Basis weight governs how paper is ordered, converted, and matched across components in the printing and manufacturing glossary. The choice of unit shifts under two conditions:

  • Cross-regional offset production: International and specialist card mills grade stock by gsm (g/m^2), which measures mass per unit area independent of sheet dimensions.
  • Mixed-component boxed games: A single project often combines booklet interiors (80–120 gsm), booklet covers (200–300 gsm), and playing or game cards (300–400 gsm), where an unqualified "80 lb" or "100 lb" callout creates a twofold mass discrepancy between Text and Cover grades.

Specifications and Basis Sheet Comparison

Plain-Text Conversion Formula

Because US basis weight equals the mass of 500 sheets cut to the grade's standard parent sheet, converting from pounds (lb) to gsm requires the parent sheet area:

gsm = (Basis Weight in lb * 453.592) / (500 * Sheet Width in m * Sheet Height in m)

For the two primary tabletop and booklet grades:

Text (25 x 38 in / 635.0 x 965.2 mm):  gsm = Text lb * 1.480
Cover (20 x 26 in / 508.0 x 660.4 mm): gsm = Cover lb * 2.704

US Text vs. US Cover Basis Reference

Grade Basis Basis Sheet Size Ream (500 Sheets) Weight Equivalent gsm Typical Tabletop Use
US Text 25 × 38 in (635.0 × 965.2 mm) 60 lb (27.2 kg) ~89 gsm Light booklet/leaflet interiors
US Text 25 × 38 in (635.0 × 965.2 mm) 80 lb (36.3 kg) ~118 gsm Standard booklet interiors (80–120 gsm)
US Text 25 × 38 in (635.0 × 965.2 mm) 100 lb (45.4 kg) ~148 gsm Heavy booklet interiors / wraps
US Cover 20 × 26 in (508.0 × 660.4 mm) 80 lb (36.3 kg) ~216 gsm Booklet covers (200–300 gsm)
US Cover 20 × 26 in (508.0 × 660.4 mm) 100 lb (45.4 kg) ~270 gsm Heavy booklet covers / light tuckboxes
US Cover 20 × 26 in (508.0 × 660.4 mm) 110 lb (49.9 kg) ~297 gsm Entry 300 gsm art/blue-core card range
US Cover 20 × 26 in (508.0 × 660.4 mm) 120 lb (54.4 kg) ~324 gsm Mid-weight card stock range
US Cover 20 × 26 in (508.0 × 660.4 mm) 130 lb (59.0 kg) ~352 gsm Heavy 350 gsm art card range

Basis Weight vs. Caliper (Thickness)

Basis weight measures mass, not thickness. Fiber density, core layers, embossing, and surface films change caliper at the same gsm:

Component / Stock Basis Weight Approximate Caliper
Booklet interior stock 80–120 gsm 0.08–0.13 mm (0.0031–0.0051 in) per sheet
Booklet cover stock 200–300 gsm Varies by coating and bulk
Art / blue-core card stock 300 gsm 0.28–0.31 mm (0.0110–0.0122 in)
Black-core linen card stock 310 gsm 0.30–0.32 mm (0.0118–0.0126 in)
Black-core card stock 330 gsm 0.32–0.34 mm (0.0126–0.0134 in)
Art card stock 350 gsm 0.34–0.38 mm (0.0134–0.0150 in)
Heavy art / board card stock 400 gsm 0.40–0.44 mm (0.0157–0.0173 in)
Double-sided film lamination — Adds 0.03–0.05 mm (0.0012–0.0020 in) per card

Job-Specific Production Steps

  1. Translate US pound specs into gsm and grade basis: Convert every US weight callout into gsm before issuing production specs. State both the metric gsm and the intended grade (for example, 80 lb / 36.3 kg Text (~118 gsm) for interior pages versus 80 lb / 36.3 kg Cover (~216 gsm) for covers).
  2. Pair gsm with core and caliper for card runs: Standard offset card runs start at 200 decks (usual tiers: 200 / 300 / 500 / 1,000+). Select card stock by both gsm and core construction (such as 300 gsm art/blue core, 310 gsm black-core linen, or 330 gsm black core) rather than pound weight alone.
  3. Calculate finished stack height for packaging: Multiply per-card caliper—including 0.03–0.05 mm (0.0012–0.0020 in) for double-sided film if applied—by the deck card count, then verify that box depth retains 1.5–3 mm (0.059–0.118 in) stack-height clearance (alongside 1.5–2.5 mm / 0.059–0.098 in width/height clearance).

Sign-Off Criteria

  • Every paper specification lists metric gsm alongside any US lb (kg) value and explicitly names Text or Cover basis.
  • Card and booklet specifications include expected caliper in mm and in, accounting for any double-sided film addition.
  • Total deck or signature stack height fits within the box's 1.5–3 mm (0.059–0.118 in) stack-height clearance tolerance.

Concrete Failure Modes

  • Unqualified pound callout (Text vs. Cover swap): Specifying 100 lb (45.4 kg) without stating Cover vs. Text results in ~148 gsm Text stock instead of ~270 gsm Cover stock, producing flimsy booklet covers or underspecified packaging wraps.
  • Substituting gsm for caliper: Switching from an uncoated or embossed 310 gsm stock to a dense 300 gsm art stock, or adding double-sided film (+0.03–0.05 mm / 0.0012–0.0020 in per card), alters deck stack height by several millimeters over a full deck and can eliminate the 1.5–3 mm (0.059–0.118 in) box stack clearance.
  • Applying card basis weights to interior signatures: Ordering booklet interiors on Cover-basis equivalents instead of 80–120 gsm (0.08–0.13 mm / 0.0031–0.0051 in per sheet) causes excessive spine bulk, cracking on folds, and signature-fit failures in saddle-stitched or bound booklets.