This configuration is the default choice when collectors or retail buyers expect every base card in checklist order upon opening, rather than randomized booster distribution. Conditions that change this build include total set mass—once a collated set exceeds roughly 1.0–1.5 kg (2.2–3.3 lb), single-ply folding cartons deform and require rigid greyboard or corrugated-liner walls—and the inclusion of bonus promo packs, checklist booklets, or gilded card edges, which alter internal clearances and lamination selection. Standard offset card production starts at 200 decks (usual tiers 200, 300, 500, and 1,000+), while boxed sets and custom tooling follow project and component minimums. For broader card stock and print options across single-deck formats, see trading cards.
Finished Bill of Materials (BOM)
A complete factory set box combines collated card bricks, protective dividers, a high-weight outer container, and optional printed inserts. Paper weights are specified in gsm alongside US basis weights, where US Text LB uses a 25 × 38 in (635 × 965 mm) basis sheet and US Cover LB uses a 20 × 26 in (508 × 660 mm) basis sheet.
| Component | Material & Weight Specification | Thickness / Dimensions | Role in Complete Set |
|---|---|---|---|
| Collated card bricks | 300 gsm art/blue core; 310 gsm black-core linen; 330 gsm black core; 350 gsm art stock; 400 gsm art stock; or 0.30 mm (0.012 in) PVC (typically ~110–148 lb US Cover LB depending on grade) | 0.28–0.44 mm (0.011–0.017 in) per card; +0.03–0.05 mm (0.001–0.002 in) with double-sided film; R3–R3.5 mm (0.118–0.138 in) corners | Holds the full checklist in fixed numerical or subset order |
| Brick overwrap | Clear heat-sealed cellophane (BOPP/cellophane film) | Tight wrap per brick (typically 50–150 cards per brick) | Locks card sequence and prevents shingling during transit without foil boosters |
| Chipboard dividers | Uncoated or printed grey/kraft chipboard | Matched to card face dimensions; 1.5–2.0 mm (0.059–0.079 in) for structural partitions or heavy card dividers | Separates bricks, absorbs lid compression, and prevents brick-to-brick edge denting |
| Outer high-weight box | Rigid greyboard wrapped in printed art paper, or corrugated-liner (E-flute/B-flute) box | Greyboard: 1.5 / 2.0 / 2.5 / 3.0 mm (0.059 / 0.079 / 0.098 / 0.118 in); wrap margin: 15–20 mm (0.591–0.787 in) | Supports 1.0–3.5+ kg (2.2–7.7+ lb) stack loads without wall bowing or corner crush |
| Optional checklist / booklet | Interior: 80–120 gsm (~54–80 lb US Text LB); Cover: 200–300 gsm (~74–111 lb US Cover LB) | Interior: 0.08–0.13 mm (0.003–0.005 in) per sheet; 4/6/8-panel leaflet, 12–40p saddle stitch, 28+p perfect, 80–100+p sewn | Provides set checklist, numbering index, or collector guide |
Card, Box, and Clearance Specifications
Card trim dimensions vary by trading card format and are set per project rather than forced to a single default. Once the card trim is locked, prepress, caliper, and box clearances follow fixed mechanical tolerances:
- Prepress and Color: Supply print-ready AI, PDF, or PSD files exported to PDF/X-1a or PDF/X-4 with outlined or embedded fonts and ≥300 DPI raster artwork. Use CMYK with separate spot layers for foil or Spot UV. Set fine text to 100% K, rich black to C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) ≤280%–300%.
- Bleed and Safety: Include 3 mm (0.118 in) bleed per side. Keep text and critical graphics inside a ≥3 mm (0.118 in) safety margin, increasing to ≥4–5 mm (0.157–0.197 in) on bordered card backs so minor guillotine or die-cut drift does not create uneven borders.
- Stock Caliper and Finish: Approximate unlaminated card calipers are 0.28–0.31 mm (0.011–0.012 in) for 300 gsm art/blue core, 0.30–0.32 mm (0.012–0.013 in) for 310 gsm black-core linen, 0.32–0.34 mm (0.013–0.013 in) for 330 gsm black core, 0.34–0.38 mm (0.013–0.015 in) for 350 gsm art stock, 0.40–0.44 mm (0.016–0.017 in) for 400 gsm, and 0.30 mm (0.012 in) for PVC. Double-sided lamination adds 0.03–0.05 mm (0.001–0.002 in) per card. Anti-scuff matte lamination suits dark artwork; avoid thick lamination if the set uses gilded edges, as thick film conflicts with edge gilding adhesion.
- Box Wall and Clearance Formulas: Rigid greyboard boxes use 1.5 mm (0.059 in) or 2.0 mm (0.079 in) board for lighter sets, stepping up to 2.5 mm (0.098 in) or 3.0 mm (0.118 in) greyboard—or a corrugated-liner outer box—when brick weight exceeds roughly 1.5 kg (3.3 lb). Calculate internal box dimensions in plain text as:
Brick height (mm) = Cards per brick * (Card caliper + Film caliper)Internal box width or length (mm) = Card trim + 1.5 to 2.5 mm (0.059 to 0.098 in)Internal box stack height (mm) = Sum of brick heights + Sum of divider thicknesses + Optional leaflet thickness + 1.5 to 3.0 mm (0.059 to 0.118 in)
Sequential Brick Wrapping & Production Steps
- Sequential Imposition and Press Check: Impose cards across press sheets in a deterministic grid so cutting and gathering preserve exact checklist order (e.g., #001 through the final card) without manual hand-sorting.
- Cutting, Cornering, and Brick Splitting: Guillotine-cut sheets into strips and individual cards, round corners to R3–R3.5 mm (0.118–0.138 in), and split the collated stream into uniform bricks (commonly 50–150 cards per brick) so each brick stays rigid enough for automated or semi-automated wrapping.
- Tight Cellophane Brick Wrapping: Overwrap each brick in clear cellophane with calibrated heat-seal tension. The film must hold the brick square so cards cannot slide or fan, while remaining loose enough at the corners to prevent bowing.
- Chipboard Divider Placement: Place rigid chipboard dividers between adjacent cellophane bricks, at the outer ends of the stack if the box has corrugated flutes, and at subset boundaries (such as separating base sets from parallel or chase cards). Dividers must match the card face footprint within the box clearance so they sit flush rather than tilting.
- High-Weight Box Fabrication and Loading: Wrap 1.5–3.0 mm (0.059–0.118 in) greyboard with a 15–20 mm (0.591–0.787 in) turn-in wrap margin (or die-cut and glue the corrugated-liner outer box), insert bricks and dividers in sequence, add any folded leaflet or bound booklet on top, and apply the outer tamper-evident shrink wrap.
Sign-Off Criteria
- Sequence Audit: Pull sample bricks from the start, middle, and end of the run to verify unbroken numerical order and zero missing or duplicated cards across brick splits.
- Brick Tension & Squareness: Bricks show zero bowed corners or pinched edges under cellophane wrap and do not shingle when shaken lightly.
- Fit & Clearance: Bricks and chipboard dividers drop into the outer box cleanly with 1.5–2.5 mm (0.059–0.098 in) lateral clearance and 1.5–3.0 mm (0.059–0.118 in) vertical clearance, leaving no rattle space that allows internal impact.
- Print & Edge Quality: Bordered backs show balanced margins, dark solids pass rub inspection without scuffing, and box wrap corners have clean 15–20 mm (0.591–0.787 in) turn-ins with no exposed greyboard.
Regulatory & Packaging Compliance Records
Applicable assessment and packaging registration steps depend on the target age group and destination market:
- Toy Safety (EU): If the complete set is marketed for play by children under 14, plan for EN 71 mechanical, flammability, and chemical migration assessment and testing, maintaining technical documentation per the European Commission Toy Safety overview.
- Packaging Registration (Germany): When placing packaged sets onto the German market, register packaging weights (outer box, chipboard dividers, cellophane wrap) and maintain data-reporting records under the Zentrale Stelle Verpackungsregister (VerpackG) guidance.
- Sorting & Recycling Marks (France): For sets distributed in France, apply the required Triman logo and Info-Tri sorting instructions for paperboard and plastic film components according to the French Ministry of Ecological Transition Info-Tri rules.
Concrete Failure Modes
- Brick-Split Sequence Errors: Cutting or gathering errors at the press-sheet boundary cause the last card of brick one and the first card of brick two to swap or drop, breaking the full-set guarantee.
- Over-Tensioned Cellophane: Excessive heat-shrink or film tension curves the top and bottom cards of a brick inward, leaving permanent bow that prevents cards from lying flat in binder sleeves.
- Missing or Undersized Chipboard Dividers: Without full-footprint chipboard partitions between bricks, heavy bricks (0.5–1.0 kg / 1.1–2.2 lb each) shift against one another during parcel shipping and dent card edges through the cellophane.
- Under-Spec Outer Box Walls: Using thin folding carton or 1.5 mm (0.059 in) greyboard for a 2.0–3.5 kg (4.4–7.7 lb) set causes sidewall bulging, lid pop-off, and crushed box corners when cartons are stacked.
- Excessive Internal Clearance: Exceeding 2.5 mm (0.098 in) lateral clearance or 3.0 mm (0.118 in) stack-height clearance turns the heavy card bricks into a battering ram inside the box during drop impacts.
- Narrow Bordered-Back Safety: Using less than 4–5 mm (0.157–0.197 in) safety on bordered card backs makes minor cutting variance immediately visible when inspecting a uniform brick edge.