Material and Binding Specifications
Bound rulebooks and art books combine lightweight interior signatures with heavier covers, creating two different paper densities under the spray gun. Basis weights in US pounds (lb) depend on the parent sheet size: US Text LB is measured on a 25 × 38 in (635 × 965 mm) basis sheet, while US Cover LB is measured on a 20 × 26 in (508 × 660 mm) basis sheet.
| Parameter | Specification | Physical Impact on Edge Spraying |
|---|---|---|
| Binding structure | Multiples of 4 pages; sewn binding (80–100+ pages recommended) or perfect binding (28+ pages) | Provides a flat, square spine and sufficient block height for hydraulic clamping; saddle stitch (12–40 pages) flexes and gaps under pressure |
| Interior stock | 80–120 gsm (approx. 54–81 lb US Text, 25 × 38 in basis); 0.08–0.13 mm (0.0031–0.0051 in) per sheet | Lightweight uncoated sheets wick liquid pigment faster than coated sheets and require tighter clamp compression |
| Cover stock & finish | 200–300 gsm (approx. 74–111 lb US Cover, 20 × 26 in basis); anti-scuff matte suits dark artwork | Thick cover lamination can lift or conflict with edge decoration if not trimmed flush before clamping |
| Bleed & safety | 3 mm (0.118 in) bleed per side; ≥3 mm (0.118 in) interior safety margin | Keeps running headers and page numbers clear of the cut edge if microscopic wicking occurs |
| Prepress & color | AI/PDF/PSD in PDF/X-1a or PDF/X-4; ≥300 DPI; CMYK + separate spot layer for edge color | Specify edge pigment as a dedicated spot color; use 100% K for fine text, rich black C40–60 M30–40 Y30–40 K100, TAC ≤280%–300% |
| Order minimums | Project and component minimums for boxed games and bound tooling | Standard offset card decks start at 200 decks (200/300/500/1,000+ tiers); bound book minimums follow project tooling |
When staging palletized book blocks before trimming and clamping, calculate stack loads using both metric and imperial units (lb = kg * 2.2046, in = mm / 25.4) so press operators do not overload clamp beds or warp bottom signatures under heavy stacks (for example, a 15 kg / 33.1 lb stack of trimmed blocks).
Production Steps
- Square and three-knife trim the bound block: Trim the head, tail, and fore-edge after the 200–300 gsm cover is bound and laminated so the cover edges sit completely flush with the 80–120 gsm interior leaves. Any overhanging lamination film acts as a lip that traps liquid pigment.
- Load into the hydraulic clamp: Jog the trimmed blocks squarely and apply high, even hydraulic compression across the book faces. Tighter clamping forces air out from between the 0.08–0.13 mm (0.0031–0.0051 in) leaves, sealing the paper edges into a solid plane.
- Mask the spine and outer cover faces: Cover the spine hinge and exposed front/back covers with protective masking before spraying. Uncoated covers and matte-laminated dark covers show pigment haze immediately if overspray drifts past the fore-edge.
- Apply thin mist passes with flash drying: Spray atomized pigment in multiple light mist passes rather than a single heavy coat. Allow each pass to flash-dry before applying the next so pigment dries on the cut fiber ends instead of soaking inward along the sheet grain.
- Unclamp and fan after surface dry: Release hydraulic pressure only after the pigment film is dry to the touch. Fan the pages gently to break any microscopic pigment bridging between adjacent leaves before packing or inserting into game boxes.
If the bound rulebook or art book ships inside a game or toy product requiring regulatory documentation, maintain material and ink assessment records under EU Toy Safety (EN 71) alongside applicable packaging compliance records such as LUCID / VerpackG and Triman / Info-tri where relevant to the destination market.
Sign-Off Criteria
- Margin cleanliness: Zero visible pigment bleed or feathering inward past the cut edge into the 3 mm (0.118 in) safety margin on uncoated or coated pages.
- Edge opacity: Even color density across the head, tail, and fore-edge, including the junction where the 200–300 gsm cover meets the text block.
- Cover and spine integrity: Clean spine hinges and cover faces free of overspray mist, masking adhesive residue, or lifted lamination at the corners.
- Page separation: Smooth fanning across all signatures without leaf-to-leaf sticking or torn paper fibers.
Concrete Failure Modes
- Capillary wicking into text margins: Low hydraulic clamping pressure or overly wet spray passes let liquid pigment wick 0.5–2.0 mm (0.020–0.079 in) inward along porous 80–100 gsm uncoated sheets. Increase clamp pressure and split the coverage into thinner mist passes with longer flash-dry intervals.
- Leaf-to-leaf bridging (stuck pages): Applying too much wet film in one pass or unclamping before the pigment sets glues adjacent 0.08–0.13 mm (0.0031–0.0051 in) sheets together. Reduce nozzle flow rate, extend drying time under clamp, and fan blocks immediately upon release.
- Spine and cover overspray: Gaps in spine masking or slight cover curl under uneven clamps allow atomized mist to settle on dark anti-scuff matte covers or spine creases. Verify flush three-knife trimming and full-coverage masking prior to spraying.
- Cover edge lifting or chipping: Thick lamination on 200–300 gsm covers can delaminate at the trim edge under clamp shear or heavy pigment wetting. Use clean knife trimming after lamination and keep mist passes light at the cover-to-text boundary.
Parent guide Colored and Painted Edges