In practice, the choice is between spraying higher-viscosity pigment in light passes or dyeing with lower-viscosity ink, and that decision shifts with artwork darkness, core absorbency, and film thickness. Dark face or back artwork, heavy ink coverage near the trim edge, and compressible velvet soft-touch film leave little margin for clamping marks or perimeter staining; for those jobs, an anti-scuff matte finish often pairs more predictably with edge finishing than a high-pile velvet soft-touch film. For the broader finish-pairing rules, see soft-touch lamination and edge finishing.
Specifications and Compatibility
Standard offset card runs start at 200 decks (usual tiers are 200, 300, 500, and 1,000+ decks). Regardless of deck format, edge coloring depends on the exposed paper core accepting pigment cleanly while the laminated faces remain sealed against overspray and pressure marks.
Card Stock, Film Caliper, and Prepress Specs
Card stocks are specified in grams per square meter (gsm) rather than US Text LB or Cover LB, which measure weight against different basis sheet sizes. Double-sided lamination adds 0.03–0.05 mm (0.0012–0.0020 in) per card; thicker film alters stack compressibility and can conflict with heavy edge treatments such as gilded edges.
| Stock / Component | Weight / Type | Approximate Caliper |
|---|---|---|
| Art / blue core | 300 gsm | 0.28–0.31 mm (0.011–0.012 in) |
| Black-core linen | 310 gsm | 0.30–0.32 mm (0.012–0.013 in) |
| Black core | 330 gsm | 0.32–0.34 mm (0.013 in) |
| Art stock | 350 gsm | 0.34–0.38 mm (0.013–0.015 in) |
| Heavy card stock | 400 gsm | 0.40–0.44 mm (0.016–0.017 in) |
| PVC | Synthetic | 0.30 mm (0.012 in) |
| Double-sided film | Soft-touch / matte | +0.03–0.05 mm (+0.0012–0.0020 in) per card |
Prepress files for edge-colored soft-touch decks require:
- File formats and resolution: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 at ≥300 DPI, with fonts outlined or embedded.
- Color and ink limits: CMYK artwork with separate spot layers for edge color specifications; 100% K for fine text; rich black at C40–60 M30–40 Y30–40 K100; total area coverage (TAC) ≤280%–300%.
- Bleed, safety, and corners: 3 mm (0.118 in) bleed per side, ≥3 mm (0.118 in) safety margin (≥4–5 mm / 0.157–0.197 in for bordered backs), and R3–R3.5 mm (0.118–0.138 in) rounded corners.
Regulatory Documentation
Where a deck falls within children's product or toy scope, surface films and edge-coloring inks are subject to EN 71 assessment and testing rather than assumed compliant from standard commercial print specs. Applicable procedures and official documentation requirements are outlined in the EU Toy Safety framework.
Job-Specific Production Steps
- Cure print and lamination before cutting: Allow offset inks and soft-touch film adhesive to bond fully before die-cutting and rounding R3–R3.5 mm (0.118–0.138 in) corners. Cutting uncured film pulls the laminate edge away from the paper core, creating channels for edge ink to wick into.
- Jog and clamp the deck stack: Align cards into a square, flush block and apply even clamping across the top and bottom sacrificial boards or full-face plates. Insufficient pressure leaves micro-gaps that admit overspray; concentrated bar pressure crushes the velvet pile.
- Control ink viscosity and pass weight: Tune pigment viscosity and spray or dye application rate to coat the exposed paper fibers without flooding the seam between film and paper. Build saturated colors in controlled passes rather than a single wet coat.
- Cure under controlled airflow before fanning: Hold the clamped stack until the edge pigment sets so wet color does not transfer onto adjacent soft-touch faces when cards are separated and collated.
Sign-Off Criteria
- Uniform edge coverage: Solid, even color across all four trimmed sides and around R3–R3.5 mm (0.118–0.138 in) corners without exposed white core streaks.
- Clean face-to-edge boundary: Sharp color termination at the laminate seam with zero overspray halo, face staining, or inward capillary bleed.
- Intact soft-touch surface: No lifted film edges, delamination at corners, or glossy clamp-bar indentations on the top and bottom cards of the stack.
- Clean separation: Cards fan and slide apart without edge-to-face blocking or pigment rub-off during handling.
Failure Modes
- Overspray face staining: Loose stack clamping or excessive spray pressure forces atomized pigment into micro-gaps between cards, leaving hazy speckles along the velvet perimeter. Because soft-touch film has a matte, textured surface, wiping away overspray burnishes and scars the coating.
- Capillary bleed under lifted film: Low-viscosity dye or over-wet ink wicks horizontally into the paper core or beneath soft-touch film edges lifted during die-cutting or corner rounding, producing feathered dark halos along card borders.
- Clamp-mark impressions on dark artwork: The clamping force required to seal a stack against overspray can flatten the compressible velvet texture on outer cards, leaving shiny bands or pressure marks. Dark artwork amplifies these marks, making anti-scuff matte a more durable alternative when heavy clamping is unavoidable.
- Edge-to-face blocking and seam chipping: Releasing or collating cards before edge pigment cures causes adjacent soft-touch faces to stick together or tears dried pigment chips away from the film-to-paper edge.
Parent guide Soft-Touch Lamination and Edge Finishing Compatibility