For general tooling geometry and impression mechanics, see the main debossing guide. On card-and-box projects, the deciding constraint is whether the reverse face is hidden during use:
- Playable cards with hidden backs: Any tactile ridge, raised dome, or gloss halo on the back marks the card. Single-ply 300–400 gsm game cards cannot take deep debossing; even shallow blind debossing over a softer anvil must leave zero reverse-side show-through under raking light.
- Dividers and display cards: Single-sided reference cards, promo cards, and box dividers have no hidden-back marking constraint. Reverse-side bruising is acceptable as long as the sheet stays flat enough to fit the box.
- Folding tuck boxes: Thick carton boards absorb impression depth better than 300–350 gsm card stocks, and the inside of the box is hidden in normal use. Deep debossing works well on exterior panels when kept clear of crease lines, tuck locks, and glue flaps.
Specifications and Material Constraints
Standard offset card runs start at 200 decks (usual tiers 200, 300, 500, and 1,000+), while boxed games and custom deboss tooling follow project and component minimums through specialist offset and tabletop manufacturing partners.
Stock Caliper and Deboss Behavior
When specifying paper weights in US units, distinguish US Cover LB (20 × 26 in / 508 × 660 mm basis sheet) from US Text LB (25 × 38 in / 635 × 965 mm basis sheet). Card stocks and folding carton boards from 300 to 400 gsm fall in the heavyweight Cover LB range rather than Text LB.
| Substrate | Caliper (mm / in) | Reverse-Side Show-Through | Suitability |
|---|---|---|---|
| 300 gsm art / blue core | 0.28–0.31 mm (0.011–0.012 in) | High; deep dies telegraph through to the back | Display cards or shallow soft-anvil accents only |
| 310 gsm black-core linen | 0.30–0.32 mm (0.012–0.013 in) | High; linen texture distorts around deep edges | Avoid on playable cards; shallow accents on dividers |
| 330 gsm black core | 0.32–0.34 mm (0.013 in) | Moderate to high without a soft anvil | Dividers and display cards; avoid deep back-marking dies |
| 350 gsm art stock | 0.34–0.38 mm (0.013–0.015 in) | Moderate; visible bump under hard counter pressure | Dividers, rigid inserts, and light tuck cartons |
| 400 gsm art / board | 0.40–0.44 mm (0.016–0.017 in) | Lower on shallow impressions; visible on deep cuts | Display cards, dividers, and folding tuck boxes |
| PVC | 0.30 mm (0.012 in) | Prone to stress whitening and spring-back | Unsuitable for standard paper-style debossing |
Prepress, Finishes, and Clearances
- File setup: Supply artwork in AI, PDF, or PSD using PDF/X-1a or PDF/X-4, with all fonts outlined or embedded. Place the deboss die on a separate spot layer above the CMYK print layers.
- Color and resolution: Keep raster graphics at 300 DPI or higher. Use 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100 for solid dark areas, and keep total area coverage (TAC) at or below 280%–300%.
- Bleed, safety, and corners: Include 3 mm (0.118 in) bleed per side. Keep deboss elements inside the safety margin of at least 3 mm (0.118 in), or 4–5 mm (0.157–0.197 in) on bordered card backs, and clear of R3–R3.5 mm (0.118–0.138 in) rounded corners.
- Lamination and edge finishes: Double-sided film lamination adds 0.03–0.05 mm (0.001–0.002 in) per card. Anti-scuff matte lamination suits dark artwork where die pressure can otherwise burnish uncoated ink. Thick lamination can conflict with gilded edges.
- Tuck box clearance: Maintain 1.5–2.5 mm (0.059–0.098 in) clearance across box width and height and 1.5–3 mm (0.059–0.118 in) for total deck stack height, accounting for both double-sided film thickness and any bowing caused by debossed dividers or display cards.
Job-Specific Production Steps
- Separate the deboss spot layer and check structural zones: Verify that deboss vectors sit on a dedicated spot layer and stay clear of card borders, rounded corners, folding box score lines, tuck tabs, and glue flaps.
- Print and coat or laminate the flat sheets: Run CMYK and any spot inks first, then apply protective coating or anti-scuff matte film so the surface resists cracking and die burnishing.
- Configure the die and anvil for the substrate: On 300–400 gsm single-ply cards where reverse-side flatness matters, pair the metal die with a softer anvil and shallow impression depth. On thick tuck boards and single-sided display cards, use firmer backing to sharpen the recessed shoulder.
- Die-cut, fold, and check stack fit: Cut cards and crease tuck cartons after debossing, then load a full deck and any dividers into the folded box to confirm the stack clears the 1.5–3 mm (0.059–0.118 in) height allowance.
Sign-Off Criteria
- Reverse-side inspection: Under raking light, playable cards with hidden backs show no raised bump, dimple, or gloss halo opposite the debossed face.
- Surface and ink integrity: Lamination and dark rich-black fills show no cracking, flaking, or polished scuff halos along the recessed edge.
- Registration: The deboss impression aligns cleanly with any printed keylines, frames, or foil elements on the face.
- Box closure and flatness: Folding tuck boxes crease cleanly without split fibers near the deboss, glue flaps bond flat, and the assembled deck fits within the 1.5–2.5 mm (0.059–0.098 in) width/height and 1.5–3 mm (0.059–0.118 in) stack-height clearances.
Concrete Failure Modes
- Card marking via reverse-side show-through: Using a hard counter or excessive impression depth on 300–400 gsm single-ply cardstock pushes a palpable bump onto the back, making individual cards identifiable in a deck.
- Film cracking and ink burnishing: Sharp, narrow die edges fracture brittle coatings or leave shiny pressure halos on dark matte artwork when anti-scuff matte lamination is omitted.
- Stack-height bloat and bowed dividers: Deep impressions across wide areas warp 300–350 gsm dividers or display cards, consuming the 1.5–3 mm (0.059–0.118 in) stack-height clearance and bowing the tuck box lid.
- Split tuck scores and weak glue seams: Placing deboss geometry across or adjacent to folding creases pre-stresses the board fibers, causing the carton to crack during folding or pop open along the glue flap.
- PVC stress whitening: Applying standard metal-die compression to 0.30 mm (0.012 in) PVC turns sharp die edges milky white and loses crispness as the plastic springs back.
Parent guide Recessed Debossing