US paper weights by basis sheet size: Text LB uses a 25 x 38 in (635 x 965 mm) basis sheet, whereas Cover LB uses a 20 x 26 in (508 x 660 mm) basis sheet.
| Component | Default Material | Basis Weight (gsm / US LB) | Caliper (mm / in) |
Finish & Notes |
|---|---|---|---|---|
| Cards (12–18 count) | 330 gsm black-core card stock | 330 gsm (~122 lb Cover; 55.3 kg / 122 lb per 500-sheet basis ream) |
0.32–0.34 mm (0.0126–0.0134 in) base; +0.03–0.05 mm (0.0012–0.0020 in) with double-sided film |
Anti-scuff matte varnish or film for dark artwork; R3–R3.5 mm (0.118–0.138 in) corners |
| Cards (waterproof alt.) | Rigid PVC card stock | Synthetic sheet (no gsm/LB paper equivalent) | 0.30 mm (0.0118 in) |
High-durability matte or smooth coating; avoids edge-splitting under moisture |
| Enclosure (Option A) | Stitched pocket wallet | Component-specific stitched shell | Sized to packed stack + pocket allowance | Reinforced perimeter stitching; no rigid greyboard required |
| Enclosure (Option B) | Folded heavy-board folio | 350–400 gsm (~130–148 lb Cover; 59.0–67.1 kg / 130–148 lb per 500-sheet basis ream) |
0.34–0.38 mm (0.0134–0.0150 in) at 350 gsm; 0.40–0.44 mm (0.0157–0.0173 in) at 400 gsm |
Scored spine/hinges; double-sided protective film adds 0.03–0.05 mm (0.0012–0.0020 in) |
| Mini-Leaflet | Uncoated or matte text paper | 80–120 gsm (~54–81 lb Text; 24.5–36.7 kg / 54–81 lb per 500-sheet basis ream) |
0.08–0.13 mm (0.0031–0.0051 in) per sheet |
Accordion-folded to 4, 6, or 8 panels; trimmed smaller than card width/height |
Pocket Clearance, Stack Height, and Fold-Crease Tolerances
Enclosure sizing depends on the combined stack height of the cards plus the folded mini-leaflet, not card count alone.
- Stack Height Calculation:
Total Stack Height = (Card Count * Card Caliper) + (Leaflet Panels * Leaflet Sheet Caliper)For 12 to 18 unfilmed 330 gsm black-core cards, the card stack alone measures3.84–6.12 mm(0.151–0.241 in), rising to4.20–7.02 mm(0.165–0.276 in) with double-sided film. For 12 to 18 PVC cards at0.30 mm(0.0118 in), the card stack measures3.60–5.40 mm(0.142–0.213 in). Adding an 8-panel leaflet on0.10 mm(0.0039 in) stock adds0.80 mm(0.031 in) before fold spring-back. - Pocket and Folio Clearances: Allow
1.5–2.5 mm(0.059–0.098 in) across both width and height between the card/leaflet edges and the stitched seam or folio crease. Allow1.5–3 mm(0.059–0.118 in) on stack height (pocket gusset or folio spine depth) so the top card slides in without catching. - Fold-Crease Tolerances (Folio & Leaflet):
- Heavy-Board Folio: Score 350–400 gsm boards parallel to the paper grain direction wherever layout permits, using a double-score channel matched to the
Total Stack Height + 1.5–3 mm(0.059–0.118 in) spine allowance. Keep critical typography at least3 mm(0.118 in) away from score lines. - Accordion Mini-Leaflet: Limit accordion folds to 4, 6, or 8 panels on
80–120 gsm(54–81 lbText) stock. Exceeding 8 panels or using heavier cover stock (200–300 gsm,74–111 lbCover) creates excessive spring-back that pushes the wallet flap open.
- Heavy-Board Folio: Score 350–400 gsm boards parallel to the paper grain direction wherever layout permits, using a double-score channel matched to the
Prepress, Production Steps, and Sign-Off Criteria
- File Setup: Export print-ready files in AI, PDF, or PSD using
PDF/X-1aorPDF/X-4with fonts outlined or embedded and images at>= 300 DPI. Convert all process artwork to CMYK with separate spot layers for die-lines, score lines, and specialty finishes. - Color & Ink Density: Set fine body text to
100% K. Build rich black backgrounds withC40–60 M30–40 Y30–40 K100, keeping Total Area Coverage (TAC) at<= 280%–300%. - Bleed, Safety, and Corners: Apply
3 mm(0.118 in) bleed per side on cards, folios, and leaflets. Maintain>= 3 mm(0.118 in) safety inside the trim on standard card layouts and>= 4–5 mm(0.157–0.197 in) safety on bordered backs to absorb die-cut shift. SpecifyR3–R3.5 mm(0.118–0.138 in) rounded corners on cards so they slide cleanly into stitched pockets. - Surface Finish Selection: Specify anti-scuff matte varnish or matte film on dark card and folio artwork. Avoid pairing thick lamination with gilded card edges, as thick film layers can conflict with edge-gilding adhesion.
- Pre-Run Sign-Off Criteria: Verify physical dummy fit using the exact target card count, coated/filmed caliper, and folded 4/6/8-panel leaflet before approving bulk cutting. Confirm that cards insert and withdraw with one hand, folio scores fold without fiber cracking, and bordered card backs show even margins within safety tolerances.
Failure Modes and Regulatory Records
Concrete Failure Modes
- Pocket Binding & Seam Strain: Omitting the
1.5–2.5 mm(0.059–0.098 in) width/height allowance or underestimating film thickness (+0.03–0.05 mm/0.0012–0.0020 inper card) causes tight pockets that bow cards or split wallet stitching. - Folio Spine Cracking: Folding
350–400 gsmboard across the grain without a double-score channel matched to the stack height cracks ink and outer film along the spine. - Leaflet Spring-Back: Using cover-weight stock (
200–300 gsm) or more than 8 panels for the mini-leaflet thickens the folded bundle and forces the wallet flap or folio tuck open. - Dark-Artwork Scuffing: Shipping uncoated or standard gloss-varnished dark cards in a tight friction-fit wallet produces visible rub marks along the outer cards during transit.
Regulatory Procedures and Source Records
Where applicable to the target market and user age group, maintain compliance documentation alongside production records:
- Toy Safety Assessment (EU): If the microgame is marketed or intended for children under 14, plan EN 71 mechanical, flammability, and chemical testing and retain test reports and technical documentation per the EU Toy Safety Directive.
- German Packaging Registration (VerpackG): Because the stitched wallet or folded folio acts as product packaging, verify producer registration and system participation records under the Zentrale Stelle Verpackungsregister (VerpackG) before shipping into Germany.
- French Sorting Signage (Triman): For sets distributed in France, include the required Triman logo and material-sorting instructions on the wallet, folio, or accompanying leaflet per the French Ministry of Ecological Transition Info-Tri guidance.
Parent guide Custom Game Card Set Printing