This bill-of-materials (BOM) configuration works when all shared game state lives in the card deck and individual player tracking lives on recessed boards. Switch to a full-size dual-layer board game layout if the game requires a shared central track, if the player boards are wider than the combined card-and-cube tray footprint, or if the stacked board height pushes the rigid box beyond standard shelf proportions.


Bill of Materials and Component Specifications

Dual-Layer Recessed Player Boards

Dual-layer player boards pair a die-cut top greyboard layer (forming recessed wells for wooden cubes or tokens) with a solid base greyboard layer, wrapped in printed art paper.

  • Greyboard Thickness: Select 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) per layer depending on recess depth and rigidity targets. A 1.5 mm (0.059 in) top layer over a 1.5 mm (0.059 in) or 2 mm (0.079 in) base keeps total stack height low while holding wooden cubes flush.
  • Wrap Margin: 15–20 mm (0.591–0.787 in) turn-in around the outer perimeter.
  • Minimum Die-Cut Bridge Width: Maintain at least 3–4 mm (0.118–0.157 in) between adjacent recessed pockets and from any pocket edge to the board perimeter so the top greyboard does not tear during die-cutting or delaminate during wrapping.
  • Surface Finish: Anti-scuff matte lamination is recommended for dark artwork to prevent rubbing marks where stacked boards contact each other in transit.

Card Decks

Standard offset card runs start at 200 decks (typical production tiers: 200, 300, 500, 1,000+), while complete boxed sets and custom die-cutting tooling follow project and component minimums.

Because card trim size varies by game, the selected deck format sets the lower insert well dimensions directly. Determine whether the card well must accommodate unsleeved cards or sleeved cards before locking the lower tray footprint and overall box height.

Card Stock Weight (gsm) Caliper (mm) Caliper (in)
Art / blue-core 300 gsm 0.28–0.31 mm 0.011–0.012 in
Black-core linen 310 gsm 0.30–0.32 mm 0.012–0.013 in
Black-core 330 gsm 0.32–0.34 mm 0.013–0.013 in
Art stock 350 gsm 0.34–0.38 mm 0.013–0.015 in
Heavy art stock 400 gsm 0.40–0.44 mm 0.016–0.017 in
PVC — 0.30 mm 0.012 in
  • Lamination Allowance: Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card. Multiply this allowance by the total card count before setting the lower well depth. Thick lamination can conflict with gilded edges.
  • Corner Radius: R3–R3.5 mm (0.118–0.138 in).

Partitioned Lower Tray, Wooden Cubes, and Rigid Box

Partner-sourced wooden cubes and non-paper markers sit in dedicated compartments beneath the player-board stack. The upper rim of the lower insert acts as a continuous flat shelf supporting the bottom player board.

  • Box and Well Clearances: Allow 1.5–2.5 mm (0.059–0.098 in) across width and height, and 1.5–3 mm (0.059–0.118 in) for total stack height (lower tray + stacked player boards + rulebook).
  • Tray Material: Folded cardstock, corrugated E-flute, or molded pulp/plastic partitions must sit flush at the top rim so the player boards cannot tilt into the cube wells.
  • Unit and Carton Mass: Keep individual boxed set weights balanced for shipping—typically 0.4–1.2 kg (0.9–2.6 lb) depending on board count and cube volume—and cap master carton pack-out weights at 15–20 kg (33.1–44.1 lb) to prevent corner crushing in transit.

Rulebooks and Paper Extras

  • Format: Use 4, 6, or 8 panels for folded leaflets. Bound booklets use signatures in multiples of four: saddle stitch for 12–40 pages, perfect binding for 28+ pages, and sewn binding for 80–100+ pages.
  • Paper Weights: Interior pages use 80–120 gsm (0.08–0.13 mm / 0.003–0.005 in per sheet); covers use 200–300 gsm. When converting US paper weights, distinguish US Text LB (based on a 25 x 38 in / 635 x 965 mm sheet) from US Cover LB (based on a 20 x 26 in / 508 x 660 mm sheet)—for example, 80 lb Cover stock is substantially heavier and stiffer than 80 lb Text stock.

Prepress and Print Specifications

  • Files and Color: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts. Use CMYK at >= 300 DPI with separate spot layers for dielines, foil, or spot UV.
  • Black Ink: Use 100% K for fine text. Use rich black (C40–60 M30–40 Y30–40 K100) for large solid areas, keeping Total Area Coverage (TAC) at <= 280%–300%.
  • Bleed and Safety: 3 mm (0.118 in) bleed per side. Maintain >= 3 mm (0.118 in) safety margin from trim or die-cut edges, and >= 4–5 mm (0.157–0.197 in) for bordered card backs.

Production Steps and Sign-Off Criteria

  1. Structural Dieline and Tray Engineering: Lock card deck stack height (including +0.03–0.05 mm / 0.001–0.002 in per card for film), cube volume, and player-board outer dimensions. Verify that the lower insert rim supports all four edges of the bottom player board.
  2. Prepress Preflight: Check PDF/X-1a or PDF/X-4 output, spot-layer separation for the top-layer pocket die, 3 mm (0.118 in) bleed into every recessed pocket edge, and TAC <= 280%–300%.
  3. White Dummy and Wet Proof Sign-Off:
    • Place the full wooden-cube count and card deck into the lower tray and stack the unprinted dual-layer boards on top. Confirm the rigid box lid closes with 1.5–3 mm (0.059–0.118 in) stack clearance and no bulging.
    • Shake-check the closed dummy to confirm wooden cubes remain inside their lower wells beneath the flat board stack.
    • Approve color accuracy and anti-scuff matte finish on wet proofs before bulk offset printing.
  4. Board Mounting and Pressing: Laminate the printed wrap onto the die-cut top layer, mount onto the solid base greyboard, and press under controlled weight and curing time to prevent moisture warping.
  5. Pack-Out: Collate decks, wooden cubes, player boards, and rulebooks into the rigid box and pack into master cartons within the 15–20 kg (33.1–44.1 lb) handling limit.

Concrete Failure Modes

  • Player-Board Warping (Cupping): Caused by unbalanced moisture between the wrapped top face and the unprinted or differently coated back face, or insufficient pressing time after mounting. Counter-mount matching paper weight on the back of the base greyboard to balance tension.
  • Pocket-Bridge Tearing or Delamination: Occurs when die-cut recesses sit closer than 3–4 mm (0.118–0.157 in) to one another or to the outer edge, leaving too little greyboard fiber to hold the wrap.
  • Lid Lift or Crushed Card Corners: Happens when stack-height calculations omit the 0.03–0.05 mm (0.001–0.002 in) per-card film thickness, neglect sleeve allowance, or skip the 1.5–3 mm (0.059–0.118 in) vertical box clearance.
  • Wooden-Cube Migration in Transit: Happens when the lower tray partition walls stop below the player-board resting plane, leaving a gap that allows small cubes to slide into adjacent card wells during shipping.
  • Art Scuffing on Stacked Boards: Dark solid wraps rub against the underside of the board above them during transit unless protected with anti-scuff matte lamination.

Regulatory and Compliance Documentation

Compliance requirements depend on the target sales region, age grading, and physical components (such as small wooden cubes). Keep source records for all applicable assessments and registrations:

  • EU Toy Safety (EN 71): Where small wooden cubes, tokens, or target age grading bring the set within EU toy-safety scope, coordinate third-party EN 71 assessment and testing against the physical production materials and retain the resulting test reports. Reference: European Commission Toy Safety.
  • Germany Packaging Act (VerpackG): Placing packaged games on the German market requires producer registration and packaging volume data reporting through the LUCID system. Reference: Zentrale Stelle Verpackungsregister.