Quick Selection by Component
- Playing and game cards: Use cold foil, flat spot UV, or metallic ink when shuffleability and uniform stack height are priorities; reserve hot foil and raised UV for low-flex areas away from R3–R3.5 mm (0.118–0.138 in) corner cuts and high-wear edges. Avoid deep embossing or debossing on double-sided cards where reverse-side distortion affects hidden information.
- Rigid boxes and game boards: Use hot foil, raised UV, and embossing/debossing on 1.5–3 mm (0.059–0.118 in) greyboard wraps; keep heavy raised UV and foil clear of the 15–20 mm (0.591–0.787 in) wrap-around fold margins to prevent cracking along box edges.
- Booklets, leaflets, and tuck packaging: Use flat spot UV, cold foil, or metallic ink across 200–300 gsm (74–111 lb Cover, 20×26 in basis) covers and 4/6/8-panel leaflets; keep decorative layers off score lines and folds.
- Partner-sourced non-paper components: Use UV-cured spot/raised coatings, white underprint, or heat-compatible transfer/foil processes on 0.30 mm (0.012 in) PVC cards and partner-made plastic, wood, or coated game pieces, matching cure temperature and ink adhesion to the non-porous or textured surface.
Process Reference & Compatibility Matrix
Routine color, pattern, and coverage variants are handled within each process specification rather than as separate finishes.
| Process | Visual & Tactile Effect | Compatible Surfaces | Tooling & Setup Drivers | Key Compatibility Limits |
|---|---|---|---|---|
| Hot Foil Stamping | High-gloss or satin metallic/pigment film with slight heat-pressed deboss | Coated card stocks (300–400 gsm), rigid box wraps, heavy covers (200–300 gsm), heat-tolerant partner plastics/wood | Custom metal stamping die per design; subject to project/component minimums | Thick film lamination can blister under die heat; avoid fine lines <0.25 mm (0.010 in) or tight reverses; conflicts with high-relief linen textures |
| Cold Foil | Flat, crisp metallic sheen overprinted with CMYK for tinted metallics | Smooth coated offset card stocks, folding cartons, booster wraps, booklet covers | Inline flexo/offset foil plate + UV adhesive; scales efficiently at 200–1,000+ tiers | Requires smooth coated substrate; matte lamination over cold foil dulls metallic brilliance unless spot-coated |
| Spot UV (Flat) | High-gloss contrast against matte or uncoated background with minimal height | Matte-laminated cards, anti-scuff matte box wraps, coated covers | Digital or screen UV mask; low mechanical tooling impact | Needs matte base or lamination for visual contrast; poor adhesion over silicone-heavy or waxy coatings |
| Raised UV (Sculpted) | Glossy, 3D tactile polymer relief | Rigid box wraps, thick card stocks (350–400 gsm), heavy covers, rigid PVC | High-build UV screen or digital inkjet pass; thickness adds to card stack height | Cracks on folding box creases and card flex zones; increases stack height beyond standard 1.5–3 mm (0.059–0.118 in) box clearance if overused |
| Embossing & Debossing | Raised (emboss) or recessed (deboss) 3D paper relief; blind or foil-registered | Thick rigid box wraps (over 1.5–3 mm greyboard), heavy covers (200–300 gsm), single-sided display boards | Brass/magnesium male-female die set; project minimums apply | Deforms reverse face on 0.28–0.44 mm (0.011–0.017 in) card stocks; unsuitable for double-sided game cards |
| Metallic Inks | Subtle metallic shimmer (gold, silver, copper, tinted Pantone metallics) | Uncoated and coated papers, card stocks, booklets (80–120 gsm interior, 200–300 gsm cover) | Dedicated offset spot ink unit; no stamping die required | Lower reflectivity than hot/cold foil; tarnishes or rubs without protective aqueous or matte varnish |
| UV-Reveal Inks | Invisible or near-invisible ink under normal light that fluoresces under 365–395 nm UV light | Coated/uncoated card stocks, booklets, punchboards, packaging inserts | Dedicated spot ink pass; requires dark-room or UV-lamp inspection | Can leave slight gloss ghosting on high-sheen stocks; requires matte finish or busy pattern underneath to mask trace sheen |
| Holographic Transfers | Prismatic, diffractive, or custom-pattern rainbow shimmer | Coated card stocks, rigid box wraps, booster packs, PVC | Hot or cold foil transfer tooling; pattern-seam alignment if continuous | Seamless patterns may show repeat lines on large boards; overprinting CMYK requires white underprint to prevent color muddying |
| White Underprint | Opaque white base layer isolating CMYK or spot colors from dark/metallic/clear media | Holographic transfers, metallic foils, dark-dyed stocks, 0.30 mm (0.012 in) clear/colored PVC, partner wood/acrylic | Dedicated opaque white screen or digital/offset pass | Misregistration leaves white halos around edges; double-hit white needed on dark or mirror-bright substrates |
Surface & Component Application
Cards & Deck Formats
Standard offset card runs start at 200 decks (usual tiers: 200, 300, 500, and 1,000+). Select card core caliper and coating before locking decorative layers:
- Card stocks and thickness: 300 gsm art/blue core measures 0.28–0.31 mm (0.011–0.012 in); 310 gsm black-core linen measures 0.30–0.32 mm (0.012–0.013 in); 330 gsm black core measures 0.32–0.34 mm (0.013–0.013 in); 350 gsm art stock measures 0.34–0.38 mm (0.013–0.015 in); 400 gsm measures 0.40–0.44 mm (0.016–0.017 in); and PVC measures 0.30 mm (0.012 in).
- Lamination and stack height: Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card. Adding raised UV or heavy hot foil across full decks compounds total deck height; verify total stacked caliper against the 1.5–3 mm (0.059–0.118 in) box stack-height clearance and 1.5–2.5 mm (0.059–0.098 in) width/height clearance.
- Linen texture vs. foil/UV: On 310 gsm black-core linen, embossed linen pockets break thin cold foil lines and can cause micro-pinholing in fine spot UV. Apply decorative finishes before linen embossing or reserve linen for decks using metallic ink or varnish.
- Edge finishing: Thick film lamination can conflict with gilded edges because laminated film resists edge-foil adhesion and creates peeling points during trim.
- Other deck formats: Non-standard deck dimensions follow the same caliper, bleed, and edge-clearance rules; keep decorative foil and raised UV inside the safe zone so die-cutting and R3–R3.5 mm (0.118–0.138 in) corner rounding do not slice through metallic or polymer layers.
Tabletop Paper, Boards & Packaging
- Greyboard and wraps: Rigid boxes and game boards use 1.5, 2, 2.5, or 3 mm (0.059, 0.079, 0.098, or 0.118 in) greyboard with a 15–20 mm (0.591–0.787 in) wrap margin. Anti-scuff matte lamination suits dark artwork on box lids and creates high contrast under spot UV or raised UV.
- Punchboards: Keep foil, raised UV, and metallic ink at least 2–3 mm (0.079–0.118 in) clear of the 3–4 mm (0.118–0.157 in) punchboard die gaps so steel-rule dies do not chip cured UV or lift foil edges during punch-out.
- Booklets and leaflets: Leaflets use 4, 6, or 8 panels; bound signatures use multiples of 4 (saddle stitch 12–40 pages, perfect binding 28+ pages, sewn binding 80–100+ pages recommended). Interior stocks run 80–120 gsm (about 0.08–0.13 mm / 0.003–0.005 in per sheet; roughly 54–81 lb Text on a 25×38 in basis sheet), and covers run 200–300 gsm (roughly 74–111 lb Cover on a 20×26 in basis sheet). Apply decorative finishes to 200–300 gsm covers only, keeping them off spine hinges and panel folds.
Note on US paper weights: US basis weights differ by sheet size (Text LB uses a 25×38 in basis sheet; Cover LB uses a 20×26 in basis sheet), so always specify gsm alongside lb when matching booklet interiors and covers.
Partner-Sourced Non-Paper Surfaces
Specialist manufacturing partners apply decorative finishes to PVC cards (0.30 mm / 0.012 in), booster foils, and non-paper game pieces (plastic, wood, acrylic, or coated tokens):
- White underprint: Required beneath CMYK or translucent spot colors on clear PVC, dark-dyed plastics, wood, and holographic substrates to maintain color opacity.
- UV-cured spot and raised coatings: Adhere well to rigid PVC and acrylic when paired with surface corona or primer treatment, without heat distortion.
- Hot foil on non-paper: Requires lower dwell temperature and heat-resistant polymer substrates; test adhesion on textured wood or soft plastics to prevent scorching or edge lift.
Prepress & File Specifications
Prepare production files in Adobe Illustrator (AI), PDF, or Photoshop (PSD) exported as PDF/X-1a or PDF/X-4 with all fonts outlined or embedded:
- Resolution & Color: ≥300 DPI for all raster artwork; CMYK base artwork with separate 100% K vector spot layers named clearly for each decorative pass (e.g.,
HOT_FOIL,SPOT_UV,RAISED_UV,EMBOSS,WHITE_UNDERPRINT,UV_REVEAL). - Black & Ink Limits: Use 100% K for fine text and micro-elements; use rich black C40–60 M30–40 Y30–40 K100 for large dark solids; keep Total Area Coverage (TAC) at ≤280%–300% to prevent ink set-off under hot foil or lamination.
- Bleed & Safety: Include 3 mm (0.118 in) bleed per side on all full-bleed decorative layers (such as edge-to-edge holographic transfers or white underprint). Keep critical foil, embossing, and UV-reveal elements at least ≥3 mm (0.118 in) inside the trim line, or ≥4–5 mm (0.157–0.197 in) on bordered card backs.
- Choke & Knockout: Choke white underprint inward by 0.1–0.2 mm (0.004–0.008 in) relative to the overprinted CMYK or foil edge to prevent white halos. Knock out CMYK behind opaque hot foil unless overprinting on cold foil or holographic film.
- Line Weights: Maintain minimum stroke weights of 0.25–0.35 mm (0.010–0.014 in) for hot foil and raised UV, and 0.4–0.5 mm (0.016–0.020 in) for embossing/debossing to ensure clean transfer and release.
Production Steps & Sign-Off Criteria
- Preflight & Spot Separation Check: Verify PDF/X-1a or PDF/X-4 compliance, ≥300 DPI, TAC ≤280%–300%, and isolated 100% K spot channels. Sign off on digital separation proofs before cutting metal dies or screens.
- Base Print & Cure: Print CMYK and metallic/UV-reveal spot inks; allow full oxidative or UV cure before lamination or foil stamping to prevent ink transfer or blistering.
- Underprint & Lamination: Apply white underprint (where required on holographic, dark, or PVC substrates) and base lamination (such as anti-scuff matte). Confirm smooth film bond with zero silvering or trapped air.
- Decorative Pass Application:
- Cold foil / Metallic ink: Applied inline during offset/flexo pass.
- Hot foil / Emboss / Deboss: Applied offline with heated metal dies on registered sheets.
- Spot UV / Raised UV: Applied post-lamination via screen or digital UV head and cured under UV lamps.
- Registration & Adhesion Sign-Off: Inspect press sheets for spot-to-CMYK registration within tolerance, clean foil release without bridging in tight reverses, and UV-reveal fluorescence under a UV light source with zero ghosting under ambient light.
- Finishing & Packaging Assembly: Die-cut cards (with R3–R3.5 mm / 0.118–0.138 in corners), punchboards (3–4 mm / 0.118–0.157 in die gap), and wraps (15–20 mm / 0.591–0.787 in margin); apply edge gilding if specified; verify final deck stack fits box clearances (1.5–2.5 mm / 0.059–0.098 in width/height; 1.5–3 mm / 0.059–0.118 in stack height).
Failure Modes & Physical Limits
- Foil bridging and flaking: Fine positive lines (<0.25 mm / 0.010 in) or tight negative spaces fill in during hot stamping, while un-cured ink or heavy linen texture causes foil to flake off during shuffling.
- Raised UV cracking on folds: Applying high-build UV across box lid hinges, tuck-box scores, or leaflet folds causes the brittle cured polymer to crack and peel along the crease.
- Emboss show-through on cards: Deep embossing or debossing on 300–400 gsm (0.28–0.44 mm / 0.011–0.017 in) card stocks creates tactile telegraphing on the opposite face, compromising card uniformity.
- Lamination and gilded-edge conflict: Thick double-sided film lamination (adding 0.03–0.05 mm / 0.001–0.002 in per card) prevents edge-gilding foil from bonding cleanly to the paper core edge and leads to peeling along card borders.
- White underprint haloing: Zero-choke white underprint extends past CMYK edges when sheet registration shifts slightly, leaving visible white outlines around graphics on dark or holographic stocks.
- UV-reveal ghosting: Printing UV-reveal ink over a uniform matte or dark solid without surface texture or pattern variation leaves a faint glossy sheen visible at oblique angles under normal room lighting.
Compliance & Documentation Procedures
When decorative finishes are used on children's games, packaged retail sets, or distributed packaging, align testing and registration records with destination market requirements:
- Toy & game safety (EN 71): For products intended for children, plan EN 71 assessment and physical/chemical testing (including heavy-metal migration and mechanical durability of coatings, foils, and small components) against European Commission Toy Safety procedures and retain lab test reports for the finished decorative stack.
- German packaging registration (VerpackG): Producers placing packaged games or decks onto the German market register packaging weights (including laminated or foil-stamped boxes and inserts, tracked in kg/lb) and report data through Zentrale Stelle Verpackungsregister (VerpackG).
- French sorting signage (Triman): Retail packaging and printed inserts distributed in France require compliant Triman and sorting-instruction markings per French Ministry of Ecological Transition Info-Tri rules, integrated into the artwork layer before final print sign-off.
Guides in this section
Parent guide Print Finishes and Compatibility