Standard offset card decks start at 200 decks (usual tiers: 200, 300, 500, and 1,000+), while boxed games and custom dual-layer tooling follow project and component minimums. For broader game assembly architecture, see custom tabletop game printing.
Finished-Product BOM & Default Specifications
Card Deck Press coordinates custom card and tabletop printing through specialist offset and tabletop manufacturing partners. Every dual-layer game BOM locks four structural groups together so component tolerances stack cleanly inside the rigid box.
Dual-Layer Player Boards
A dual-layer player board consists of a die-cut top layer (with recessed wells) laminated onto a solid backing board.
| Parameter | Default Specification (Metric / Imperial) | Production Condition |
|---|---|---|
| Greyboard Core Options | 1.5 mm (0.059 in), 2.0 mm (0.079 in), 2.5 mm (0.098 in), 3.0 mm (0.118 in) | Select top-layer thickness to match token/cube recess depth; select backing board for flatness. |
| Wrap Margin | 15–20 mm (0.591–0.787 in) | Required for clean edge turn-in on wrapped greyboard layers. |
| Well-to-Well & Edge Die Gap | 3–4 mm (0.118–0.157 in) minimum | Prevents narrow paperboard bridges from crushing or delaminating during die-cutting. |
| Surface Finish | Anti-scuff matte lamination | Recommended for dark artwork to resist rubbing during stacking and play. |
Paired Cards, Punchboards & Partner-Sourced Pieces
- Card Decks: Select deck format and card count based on hand ergonomics, table footprint, and box cavity layout without assuming a fixed default trim. Round corners to R3–R3.5 mm (0.118–0.138 in).
- 300 gsm art/blue core: 0.28–0.31 mm (0.011–0.012 in)
- 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in)
- 330 gsm black core: 0.32–0.34 mm (0.013 in)
- 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in)
- 400 gsm: 0.40–0.44 mm (0.016–0.017 in)
- PVC: 0.30 mm (0.012 in)
- Film Allowance: Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card. Thick lamination can conflict with gilded edges.
- Punchboards: Die-cut from 1.5–3.0 mm (0.059–0.118 in) greyboard with a 3–4 mm (0.118–0.157 in) die gap between tokens.
- Partner-Sourced Game Pieces: Wooden cubes, discs, and tokens must be measured against the actual top-layer greyboard plus wrap thickness so pieces sit flush inside the wells.
Rulebooks, Leaflets, Inserts & Rigid Boxes
- Leaflets & Rulebooks: Folded leaflets use 4, 6, or 8 panels. Bound rulebook signatures use multiples of four:
- Saddle stitch: 12–40 pages
- Perfect binding: 28+ pages
- Sewn binding: 80–100+ pages recommended
- Paper Weight Basis Distinction: Specify all stocks in gsm, and distinguish US Text LB (based on a 25 x 38 in / 635 x 965 mm basis sheet) from US Cover LB (based on a 20 x 26 in / 508 x 660 mm basis sheet):
- Interior stock: 80–120 gsm (US Text LB basis), caliper 0.08–0.13 mm (0.003–0.005 in) per sheet
- Rulebook covers: 200–300 gsm (US Cover LB basis)
- Rigid Boxes & Inserts: Use 1.5, 2.0, 2.5, or 3.0 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard with a 15–20 mm (0.591–0.787 in) wrap margin.
- Box Clearance: Maintain 1.5–2.5 mm (0.059–0.098 in) clearance across internal width and height, and 1.5–3.0 mm (0.059–0.118 in) clearance for total component stack height (stacked dual-layer boards, sleeved or unsleeved cards, rulebook, and insert).
- Freight & Pack-Out Weights: Record unit net weight and master carton gross weight in both kg and lb on the finalized BOM.
Prepress & File Specifications
- File Formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts.
- Color & Resolution: CMYK with separate spot layers (for foil, spot UV, and die lines) at >=300 DPI.
- Bleed & Safety: 3 mm (0.118 in) bleed per side; >=3 mm (0.118 in) safety margin (>=4–5 mm / 0.157–0.197 in for bordered card backs).
- Black & Ink Density: 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; Total Area Coverage (TAC) <=280%–300%.
Production Steps & Sign-Off Criteria
- BOM Lock & Stack-Height Calculation
- Sum the calipers of all stacked dual-layer boards, card decks (including 0.03–0.05 mm / 0.001–0.002 in per card if double-sided film is used), rulebooks, and inserts.
- Verify box internal dimensions include 1.5–2.5 mm (0.059–0.098 in) width/height clearance and 1.5–3.0 mm (0.059–0.118 in) stack-height clearance.
- Prepress & Die-Line Separation
- Confirm all recessed well cutouts maintain 3–4 mm (0.118–0.157 in) minimum spacing from adjacent wells and board edges.
- Check 3 mm (0.118 in) bleed, >=3 mm (0.118 in) safety (>=4–5 mm / 0.157–0.197 in on bordered card backs), separate spot layers, and TAC <=280%–300%.
- White Dummy & Pre-Production Sign-Off
- Test partner-sourced wooden cubes and tokens inside the die-cut white dummy wells to confirm flush seating without binding.
- Inspect laminated dual-layer board samples for flatness and balanced grain direction across top and backing sheets before full press release.
- Offset Printing, Lamination, Die-Cutting & Assembly
- Print, laminate (anti-scuff matte for dark artwork), die-cut the top layer, and press-laminate onto the backing board.
- Collate with cards, punchboards, rulebooks, inserts, and partner-sourced pieces; log final unit and carton weights in kg and lb.
Regulatory & Compliance Records
Where distribution markets require product safety or packaging compliance, maintain applicable technical documentation and registration records rather than assuming blanket coverage:
- Toy Safety (EU/EEA): When a game falls within toy safety scope, conduct applicable conformity assessment, physical/mechanical/chemical testing, and technical file compilation per the European Commission EU Toy Safety (EN 71) framework.
- Packaging Registration (Germany): Complete producer registration and packaging volume reporting under VerpackG through Verpackungsregister (LUCID).
- Sorting & Recycling Marking (France): Apply required consumer sorting instructions and Triman marking per Info-Tri / Triman guidance.
Concrete Failure Modes & Prevention
- Board Warping (Cupping or Twisting): Occurs when the top and bottom sheets have mismatched paper grain directions or unbalanced lamination (e.g., film on the top face without a balancing liner on the back). Prevention: Align grain direction across all layers and balance surface tension between the top wrap and backing liner.
- Crushed or Delaminated Well Bridges: Occurs when recessed cutouts are placed closer than 3–4 mm (0.118–0.157 in) apart or too near the outer trim, causing the die rule to crush the greyboard core. Prevention: Enforce >=3–4 mm (0.118–0.157 in) bridges in the die line before tooling sign-off.
- Tokens Binding or Protruding Above Wells: Occurs when glue squeeze-out narrows the recessed walls or when top-layer greyboard thickness does not match token height. Prevention: Verify token caliper against the laminated top-layer thickness on the white dummy and control adhesive application around well perimeters.
- Box Lid Tightness or Crushed Corners: Occurs when stack-height math omits 0.03–0.05 mm (0.001–0.002 in) per card for film lamination or wrap buildup on stacked dual-layer boards. Prevention: Include all lamination and wrap allowances in the stack total and enforce 1.5–3.0 mm (0.059–0.118 in) vertical clearance.
- Scuffing on Dark Artwork & Gilded-Edge Failure: Occurs when dark ink exceeds 280%–300% TAC without protective film, or when thick lamination interferes with gilded card edges. Prevention: Use anti-scuff matte lamination on dark boards and cards, cap TAC at 280%–300%, and avoid thick lamination on gilded-edge decks.