For baseline film properties and card-stock comparisons, see the soft-touch lamination overview.
Surface Behavior: Token Friction, Glare, and Palm-Oil Staining
- Token friction: The micro-matte surface texture increases drag compared to gloss or standard aqueous coatings, helping tokens, dice, and standees stay in place when a board is bumped or sits over a slight fold bow.
- Glare reduction: Soft-touch diffuses overhead room lighting across wide board spreads and upright GM screen panels, keeping small
100% Kreference tables legible from oblique seating angles. - Palm-oil retention: The same micro-texture holds skin oils, lotions, and food residue. On folding boards where players rest wrists or slide pieces, and along the outer grip edges of GM screens, oils create persistent glossy patches—most visible on rich black (
C40–60 M30–40 Y30–40 K100) and deep-saturated panels. - Dark-artwork alternative: Anti-scuff matte suits dark artwork better than standard soft-touch because its harder topcoat resists burnishing and oily sheen under repeated sliding.
Board Construction and Lamination Specs
| Parameter | Specification | Impact on Folding Boards & GM Screens |
|---|---|---|
| Greyboard core | 1.5 / 2 / 2.5 / 3 mm (0.059 / 0.079 / 0.098 / 0.118 in) |
Thicker cores stay flatter across wide spans but increase hinge tension at 180-degree folds |
| Wrap margin | 15–20 mm (0.591–0.787 in) |
Turn-in allowance around board edges; film must bond cleanly into the inner liner overlap |
| Film thickness | 0.03–0.05 mm (0.0012–0.0020 in) double-sided |
Double-sided film reference; single-sided face lamination adds half that thickness to the outer wrap |
| Bleed & safety | 3 mm (0.118 in) bleed per side; >=3 mm (0.118 in) safety |
Keeps key grid lines, icons, and text clear of wrapped edges and hinge channels |
| Color & ink limit | CMYK + separate spot layers; TAC <=280%–300% |
Excessive ink saturation weakens film adhesion along folded wrap joints |
| Text & rich black | 100% K fine text; C40–60 M30–40 Y30–40 K100 rich black |
Prevents registration halos on screen tables and controls ink buildup under the film |
| File setup | AI / PDF / PSD exported as PDF/X-1a or PDF/X-4, >=300 DPI, outlined/embedded fonts |
Keeps spot-coating masks (such as spot UV over soft-touch) aligned to board panels |
Job-Specific Production Steps
- Prepress separation and ink control: Keep
TAC <=280%–300%across hinge paths and dark borders. Place fine rules and GM reference text in100% Kand keep critical artwork at least3 mm(0.118 in) clear of trim and fold channels. If combining soft-touch with spot UV highlights, supply the spot mask on a separate vector layer and keep it off the hinge line. - Print and full ink cure: Print the wrap sheet at
>=300 DPIand allow the ink to dry and cure completely before lamination. Uncured solvent or heavy rich-black ink outgasses under the film and causes bubbling at the fold. - Sheet lamination and grain-aligned wrapping: Apply soft-touch film to the printed wrap sheet, then mount onto
1.5–3 mm(0.059–0.118 in) greyboard with a15–20 mm(0.591–0.787 in) wrap margin. Align paper and board grain parallel to the primary 180-degree hinge so the wrap bends with the fibers rather than tearing across them. - Hinge pressing and 180-degree folding: Press the wrapped board channels and allow wrap adhesive to set before folding panels flat. Pre-flexing a warm or uncured joint stretches the soft-touch film and accelerates crease whitening.
Sign-Off Criteria
- Glare and tone check: Inspect the laminated wrap under angled overhead light. Verify that soft-touch muting does not muddy dark grid lines and that
100% Ktable text on GM screens remains crisp. - 180-degree hinge flex: Cycle the folding board and GM screen joints through full open and closed positions. Confirm the film shows no white stress line along the outer spine, no tenting in the hinge channel, and no edge lift at the
15–20 mm(0.591–0.787 in) inner wrap. - Surface-oil and scuff check: Rub a dark-inked panel lightly with a clean finger and a wooden token edge. Confirm the finish does not immediately burnish into a permanent shiny streak.
Failure Modes and Fixes
| Failure Mode | Physical Cause | Correction |
|---|---|---|
| Crease whitening along 180-degree hinges | Soft-touch film stretches over dark ink at a tight fold radius or cross-grain wrap | Align wrap grain parallel to the hinge, lower TAC along the spine, or avoid solid dark ink directly across the fold |
| Glossy palm-oil patches on dark panels | Micro-textured soft-touch traps skin oils on high-contact rich-black areas | Switch to anti-scuff matte lamination for dark artwork or heavy-handling surfaces |
| Film delamination at wrap turn-ins | High ink load (>300% TAC) or uncured ink under the 15–20 mm (0.591–0.787 in) turn-in |
Cap TAC <=280%–300%, cure sheets fully before laminating, and verify adhesive wet-out on the inner liner |
| Cracking on spot UV over soft-touch | Brittle spot varnish placed across a flexing GM screen or board joint | Keep spot UV plates inset from all hinge channels and crease lines |
Parent guide Soft-Touch (Velvet) Film Lamination