Specifications and Clearance Conditions

Foil placement changes between single-ply folding cartons (tuck boxes) and multi-panel rigid boards (game boards and GM screens) due to how each component bends and wraps.

Component Type Structural Build Foil Clearance Rule
Folding tuck boxes Printed paperboard with die-cut scores and tuck flaps Keep foil off all crease lines, flap folds, and glue tabs
Folding game boards Printed wrap mounted to 1.5–3 mm (0.059–0.118 in) greyboard Confine foil to flat panel faces; clear hinge gutters and 15–20 mm (0.591–0.787 in) wrap margins
GM screens Multi-panel rigid greyboard (1.5–3 mm / 0.059–0.118 in) with hinged seams Keep foil on rigid interior/exterior faces, clear of fold seams and board edges

File and Surface Requirements

  • Prepress format: Supply AI, PDF, or PSD files exported as PDF/X-1a or PDF/X-4 with outlined or embedded fonts and raster elements at 300 DPI or higher.
  • Color and spot separation: Set artwork in CMYK with separate spot layers for the hot foil stamping plate. Use 100% K for fine text, rich black at C40–60 M30–40 Y30–40 K100, and total area coverage (TAC) at or below 280%–300%.
  • Bleed and safety: Include 3 mm (0.118 in) bleed per side on printed artwork and maintain at least 3 mm (0.118 in) safety margin from trim lines, score lines, and hinge gutters.
  • Surface coatings: Anti-scuff matte lamination suits dark artwork by preventing rub marks during folding and assembly while giving foil a smooth, uniform bonding surface.
  • Tooling and minimums: Standard offset card decks start at 200 decks (usual tiers of 200, 300, 500, and 1,000+), while boxed games, custom tuck boxes, and folding boards follow project and component tooling minimums with specialist offset and tabletop manufacturing partners.

Job-Specific Production Steps

  1. Print the flat sheet: Offset print the tuck-box carton sheet or the game-board/GM-screen wrap sheet in CMYK.
  2. Apply surface coating: Laminate or coat the flat sheet (such as anti-scuff matte film on dark backgrounds) before stamping so the foil bonds cleanly to the top surface without cracking the ink layer underneath.
  3. Hot foil stamp on the flat sheet: Stamp the metallic foil using a metal die registered to the printed press sheet guides.
  4. Die-cut or mount:
    • Tuck boxes: Die-cut and crease the stamped sheet, then fold and glue along the designated glue flap.
    • Game boards and GM screens: Trim and mount the stamped wrap onto 1.5 mm (0.059 in), 2 mm (0.079 in), 2.5 mm (0.098 in), or 3 mm (0.118 in) greyboard panels, folding the 15–20 mm (0.591–0.787 in) wrap margin over the board edges and forming the hinged seams.

Sign-Off Criteria

  • Spot-layer verification: The foil spot layer aligns cleanly with the CMYK art in the PDF/X-1a or PDF/X-4 proof, with no unintended overprint or knockout gaps.
  • Dieline and seam clearance: Every foil element on the dieline overlay sits clear of tuck-box score lines, panel hinge gutters, and the 15–20 mm (0.591–0.787 in) board wrap margin.
  • Flat-sheet registration: Press-sheet inspection confirms that foil impressions align with both the printed graphics and the die-cut/mounting registration marks before full-run stamping proceeds.

Concrete Failure Modes

  • Foil cracking along folds and hinges: Foil placed across a tuck-box score line or a game-board/GM-screen hinge fractures and flakes along the crease as soon as the carton folds or the board opens.
  • Edge lifting on wrapped board margins: Foil extending into the 15–20 mm (0.591–0.787 in) wrap turn-in splits or peels when the paper wrap is pulled tight around 1.5–3 mm (0.059–0.118 in) greyboard edges.
  • Registration drift on multi-up tuck sheets: Normal sheet-fed shift between printing, foil stamping, and die-cutting pushes tight foil borders onto a crease or trim edge when insufficient safety clearance is left around score lines.
  • Poor adhesion or surface scuffing: Applying foil over incompatible heavy coatings or unlaminated dark ink causes patchy transfer or rub-off during folding and boxing; anti-scuff matte lamination stabilizes dark backgrounds around the stamped detail.