Conditions that change the choice:

  • Dark or high-coverage artwork: Use anti-scuff matte film (see Matte Lamination) when outer wraps use rich black (C40–60 M30–40 Y30–40 K100) or deep solid colors, because standard matte film shows shiny burnish marks along box edges during wrapping and packing.
  • Board thickness and lid span: Thinner 1.5 mm (0.059 in) greyboard bows more easily under single-sided film tension than 2.5–3.0 mm (0.098–0.118 in) board, making a matched inner liner mandatory on large or shallow lids.
  • Production minimums: Boxed games and rigid box tooling follow project and component minimums rather than the 200-deck starting tier for standard offset cards.

Specifications

Parameter Specification Notes
Greyboard caliper 1.5 / 2.0 / 2.5 / 3.0 mm (0.059 / 0.079 / 0.098 / 0.118 in) Select thicker board for larger lids to resist film pull
Wrap turn-in margin 15–20 mm (0.59–0.79 in) Folded over board edges onto the inner face
Box fit clearance 1.5–2.5 mm (0.059–0.098 in) width/height; 1.5–3.0 mm (0.059–0.118 in) stack height Absorbs wrap thickness and minor seasonal board movement
Bleed & safety 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety Keep type and borders clear of fold and trim lines
Prepress & ink limits CMYK + separate spot layers, ≥300 DPI, PDF/X-1a or PDF/X-4 (AI/PDF/PSD), outlined or embedded fonts, 100% K fine text, rich black C40–60 M30–40 Y30–40 K100, TAC ≤280%–300% Prevents ink set-off and film delamination along folds

When specifying outer wrap and inner liner papers, state weights in gsm and distinguish US Text LB (25 × 38 in basis sheet) from US Cover LB (20 × 26 in basis sheet) so exterior and interior sheet weights are compared on the same basis.

Wrap-Margin Adhesion and Corner-Miter Controls

Turn-in dimensions and corner-miter geometry follow Wrap Turn-In and Corner Allowances; adding matte film introduces three specific bonding constraints:

  • Film-grade adhesive on overlapped turn-ins: Standard board glue bonds the unlaminated paper back of the 15–20 mm (0.59–0.79 in) wrap margin to raw greyboard, but fails where a folded flap overlaps a matte-laminated edge or corner tab. Use film-grade wrap adhesive on all overlap zones to hold edges flat.
  • Clean corner miters to reduce film bulk: Matte film increases sheet stiffness at 90-degree folds. Accurate corner miters eliminate double-thickness film ridges that hold flaps away from the board during pressing.
  • Fold-line ink and cure control: Folding a laminated sheet over 1.5–3.0 mm (0.059–0.118 in) greyboard puts maximum shear stress on the outer spine and edge creases. Ink must cure completely before lamination, and total area coverage (TAC) must stay at or below 280%–300% to prevent edge whitening or film lifting.

Single-Sided Warp Control

Applying matte film to only the exterior face of the wrap sheet creates an asymmetric moisture barrier across the 1.5–3.0 mm (0.059–0.118 in) greyboard. As water-based wrap adhesive dries, moisture escapes faster from the unlaminated interior than through the film-sealed exterior, pulling the board into a bow.

  • Balanced inner lining: Line the inside of the greyboard with a matched inner paper sheet to equalize moisture loss and counter-balance the exterior film tension.
  • Controlled pressing and curing: Press wrapped lids and bases flat while the adhesive cures so the board sets in plane before lids are fitted onto bases within the 1.5–2.5 mm (0.059–0.098 in) width/height clearance.

Job-Specific Production Steps

  1. Prepress check: Verify CMYK + separate spot layers, ≥300 DPI, 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety from fold lines, TAC ≤280%–300%, and PDF/X-1a or PDF/X-4 output.
  2. Print and cure wrap sheets: Offset print the exterior wrap and allow full ink drying before lamination so residual solvents do not weaken film adhesion.
  3. Single-sided matte lamination: Apply matte film (anti-scuff matte for dark artwork) to the printed face only.
  4. Die-cut and miter: Cut the laminated wrap sheet with 15–20 mm (0.59–0.79 in) turn-in margins and clean corner miters.
  5. Wrap, line, and cure flat: Mount the wrap onto 1.5–3.0 mm (0.059–0.118 in) greyboard using film-grade wrap adhesive on overlapped turn-in edges, apply the balanced inner liner, and cure flat under pressure.

Sign-Off Criteria

  • All 15–20 mm (0.59–0.79 in) turn-in edges and mitered corners lie flush against the greyboard with no lifting or spring-back after curing.
  • Folded edges and spines show no film bubbling, edge whitening, or ink cracking.
  • Finished lids sit flat on a level surface without rocking and fit over bases cleanly within the 1.5–2.5 mm (0.059–0.098 in) width/height clearance.

Failure Modes

Failure Mode Physical Cause Corrective Action
Turn-in flaps lifting at corners Standard paper glue applied over matte-laminated overlap Use film-grade wrap adhesive on overlapped edges and verify miter geometry
Lid or tray bowing (warp) Single-sided film tension and uneven moisture loss on 1.5–3.0 mm (0.059–0.118 in) greyboard Add a balanced inner liner and cure components flat under pressure
Film bubbling or whitening along folds Insufficient ink cure before lamination or TAC above 280%–300% Cure printed sheets fully before laminating and cap TAC at 280%–300%
Glossy rub marks on dark lids Standard matte film abraded during wrapping or transit Specify anti-scuff matte film for dark and high-coverage artwork