Material and Prepress Specifications

Boxed game components and custom steel-rule tooling follow project and component minimums. Keep top-sheet artwork, ink density, and board geometry within these tolerances before mounting and cutting:

  • Greyboard Thickness: 1.5 mm (0.059 in), 2.0 mm (0.079 in), 2.5 mm (0.098 in), or 3.0 mm (0.118 in).
  • Board and Die Clearances: 15–20 mm (0.591–0.787 in) wrap margin on wrapped boards; 3–4 mm (0.118–0.157 in) die gap between adjacent punchboard tokens.
  • Artwork Bleed and Safety: 3 mm (0.118 in) bleed per side and at least 3 mm (0.118 in) safety margin inside trim lines.
  • File Format and Resolution: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 at ≥300 DPI, with outlined or embedded fonts.
  • Color and Ink Limits: CMYK with separate spot layers, 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and Total Area Coverage (TAC) ≤280%–300%. Keeping TAC at or below 300% preserves film-to-paper bond strength at cut edges.

Production Steps

  1. Print and Cure Top Sheets: Print the CMYK top sheet within the 280%–300% TAC limit and allow full drying before lamination so residual solvents or wet ink do not weaken film adhesion.
  2. Apply Low-Elongation Matte BOPP: Laminate the printed sheet with low-elongation BOPP matte film (anti-scuff matte for dark solids). Low-elongation film snaps cleanly when struck by a steel rule instead of stretching into the kerf.
  3. Mount to Greyboard: Laminate the coated top sheet (and backing sheet, where double-sided) onto 1.5–3.0 mm (0.059–0.118 in) greyboard and cure flat under pressure to prevent edge curl before die-cutting.
  4. Die-Cut with Sharp Steel-Rule Knives: Cut punchboards with 3–4 mm (0.118–0.157 in) spacing between tokens so the board supports rule pressure evenly. For jigsaw puzzles, use freshly sharpened steel-rule dies matched to the board caliper so tight interlocking curves shear cleanly in a single stroke.

Sign-Off Criteria

  • Clean Perimeter Shear: Every token and puzzle piece separates cleanly with no stretched plastic threads or film bridging across die nicks.
  • Flat Corner and Knob Adhesion: Film remains bonded flush to the paper fiber at sharp token corners and narrow puzzle knob necks after punching and handling.
  • Intact Board Faces: Top sheets show no fiber tearing, crushed edges, or scuffing across dark solids after waste stripping.
  • Compliance Documentation: Where finished punchboards or puzzles fall under toy safety rules, maintain material and coating records for EN 71 assessment and testing as required for the target market.

Failure Modes

Failure Mode Physical Cause Correction
Film stringing (whiskering) High-elongation film or dull steel-rule knives stretch the BOPP layer rather than shearing it, leaving plastic strands across nicks and puzzle cuts. Switch to low-elongation BOPP film and replace or resharpen worn steel-rule knives.
Lifted token corners TAC above 300%, uncured ink, or excessive knife compression breaks the adhesive bond at acute token angles. Cap ink density at ≤280%–300% TAC, cure sheets fully before laminating, and verify knife-to-board pressure.
Torn puzzle knobs Dull blades or tight interlock geometries drag the laminated face sheet into the greyboard kerf, ripping paper fibers at the narrow neck. Use sharp, properly beveled steel-rule dies matched to the 1.5–3.0 mm (0.059–0.118 in) board caliper.
Edge and surface scuffing Standard matte film abrades during stripping, tumbling, and packing on dark ink builds. Specify anti-scuff matte BOPP for dark artwork.