While standard offset card decks start at 200 decks (usual tiers of 200, 300, 500, and 1,000+), integrated boxed games follow project- and component-specific tooling minimums for rigid box wraps, multi-panel screen mounting, custom punchboard dies, and bookbinding signatures. For broader component families and standalone formats, see tabletop game printing.
Finished-Product Bill of Materials (BOM) and Specifications
Every component in a GM-screen boxed set interacts with the inner tray and lid clearance. Paper weights are specified in gsm alongside US basis weights—distinguishing US Text LB (based on a 25 × 38 in / 635 × 965 mm sheet) from US Cover LB (based on a 20 × 26 in / 508 × 660 mm sheet).
| Component | Default Material & Weight | Thickness / Caliper & Tolerance | Structural & Finishing Notes |
|---|---|---|---|
| Outer Rigid Box (Lid & Base) | 2–3 mm greyboard wrapped in 128–157 gsm art paper (approx. 86–106 lb US Text) | 2–3 mm (0.079–0.118 in) board; 15–20 mm (0.591–0.787 in) wrap margin | Anti-scuff matte lamination recommended for dark artwork; 1.5–2.5 mm (0.059–0.098 in) XY clearance |
| Internal Insert / Partition | Moulded pulp, EVA foam, or folded greyboard/cardboard divider | Sized to cavity load | Isolates hard dice from paper edges and supports the folded screen above lower compartments |
| Folding GM Screen | 2–3 mm greyboard core wrapped in printed art stock | 2–3 mm (0.079–0.118 in) board; 15–20 mm (0.591–0.787 in) wrap margin | Typically 3 or 4 panels; hinge gaps calibrated to board caliper so panels fold flat without wrap cracking |
| Bound Rulebook(s) | Interior: 80–120 gsm (approx. 54–81 lb US Text); Cover: 200–300 gsm (approx. 74–111 lb US Cover) | Interior: 0.08–0.13 mm (0.003–0.005 in) per sheet | Signatures in multiples of 4: saddle stitch (12–40 pp), perfect binding (28+ pp), or sewn binding (80–100+ pp) |
| Folded Map Sheets | 120–170 gsm matte-coated or uncoated stock (approx. 81–115 lb US Text) | ~0.11–0.18 mm (0.004–0.007 in) per sheet | 4-, 6-, or 8-panel accordion/leaflet folds or cross-folds sized inside the folded screen footprint |
| Reference Cards | 300–400 gsm paper core or PVC (see stock table below) | 0.28–0.44 mm (0.011–0.017 in); +0.03–0.05 mm (0.001–0.002 in) for double-sided film | Custom trim matched to box tray well; R3–R3.5 mm (0.118–0.138 in) rounded corners |
| Punchboard Standees & Tokens | 1.5–2.5 mm greyboard with printed art wrap | 1.5–2.5 mm (0.059–0.098 in) core; 3–4 mm (0.118–0.157 in) die gap | Standee bases (partner-sourced plastic or slotted punchboard) matched to laminated board caliper |
| Dice (Partner-Sourced) | Acrylic, resin, or urea-formaldehyde polyhedral sets | Varies by die set | Sourced via specialist partners; packed in sealed polybags or recessed tray wells |
Box Sizing Formulas
Calculate interior box dimensions from the largest rigid item (normally the folded GM screen) and the total compressed stack height of all layered components:
Box Inner Width = Max Component Width + 1.5 to 2.5 mm (0.059 to 0.098 in)Box Inner Length = Max Component Length + 1.5 to 2.5 mm (0.059 to 0.098 in)Box Inner Depth = Sum of Component Stack Heights + 1.5 to 3.0 mm (0.059 to 0.118 in)
Reference Card Stock Selection
Select card stock based on shuffling frequency and whether cards sit in a tight tray well or plastic sleeve. Trim dimensions are set by the box layout and sleeve clearance rather than a fixed default.
- 300 gsm art / blue core: 0.28–0.31 mm (0.011–0.012 in) — suited for light reference decks.
- 310 gsm black-core linen: 0.30–0.32 mm (0.012–0.013 in) — textured surface for frequent handling and reduced glare.
- 330 gsm black core: 0.32–0.34 mm (0.013 in) — higher snap and opacity for double-sided reference cards.
- 350 gsm art stock: 0.34–0.38 mm (0.013–0.015 in) — rigid feel for non-shuffled table trackers.
- 400 gsm art stock: 0.40–0.44 mm (0.016–0.017 in) — heavy reference plaques or initiative markers.
- PVC: 0.30 mm (0.012 in) — waterproof and wipeable for dry-erase tracking.
- Double-sided film lamination: Adds 0.03–0.05 mm (0.001–0.002 in) per card to stack height.
Prepress and Artwork Preparation
Card Deck Press coordinates prepress across specialist offset and tabletop manufacturing partners. All print-ready files must meet the following parameters before plating:
- File Formats & Fonts: Supply Adobe Illustrator (AI), PDF, or Photoshop (PSD) exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Color & Ink Density: Build artwork in CMYK at ≥300 DPI with separate spot layers for metallic foil, spot UV, and die/crease/fold lines. Use 100% K for fine body text, rich black (C40–60 M30–40 Y30–40 K100) for large dark solids, and keep total area coverage (TAC) at ≤280%–300%.
- Bleed & Safety Margins: Include 3 mm (0.118 in) bleed per side on all printed components. Keep critical text and icons ≥3 mm (0.118 in) inside the trim line, increasing to ≥4–5 mm (0.157–0.197 in) on bordered card backs.
- Finishing Compatibility: Specify anti-scuff matte lamination on dark GM screens and box lids to prevent transit rub. If gilded edges are specified on reference cards, avoid thick film lamination that interferes with edge-gilding adhesion.
Job-Specific Production Steps and Sign-Off Criteria
- Dieline & Structural Engineering: Lock the folded GM screen footprint, hinge gutter widths, punchboard 3–4 mm (0.118–0.157 in) die gaps, and rigid box clearances (1.5–2.5 mm / 0.059–0.098 in XY; 1.5–3 mm / 0.059–0.118 in Z).
- White Dummy & Proof Sign-Off: Assemble an unprinted structural dummy using exact production paper calipers, greyboard thicknesses, and partner-sourced dice/bases. Confirm that the lid closes flush without bowing and that standee slots grip the laminated punchboard cleanly. Approve wet or calibrated digital proofs for color and TAC.
- Offset Printing & Lamination: Print box wraps, screen sheets, rulebook signatures, maps, punchboard sheets, and reference cards. Apply anti-scuff matte or specified coatings and allow ink curing before mounting or cutting.
- Board Mounting, Binding & Die-Cutting: Wrap rigid boxes and GM screens with 15–20 mm (0.591–0.787 in) turn-ins. Bind rulebooks in 4-page signatures (saddle stitch, perfect, or sewn binding per page count). Die-cut punchboards and round card corners to R3–R3.5 mm (0.118–0.138 in).
- Kitting & Master Carton Pack-Out: Seat the insert, dice, cards, punchboards, maps, rulebook, and GM screen in sequence. Pack master cartons within safe handling limits (typically keeping gross carton weight under 15–20 kg / 33.1–44.1 lb) with corner protectors to prevent edge crush.
Sign-Off Criteria
- GM Screen: Panels open and stand upright on a flat table without warping, and hinges fold 180° without wrap splitting or delamination.
- Rulebook & Maps: Sewn or perfect-bound spines hold without cracking during flat-table reference; map folds lie flat without tearing at cross-creases.
- Punchboards & Standees: Tokens pop cleanly without tearing face paper; standees seat firmly in their bases without crushing the board edge.
- Box Fit: Lid telescopes smoothly onto the base with controlled air-release friction and zero side-wall bulge.
Regulatory and Packaging Compliance Records
Depending on destination market and age grading, maintain applicable compliance documentation alongside production records:
- EU Toy Safety (EN 71): Where the boxed game is intended for children or falls within toy safety scope, coordinate applicable assessment and testing under the EU Toy Safety Directive (EN 71) and retain test reports and technical files.
- Germany Packaging Act (VerpackG): For products placed on the German market, register and report packaging material weights (in kg / lb) through Verpackungsregister (VerpackG).
- France Triman Marking: For consumer-facing packaging sold in France, apply the required sorting signage and maintain documentation per Info-tri (Triman).
Concrete Failure Modes and Remedies
- Box lid fails to seat or sides bulge: Caused by calculating depth from nominal gsm instead of actual caliper (omitting +0.03–0.05 mm / 0.001–0.002 in per laminated card or rulebook signature swell). Remedy: Verify stack height with a physical white dummy built from actual production stocks and enforce 1.5–3 mm (0.059–0.118 in) Z-axis clearance.
- GM screen hinge cracks or springs open: Caused by hinge gutters too narrow for 2–3 mm (0.079–0.118 in) greyboard or brittle film over the fold. Remedy: Size hinge gutters to accommodate double board thickness plus wrap, and use flexible anti-scuff matte lamination or cloth hinge reinforcement.
- Punchboard standees tear or wobble in bases: Caused by die gaps narrower than 3 mm (0.118 in) or standee slots cut before measuring final laminated board caliper. Remedy: Maintain 3–4 mm (0.118–0.157 in) die spacing and calibrate standee base slots to the finished laminated punchboard thickness.
- Dice dent rulebook covers or map edges in transit: Caused by unpartitioned dice shifting against paper edges inside the box. Remedy: Seat dice inside a dedicated recessed insert compartment or sealed polybag separated from paper stacks.
- Scuffing and ink rub on dark box lids and screens: Caused by TAC exceeding 300% or unlaminated dark solids rubbing during assembly and shipping. Remedy: Cap TAC at ≤280%–300%, use rich black C40–60 M30–40 Y30–40 K100, and apply anti-scuff matte lamination.
Parent guide Custom Tabletop Game Printing