For general film behavior, ink interaction, and finish compatibility across board and card components, see the soft-touch lamination overview.
When to Choose Soft-Touch vs. Anti-Scuff Matte
- Choose soft-touch lamination when tactile velvet feel on the outer lid is the priority and the box structure accommodates looser width/height clearance without sacrificing shelf stability.
- Switch to anti-scuff matte when the wrap uses dark artwork or heavy rich black coverage, where skin oils, burnished rub lines, and assembly handling marks show readily on soft-touch film.
- Split lid and base finishes when two soft-touch surfaces bind during opening; keeping soft-touch on the outer lid and using an uncoated or smoother matte wrap on the inner base reduces sliding drag.
Rigid Box & Wrap Specifications
| Parameter | Specification | Notes for Soft-Touch Wraps |
|---|---|---|
| Greyboard caliper | 1.5 / 2.0 / 2.5 / 3.0 mm (0.059 / 0.079 / 0.098 / 0.118 in) | Thicker boards increase corner turn-in tension on laminated wraps |
| Wrap margin | 15–20 mm (0.591–0.787 in) | Folded over greyboard edges onto the inner box wall |
| Width/height clearance | 1.5–2.5 mm (0.059–0.098 in) | Tune toward the 2.5 mm (0.098 in) end to offset lid-to-base friction |
| Stack-height clearance | 1.5–3.0 mm (0.059–0.118 in) | Accounts for internal contents and lid seating depth |
| Wrap-sheet prepress | CMYK + separate spot layers, >=300 DPI, 3 mm (0.118 in) bleed per side | Supply PDF/X-1a or PDF/X-4 with outlined or embedded fonts |
| Ink & black limits | Rich black C40–60 M30–40 Y30–40 K100; 100% K fine text; TAC <=280%–300% | Prevents ink splitting and edge lift along 90-degree board folds |
Job-Specific Production Steps
- Prep wrap sheets within ink limits: Keep total area coverage at or below 280%–300% across folds and the 15–20 mm (0.591–0.787 in) wrap margin so the film-to-paper bond holds when turned around greyboard edges.
- Tune telescopic lid clearance: Set the lid-to-base gap toward the upper end of the 1.5–2.5 mm (0.059–0.098 in) width/height range whenever both lid and base wraps are soft-touch laminated.
- Enforce gloved assembly handling: Require clean, lint-free gloves at sheet-to-board laminating, corner-turning, and lid-fitting stations so skin oils do not transfer onto the velvety surface.
- Seat and cure wrap margins: Press the 15–20 mm (0.591–0.787 in) turn-ins firmly against the inner greyboard face and allow adhesive to set before nesting lids onto bases.
Sign-Off Criteria
- Lid drop and release: The telescopic lid slides onto the base smoothly under its own weight and lifts off without gripping, squeaking, or pulling the base upward.
- Surface uniformity: Wrapped panels show even matte velvet texture under raking light, with no glossy fingerprint smudges, oil mottling, or burnished corner rub marks.
- Wrap-margin adhesion: All 15–20 mm (0.591–0.787 in) turn-ins and mitered corners sit flush against the greyboard with no tenting, bubbling, or edge lift.
Failure Modes & Fixes
- Telescopic lid drag or binding: Soft-touch film against soft-touch film creates high surface friction, causing tight lids to stall halfway down or lock onto the base. Open lid-to-base clearance toward 2.5 mm (0.098 in), or keep soft-touch on the lid only and use a smoother wrap on the base.
- Oil mottling and handling marks: Bare-hand contact during corner pressing or lid fitting leaves dark, glossy patches that are most visible on rich black (C40–60 M30–40 Y30–40 K100) and dark-ink wraps. Enforce clean glove protocols at every assembly station or move dark-artwork wraps to anti-scuff matte.
- Wrap-margin lifting at board edges: Heavy ink build above TAC 280%–300% or stiff film tension pulls the 15–20 mm (0.591–0.787 in) turn-in away from the greyboard edge after folding. Keep TAC within 280%–300%, press turn-ins firmly during wrapping, and verify adhesive grab on the laminated stock before full assembly.
Parent guide Soft-Touch (Velvet) Film Lamination