This guide covers the substrate-specific mechanics of white underprint on clear PVC cards and rigid acrylic standees or tokens.
Choosing Single-Hit vs. Double-Hit White and Print Order
The right ink stack depends on how much background light should pass through the artwork and which side of the component takes physical wear:
- Single-hit white: Deposits one pass of white ink under CMYK. Colors stay semi-translucent, letting underlying card layers, playmats, or table surfaces tint the art. Use single-hit white for stained-glass effects, layered card overlays, or subtle frosted graphics.
- Double-hit white: Deposits two passes of white ink (or a high-opacity double strike) under CMYK. Artwork reads solid and color-accurate even over dark or patterned surfaces, while unprinted areas remain clear. Use double-hit white for character art, readable typography, and opaque game icons.
- First-surface (front) printing: Ink sits on the viewing face (Substrate → White → CMYK → protective clear coat). Standard for clear PVC cards that flex during shuffling and require ink on one or both faces.
- Second-surface (reverse) printing: CMYK is mirrored and printed on the back of the clear material, followed by white backing (Substrate → Mirrored CMYK → White). Standard for partner-sourced acrylic tokens and standees so the solid acrylic body shields the ink from scratches and table wear.
Specifications for Clear PVC and Acrylic Runs
Card Deck Press produces clear PVC decks and partner-sourced acrylic pieces with specialist offset and tabletop manufacturing partners.
| Specification | Clear PVC Cards | Acrylic Tokens & Standees |
|---|---|---|
| Substrate & thickness | Translucent clear PVC, 0.30 mm (0.012 in) | Partner-sourced clear cast or extruded acrylic; thickness set by project tooling |
| Minimum order | Standard card runs start at 200 decks (usual tiers: 200 / 300 / 500 / 1,000+) | Follows project and component minimums for partner cutting and tooling |
| Print order | First-surface (Substrate → White → CMYK → protective coating) or dual-sided sandwich | Second-surface mirrored (Acrylic → Mirrored CMYK → White) for single-sided viewing |
| White opacity | Single-hit (semi-translucent) or double-hit (solid opaque backing) | Single-hit or double-hit; double-hit preferred for high-contrast tabletop pieces |
| Bleed & safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) safety (≥4–5 mm / 0.157–0.197 in for bordered backs) | Extend full-bleed graphics past cut path per component dieline; keep fine text inside safe zone |
| Corner radius | R3–R3.5 mm (0.118–0.138 in) standard card corners | Custom laser-cut or routed profiles |
| Prepress files | AI, PDF, or PSD; PDF/X-1a or PDF/X-4; ≥300 DPI | AI, PDF, or PSD; PDF/X-1a or PDF/X-4; ≥300 DPI |
| Color & ink limits | CMYK + separate spot layer for white; 100% K fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% | CMYK + separate spot layer for white; 100% K fine text; rich black C40–60 M30–40 Y30–40 K100; TAC ≤280%–300% |
Note: Clear PVC card trim dimensions vary by deck format; establish the exact millimetre trim and die profile in the job specification before building the white spot layer.
Job-Specific Production Steps
- Build the white spot channel and choke: Create a dedicated 100% spot-ink layer or channel (for example,
White_Underprint) separate from CMYK. Leave clear windows completely empty (0% CMYK, 0% white). Choke (inset) the white spot silhouette slightly inside the CMYK perimeter so normal press registration variance does not expose a white rim. - Verify mirroring and layer order: For second-surface acrylic tokens and standees, mirror the artwork horizontally and verify the RIP order prints CMYK first onto the acrylic back, followed by the white backing pass. For clear PVC cards, keep artwork right-reading on the printed face.
- UV-cure between white and CMYK passes: Clear PVC and acrylic are non-absorbent substrates. UV curing locks the first white pass before the second white pass or CMYK overprint is applied, preventing ink spread and preserving sharp edges.
- Cut, corner-round, and mask: Die-cut and round clear PVC cards to R3–R3.5 mm (0.118–0.138 in) after full curing. Partner-made acrylic pieces are laser-cut or routed with protective masking left on the clear viewing face until final packing.
- Maintain regulatory records where applicable: When clear PVC cards or acrylic game pieces are supplied for products intended for children in the EU, compile EN 71 assessment and testing documentation against EU Toy Safety requirements.
Sign-Off Criteria
Before approving a production proof or press sheet for clear PVC or acrylic runs, verify four physical checkpoints:
- Opacity over contrasting surfaces: Place the proofed PVC card or acrylic token over both a bright white sheet and a dark black surface. Double-hit white zones must keep CMYK colors saturated without dark background bleed-through; single-hit zones must show uniform, intentional translucency.
- Zero edge haloing: Inspect high-contrast graphic borders and fine type at normal viewing distance. The choked white underprint must stay concealed behind the CMYK edge with no white outline peeking around characters or icons.
- Window clarity: Unprinted zones must remain optically clear without ink misting, static-induced spray, or stray halftone dots.
- Adhesion and flex integrity: On 0.30 mm (0.012 in) PVC cards, flexed corners and shuffled edges must show no ink cracking or flaking. On second-surface acrylic pieces, the exposed clear face must be scratch-free and free of ink bleed along cut edges.
Concrete Failure Modes
- White edge haloing: Supplying the white spot plate at an exact 1:1 match with the CMYK artwork causes any slight registration shift to expose a bright white outline around dark or saturated shapes. Fix: Choke the white underprint inward relative to the CMYK boundary and avoid hairline white-backed strokes on transparent backgrounds.
- Washed-out colors over dark tables: Using single-hit white behind light or medium CMYK tones lets dark tabletops or overlapping cards show through, muddying yellows, reds, and skin tones. Fix: Specify double-hit white under all artwork that must read solid regardless of background.
- Inverted second-surface ink order: Printing white before CMYK on the back of an acrylic standee—or failing to mirror the file—places the white layer between the viewer and the color, hiding the artwork or reading backwards. Fix: Confirm mirrored orientation and
CMYK → Whitelayer order in the PDF/X-4 proof. - Ink cracking or scuffing on exposed faces: Heavy double-hit white plus high-TAC CMYK on an unsealed PVC face or first-surface acrylic token scuffs rapidly during play. Fix: Cap CMYK total area coverage at ≤280%–300%, use rich black within C40–60 M30–40 Y30–40 K100, apply a protective clear coating on PVC, and route single-sided acrylic pieces to second-surface printing.
Parent guide Opaque White Underprint