For press mechanics, adhesive curing, and comparisons with hot stamping, see the cold foil finishing guide.
When to Apply Cold Foil to Flat Sheets vs. Alternatives
- Rigid game boards and two-piece rigid boxes: Apply cold foil to the flat 128–157 gsm coated wrap paper first, seal it with a protective varnish or film lamination, and mount it onto 1.5–3 mm (0.059–0.118 in) greyboard afterward.
- Folding tuck boxes: Run cold foil inline on flat 300–400 gsm coated folding boxboard prior to die-cutting and creasing. Keep solid metallic areas clear of high-stress score lines, or seal the sheet with film lamination before folding.
- Unvarnished or deeply textured wraps: Inline cold foil relies on smooth surface contact against the offset blanket to transfer cleanly. Uncoated, porous, or heavily embossed papers cause broken edges and haloing; apply cold foil only to smooth coated sheets, or use post-press hot stamping on deep textures.
Specifications and Material Limits
- Wrap paper (rigid boxes and boards): 128–157 gsm coated art paper—approximately 86–106 lb US Text on a 25 × 38 in basis sheet (distinct from US Cover LB, which uses a 20 × 26 in basis sheet).
- Rigid greyboard core (mounted post-foil): 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in).
- Wrap turn-in margin: 15–20 mm (0.59–0.79 in) folded around the greyboard edges and anchored to the interior face.
- Tuck-carton board: 300–400 gsm coated folding boxboard—approximately 111–148 lb US Cover on a 20 × 26 in basis sheet, with typical calipers around 0.34–0.44 mm (0.013–0.017 in) depending on mill grade.
- Protective topcoat: Inline UV/aqueous varnish or BOPP/PET film lamination. Anti-scuff matte lamination suits dark artwork overprinted onto cold foil; double-sided film lamination on card stock adds 0.03–0.05 mm (0.001–0.002 in) total caliper.
- Prepress file setup:
- Format: AI, PDF, or PSD exported as PDF/X-1a or PDF/X-4 at ≥300 DPI.
- Color and layers: CMYK process layers plus a separate 100% spot vector layer for the cold-foil adhesive mask.
- Bleed and safety: 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety margin from trim, score channels, and wrap fold lines.
- Type and ink limits: Outlined or embedded fonts, 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) ≤280%–300%.
Production Steps
- Prepress separation and score clearance: Build the foil mask as clean vector shapes on a dedicated spot channel. Pull fine foil borders and reverses at least 3 mm (0.118 in) back from tuck-carton score lines and the 15–20 mm (0.59–0.79 in) board-wrap hinge lines where possible.
- Inline foil transfer and CMYK overprint: On the sheetfed offset press, the first unit prints UV-curable adhesive onto the flat 128–157 gsm wrap sheet or flat tuck-carton sheet. The foil unit nips the metallic carrier web onto the tacky adhesive, strips the carrier away, cures the bond, and sends the sheet through the remaining CMYK units in the same pass to create overprinted metallic tints.
- Topcoating or lamination: Apply an inline protective varnish or off-press film lamination over the cured foil and ink before any mechanical folding or wrapping occurs.
- Die-cutting, scoring, and mounting:
- Tuck boxes: Die-cut and crease the flat foiled sheets, then fold and glue the side seam and dust flaps.
- Rigid boxes and boards: Coat the back of the foiled wrap sheet with mounting glue, register it onto the 1.5–3 mm (0.059–0.118 in) greyboard, and fold the 15–20 mm (0.59–0.79 in) margins tightly around the board edges under roller pressure.
Sign-Off Criteria
- Registration and edge sharpness: Metallic edges align with CMYK overprints without visible adhesive halos, bridging in fine knockouts, or missing transfer specks.
- Fold and crease integrity: Scored tuck-box flaps and 90-degree or 180-degree wrapped board edges show continuous metallic coverage without cracking, flaking, or white substrate exposure along the fold.
- Surface rub resistance: Protective varnish or film lamination prevents scratching and ink lift when rubbed against adjacent cartons or board surfaces.
- Wrap adhesion: The 15–20 mm (0.59–0.79 in) turn-in margins lie flat against the greyboard interior without bubbling, edge lift, or glue bleed-through.
Failure Modes and Prevention
| Failure Mode | Physical Cause | Prevention |
|---|---|---|
| Foil cracking along tuck scores | Heavy metallic foil bridges a 90-degree crease channel without surface flexibility | Clear foil away from score channels or apply flexible film lamination before die-cutting |
| Abrasion on 15–20 mm (0.59–0.79 in) wrap folds | Rigid-box wrapping belts and turning bars scuff unsealed cold foil | Seal wrap sheets with protective varnish or anti-scuff matte lamination prior to mounting |
| Foil haloing or plugged fine detail | Excess UV adhesive tack, over-pressure at the foil nip, or porous paper stock | Use smooth coated wrap paper, control adhesive film weight, and keep fine knockouts above press minimum line weights |
| Turn-in edge lift after mounting | Tension from laminated wrap paper pulls the 15–20 mm (0.59–0.79 in) margin off the greyboard | Match mounting glue tack to laminated wrap stiffness and maintain full 15–20 mm (0.59–0.79 in) wrap width |
| Press jam or cylinder damage | Attempting to feed pre-mounted 1.5–3 mm (0.059–0.118 in) greyboard through an offset press | Always foil flat 128–157 gsm wrap sheets first and mount onto greyboard afterward |
Parent guide Inline Cold Foil Transfer