This baseline changes under four production conditions:
- Heavy-shuffle or wet-table use: Switching from protective varnish to double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card, and 0.30 mm (0.012 in) PVC replaces paperboard when waterproof durability is required.
- Dark full-bleed artwork: Anti-scuff matte coating replaces standard gloss or satin varnish to prevent surface marking during high-speed hopper collation.
- Gilded edges: Thick film lamination conflicts with metallic edge gilding; keep to protective varnish or thin coating when edge treatments are specified.
- Other deck formats: When a game uses non-standard card dimensions outside the standard 63 x 88 mm (2.48 x 3.46 in) format, sheet imposition, corner-rounding dies, and flow-wrap forming collars must be matched to the project's exact trim and stack height rather than forcing a standard wrapper geometry. For full-deck formats and boxed sets without randomized collation, see Trading Cards.
Finished Bill of Materials and Default Specifications
Card Deck Press produces booster packs through specialist offset and tabletop manufacturing partners. Standard offset card printing starts at 200 decks (usual tiers 200 / 300 / 500 / 1,000+), while multi-hopper collation and custom foil flow-wrap tooling follow project and component minimums.
When comparing paper weights, distinguish US Cover LB (measured on a 20 x 26 in / 508 x 660 mm basis sheet) from US Text LB (measured on a 25 x 38 in / 635 x 965 mm basis sheet). At 330 gsm (0.330 kg/m^2 or 0.068 lb/ft^2), the standard card stock equates to roughly 122 lb Cover (20 x 26 in) or 223 lb Text (25 x 38 in).
| Component | Default Specification | Alternative / Conditional Options |
|---|---|---|
| Card Stock & Core | 330 gsm black-core smooth stock; caliper 0.32–0.34 mm (0.013 in) | 300 gsm art/blue core at 0.28–0.31 mm (0.011–0.012 in); 310 gsm black-core linen at 0.30–0.32 mm (0.012–0.013 in); 350 gsm art stock at 0.34–0.38 mm (0.013–0.015 in); 400 gsm art stock at 0.40–0.44 mm (0.016–0.017 in); 0.30 mm (0.012 in) PVC |
| Card Trim & Corners | 63 x 88 mm (2.48 x 3.46 in); R3–R3.5 mm (0.118–0.138 in) corners | Project-specific trim and tooling for non-standard formats |
| Surface Finish | Protective varnish (matte, satin, or gloss) | Anti-scuff matte for dark artwork; double-sided film lamination (+0.03–0.05 mm / 0.001–0.002 in per card); foil stamping or spot UV on chase slots |
| Collation Slot Structure | Multi-hopper fixed slot order (e.g., commons, uncommons, rare/chase, token or insert) | Variable rarity ratios across separate offset press forms; foil/holo slots isolated on dedicated sheets with opaque white underbase |
| Primary Wrapper | Opaque metallized foil flow-wrap with longitudinal fin-seal and crimped ends | Cold-seal or heat-seal laminate; hang-hole punch on top fin for pegboard retail |
| Optional Display Box & Leaflets | Rigid or folding carton display box; optional 4/6/8-panel leaflet on 80–120 gsm (54–81 lb Text, 25 x 38 in; 0.08–0.13 mm / 0.003–0.005 in per sheet) | Rigid display box using 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) greyboard with 15–20 mm (0.591–0.787 in) wrap margin; clearance 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack height |
Prepress and File Requirements
- File formats: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded.
- Color & ink limits: CMYK with separate spot layers for foil, spot UV, or white underbase; >=300 DPI resolution; 100% K for fine text; rich black C40–60 M30–40 Y30–40 K100; total area coverage (TAC) <=280%–300%.
- Bleed & safety: 3 mm (0.118 in) bleed per side; >=3 mm (0.118 in) safety margin inside the trim line, increasing to >=4–5 mm (0.157–0.197 in) for bordered card backs.
Collation Slot Structure and Production Steps
- Press-form separation and imposition: Card artwork is grouped by rarity tier and surface treatment onto separate offset press forms so common, uncommon, and rare/foil sheets run in proportional quantities without wasting chase-card stock.
- Offset printing and coating: Sheets are printed in CMYK plus any spot layers, then sealed with protective varnish or laminated. Printed wrapper film is gravure- or flexo-printed in parallel on opaque metallized roll stock.
- Slitting, corner rounding, and conditioning: Sheets are slit into strips, die-cut or guillotined to 63 x 88 mm (2.48 x 3.46 in) with R3–R3.5 mm (0.118–0.138 in) corners, and conditioned so sheet curl stays flat before entering collation hoppers.
- Multi-hopper collation: Each rarity slot is loaded into its assigned feeder hopper. Cards drop sequentially onto a lugged conveyor in fixed slot order (for example, common slots first, followed by uncommon, rare/chase, and any token or 4/6/8-panel leaflet).
- Flow-wrap sealing and secondary packing: The collated stack enters the forming collar of the horizontal flow-wrapper, which wraps the opaque foil film around the stack, forms the back fin-seal, and crimps and cuts the ends. Finished packs are weighed, batch-coded, and packed into display boxes and master cartons (typically capped at <=15–20 kg / 33.1–44.1 lb per carton for transit handling).
Sign-Off Criteria
Before approving full production and shipment, verify these physical checkpoints against the approved proof:
- Opacity and light-blocking: Hold an assembled card stack and a sealed foil wrapper against a direct light source; zero card-face show-through is visible through the black-core stock or the foil wrapper.
- Border centering: Measure bordered card backs across sample sheets; trim variance must remain within the >=4–5 mm (0.157–0.197 in) safety zone so borders appear even on all four sides.
- Stack caliper and pack mass: Verify total stack thickness (
card count x 0.32–0.34 mm, e.g., 15 cards = 4.80–5.10 mm / 0.189–0.201 in) and finished pack weight (approx. 0.030 kg / 0.066 lb for a 15-card wrapped pack) against inline checkweigher tolerances to catch missing or double-fed cards. - Seal integrity: Pull-test the longitudinal fin-seal and end-crimps on sample packs; seals must hold without pinholes, burn-through, or crushed card corners inside the crimp zone.
- Surface scuff and ink adhesion: Rub dark full-bleed cards face-to-back under firm finger pressure; anti-scuff matte or varnish must show no chalking or ink transfer.
Regulatory and Packaging Compliance Records
Depending on the target sales region and age grading, maintain the following procedural records and registrations before market placement:
- EU Toy Safety (EN 71): When booster packs are marketed to or intended for children under 14 in the EU, complete applicable EN 71 assessment and third-party laboratory testing on card inks, coatings, and foil wrappers, and retain the technical file and Declaration of Conformity per European Commission Toy Safety.
- Germany Packaging Act (VerpackG): Foil flow-wrap, paperboard display boxes, and shipping cartons placed on the German market require producer registration and packaging volume reporting in the LUCID register per Zentrale Stelle Verpackungsregister.
- France Sorting Info (Triman): Consumer-facing foil wrappers and paperboard display cartons sold in France require the Triman logo and material-specific sorting instructions per French Ministry of Ecological Transition (Info-tri / Triman).
Concrete Failure Modes
- Light-sorting ("pack searching"): Using standard 300 gsm or 350 gsm art board without a black core—or using thin single-layer poly wrap instead of opaque metallized foil—allows bright light or edge-flexing to reveal rare or foil card positions inside sealed packs.
- Visible border skew: Designing bordered card backs with less than 4–5 mm (0.157–0.197 in) safety margin exposes normal guillotine or die-cut drift, making cards look off-center.
- Scuffing on dark backgrounds: Running dark rich-black artwork with standard gloss or satin varnish instead of anti-scuff matte causes visible rub lines when cards slide across metal collation hoppers.
- Crushed corners or weak end-crimps: Running a flow-wrap forming collar sized for a thinner or thicker card count leaves either too little film slack (crushing R3–R3.5 mm / 0.118–0.138 in corners in the crimp jaws) or excess air pockets that burst under transit compression.
- Hopper double-feeds and static jams: Unconditioned sheets with residual static or curl after lamination cause two cards to stick together in a single rarity hopper, throwing off pack counts and checkweigher rejection rates.
- Gilded-edge delamination: Applying metallic edge gilding over thick double-sided film lamination causes the film edge to lift or peel during normal pack opening and handling.